High Speed Steel (HSS): Properties and Key Applications
Share
Table Of Content
Table Of Content
High Speed Steel (HSS) is a category of tool steel known for its ability to withstand high temperatures without losing its hardness. Classified as a high-carbon alloy steel, HSS typically contains significant amounts of tungsten, molybdenum, chromium, and vanadium, which contribute to its unique properties. These alloying elements enhance its wear resistance, toughness, and ability to retain hardness at elevated temperatures, making it ideal for cutting tools and machining applications.
Comprehensive Overview
High Speed Steel is primarily used in the manufacturing of cutting tools, such as drill bits, milling cutters, and saw blades. Its ability to maintain hardness at high temperatures (up to 600°C or 1112°F) allows it to perform effectively in high-speed machining operations. The key characteristics of HSS include excellent wear resistance, high toughness, and the ability to be hardened to a high degree.
Advantages of High Speed Steel:
- High Hardness: Retains hardness even at elevated temperatures, which is crucial for cutting applications.
- Wear Resistance: Excellent resistance to abrasion and wear, extending tool life.
- Versatility: Can be used for a variety of cutting tools and applications.
- Toughness: Good resistance to chipping and breaking under stress.
Limitations of High Speed Steel:
- Brittleness: Can be more brittle compared to other tool steels, making it susceptible to cracking under certain conditions.
- Cost: Generally more expensive than conventional carbon steels.
- Machinability: More challenging to machine than softer steels, requiring specialized tools.
Historically, HSS has played a significant role in the development of modern machining processes, enabling faster and more efficient production methods. Its market position remains strong, particularly in industries that require precision cutting tools.
Alternative Names, Standards, and Equivalents
| Standard Organization | Designation/Grade | Country/Region of Origin | Notes/Remarks |
|---|---|---|---|
| UNS | T1 | USA | Closest equivalent to AISI M2 |
| AISI/SAE | M2 | USA | Widely used; good balance of hardness and toughness |
| ASTM | A600 | USA | General specification for HSS |
| EN | 1.3343 | Europe | Equivalent to AISI M2; minor compositional differences |
| DIN | HS 6-5-2 | Germany | Similar properties; used in European applications |
| JIS | SKH2 | Japan | Comparable to M2, with slight variations in composition |
| GB | W18Cr4V | China | Equivalent to M2; used in Chinese manufacturing |
| ISO | 4957 | International | General standard for tool steels |
The differences between equivalent grades can significantly affect performance. For instance, while M2 and T1 are often considered interchangeable, M2 typically offers better toughness, making it preferable for applications requiring resilience against impact.
Key Properties
Chemical Composition
| Element (Symbol and Name) | Percentage Range (%) |
|---|---|
| C (Carbon) | 0.70 - 1.50 |
| Cr (Chromium) | 3.75 - 4.50 |
| Mo (Molybdenum) | 5.00 - 6.75 |
| W (Tungsten) | 5.50 - 6.75 |
| V (Vanadium) | 1.00 - 2.00 |
| Fe (Iron) | Balance |
The primary alloying elements in High Speed Steel play crucial roles:
- Tungsten (W): Enhances hardness and wear resistance, allowing the steel to maintain its cutting edge at high temperatures.
- Molybdenum (Mo): Improves toughness and hardenability, contributing to the overall strength of the steel.
- Vanadium (V): Increases wear resistance and refines the grain structure, enhancing toughness and stability during heat treatment.
Mechanical Properties
| Property | Condition/Temper | Test Temperature | Typical Value/Range (Metric) | Typical Value/Range (Imperial) | Reference Standard for Test Method |
|---|---|---|---|---|---|
| Tensile Strength | Quenched & Tempered | Room Temp | 900 - 1200 MPa | 130 - 175 ksi | ASTM E8 |
| Yield Strength (0.2% offset) | Quenched & Tempered | Room Temp | 600 - 1000 MPa | 87 - 145 ksi | ASTM E8 |
| Elongation | Quenched & Tempered | Room Temp | 5 - 10% | 5 - 10% | ASTM E8 |
| Hardness | Quenched & Tempered | Room Temp | 60 - 67 HRC | 60 - 67 HRC | ASTM E18 |
| Impact Strength | Quenched & Tempered | -20°C (-4°F) | 20 - 30 J | 15 - 22 ft-lbf | ASTM E23 |
The combination of these mechanical properties makes High Speed Steel particularly suitable for high-stress applications where cutting tools are subjected to significant mechanical loading. Its high tensile and yield strengths ensure durability, while its hardness allows for effective cutting performance.
Physical Properties
| Property | Condition/Temperature | Value (Metric) | Value (Imperial) |
|---|---|---|---|
| Density | - | 7.85 g/cm³ | 0.284 lb/in³ |
| Melting Point | - | 2800°C | 5072°F |
| Thermal Conductivity | 20°C | 25 W/m·K | 17.3 BTU·in/h·ft²·°F |
| Specific Heat Capacity | 20°C | 460 J/kg·K | 0.11 BTU/lb·°F |
| Electrical Resistivity | 20°C | 0.0001 Ω·m | 0.0001 Ω·in |
| Coefficient of Thermal Expansion | 20-100°C | 11.5 x 10⁻⁶/K | 6.4 x 10⁻⁶/°F |
Key physical properties such as density and thermal conductivity are significant for applications involving high-speed machining. The high melting point indicates stability under extreme conditions, while the thermal conductivity affects heat dissipation during cutting operations.
Corrosion Resistance
| Corrosive Agent | Concentration (%) | Temperature (°C/°F) | Resistance Rating | Notes |
|---|---|---|---|---|
| Chlorides | 5-10 | 20-60 / 68-140 | Fair | Risk of pitting |
| Acids | 10-20 | 20-60 / 68-140 | Poor | Susceptible to corrosion |
| Alkaline Solutions | 5-10 | 20-60 / 68-140 | Fair | Moderate resistance |
High Speed Steel exhibits moderate resistance to corrosion, particularly in chloride environments, where pitting can occur. Compared to stainless steels, HSS is less resistant to acidic and alkaline conditions, making it less suitable for applications exposed to harsh chemicals.
When compared to other tool steels, such as D2 or M2, HSS generally offers better wear resistance but at the cost of lower corrosion resistance. This trade-off is crucial when selecting materials for specific applications.
Heat Resistance
| Property/Limit | Temperature (°C) | Temperature (°F) | Remarks |
|---|---|---|---|
| Max Continuous Service Temp | 600°C | 1112°F | Retains hardness at high temps |
| Max Intermittent Service Temp | 650°C | 1202°F | Short-term exposure |
| Scaling Temperature | 700°C | 1292°F | Risk of oxidation above this temp |
| Creep Strength Considerations | 500°C | 932°F | Begins to lose strength |
High Speed Steel maintains its hardness and strength at elevated temperatures, making it suitable for high-speed cutting applications. However, prolonged exposure to temperatures above 600°C can lead to oxidation and scaling, which can compromise tool integrity.
Fabrication Properties
Weldability
| Welding Process | Recommended Filler Metal (AWS Classification) | Typical Shielding Gas/Flux | Notes |
|---|---|---|---|
| MIG | ER70S-6 | Argon + CO2 | Preheat recommended |
| TIG | ER80S-D2 | Argon | Requires careful control |
| Stick | E7018 | - | Not recommended for thick sections |
High Speed Steel is generally not recommended for welding due to its high carbon content, which can lead to cracking. Preheating and post-weld heat treatment are essential to minimize stress and improve weld integrity.
Machinability
| Machining Parameter | [High Speed Steel] | [AISI 1212] | Notes/Tips |
|---|---|---|---|
| Relative Machinability Index | 50 | 100 | HSS requires slower speeds |
| Typical Cutting Speed (Turning) | 30-40 m/min | 80-100 m/min | Use carbide tools for best results |
Machining High Speed Steel can be challenging due to its hardness. Optimal conditions include using carbide tools and slower cutting speeds to prevent tool wear.
Formability
High Speed Steel is not typically formed due to its hardness and brittleness. Cold and hot forming processes are generally avoided, as they can lead to cracking.
Heat Treatment
| Treatment Process | Temperature Range (°C/°F) | Typical Soaking Time | Cooling Method | Primary Purpose / Expected Result |
|---|---|---|---|---|
| Annealing | 700-800 / 1292-1472 | 1-2 hours | Air | Reduce hardness, improve machinability |
| Hardening | 1200-1300 / 2192-2372 | 30-60 minutes | Oil/Water | Increase hardness |
| Tempering | 500-600 / 932-1112 | 1 hour | Air | Reduce brittleness, improve toughness |
The heat treatment process for High Speed Steel involves hardening and tempering to achieve the desired balance of hardness and toughness. During hardening, the steel is heated to a high temperature and then rapidly cooled, which transforms its microstructure. Tempering follows to relieve stresses and reduce brittleness.
Typical Applications and End Uses
| Industry/Sector | Specific Application Example | Key Steel Properties Utilized in this Application | Reason for Selection (Brief) |
|---|---|---|---|
| Aerospace | Turbine blades | High hardness, wear resistance | High-performance requirements |
| Automotive | Cutting tools | Toughness, heat resistance | Precision machining |
| Manufacturing | Drill bits | Wear resistance, hardness | Long tool life |
| Metalworking | Milling cutters | High-speed performance | Efficiency in cutting |
Other applications include:
- Tooling for injection molding
- Saw blades for metal cutting
- Forming tools for sheet metal
High Speed Steel is chosen for these applications due to its ability to maintain sharp cutting edges and resist wear, which is critical in high-volume production environments.
Important Considerations, Selection Criteria, and Further Insights
| Feature/Property | [High Speed Steel] | [D2 Tool Steel] | [M2 Tool Steel] | Brief Pro/Con or Trade-off Note |
|---|---|---|---|---|
| Key Mechanical Property | High hardness | Good wear resistance | High toughness | HSS excels in high-speed applications |
| Key Corrosion Aspect | Moderate resistance | Poor | Fair | HSS is less corrosion-resistant than stainless steels |
| Weldability | Poor | Fair | Good | HSS requires special considerations for welding |
| Machinability | Moderate | Good | Excellent | HSS is harder to machine than softer steels |
| Formability | Poor | Fair | Good | HSS is not suited for forming processes |
| Approx. Relative Cost | High | Moderate | Moderate | Cost may be justified by performance benefits |
| Typical Availability | Moderate | High | High | HSS may be less readily available than other grades |
When selecting High Speed Steel, considerations include cost-effectiveness, availability, and specific application requirements. Its unique properties make it suitable for high-performance cutting tools, but its brittleness and welding challenges must be taken into account.
In summary, High Speed Steel remains a critical material in the tool-making industry, providing a balance of hardness, toughness, and wear resistance that is essential for modern machining applications.