CPM 10V steel is a high-performance tool steel known for its exceptional wear resistance and toughness. Classified as a high-carbon, high-vanadium alloy steel, CPM 10V is part of the CPM (Crucible Particle Metallurgy) family, which enhances its properties through advanced manufacturing techniques. The primary alloying elements in CPM 10V include carbon (C), vanadium (V), chromium (Cr), and molybdenum (Mo), each contributing to the steel's overall performance.
Comprehensive Overview
CPM 10V is characterized by its high carbon content (around 1.5%) and significant vanadium content (approximately 9.0%), which provide excellent hardness and wear resistance. The chromium and molybdenum enhance its toughness and corrosion resistance, making it suitable for demanding applications. The unique particle metallurgy process used in its production results in a fine, uniform microstructure that further improves its mechanical properties.
Advantages:
- Exceptional Wear Resistance: The high vanadium content contributes to the formation of hard vanadium carbides, which significantly enhance wear resistance.
- High Toughness: Despite its hardness, CPM 10V maintains good toughness, reducing the risk of chipping or cracking during use.
- Good Edge Retention: Ideal for cutting tools and blades, CPM 10V retains a sharp edge longer than many other tool steels.
Limitations:
- Difficult to Machine: The high hardness can make machining and grinding more challenging compared to lower alloy steels.
- Cost: Generally more expensive than conventional tool steels due to the advanced manufacturing process and alloying elements.
Historically, CPM 10V has gained popularity in the manufacturing of high-performance cutting tools, such as knives and industrial blades, due to its superior properties. Its market position is strong among tool steels, particularly for applications requiring high wear resistance and toughness.
Alternative Names, Standards, and Equivalents
Standard Organization | Designation/Grade | Country/Region of Origin | Notes/Remarks |
---|---|---|---|
UNS | T10402 | USA | Closest equivalent to AISI D2 with higher vanadium content |
AISI/SAE | CPM 10V | USA | High-performance tool steel |
ASTM | A681 | USA | Specification for tool steels |
JIS | SKD11 | Japan | Similar properties but different composition |
ISO | 1.2379 | International | Equivalent with minor compositional differences |
The differences between CPM 10V and its equivalents, such as JIS SKD11, primarily lie in the vanadium content and the manufacturing process, which can affect performance in specific applications.
Key Properties
Chemical Composition
Element (Symbol and Name) | Percentage Range (%) |
---|---|
C (Carbon) | 1.50 - 1.60 |
V (Vanadium) | 8.00 - 9.00 |
Cr (Chromium) | 4.00 - 5.00 |
Mo (Molybdenum) | 1.00 - 1.50 |
Mn (Manganese) | 0.20 - 0.50 |
Si (Silicon) | 0.20 - 0.50 |
P (Phosphorus) | ≤ 0.030 |
S (Sulfur) | ≤ 0.030 |
The primary role of the key alloying elements in CPM 10V is as follows:
- Vanadium (V): Enhances wear resistance through the formation of hard carbides.
- Chromium (Cr): Improves hardness and corrosion resistance.
- Molybdenum (Mo): Increases toughness and helps maintain hardness at elevated temperatures.
Mechanical Properties
Property | Condition/Temper | Test Temperature | Typical Value/Range (Metric) | Typical Value/Range (Imperial) | Reference Standard for Test Method |
---|---|---|---|---|---|
Tensile Strength | Quenched & Tempered | Room Temp | 2100 - 2300 MPa | 305 - 335 ksi | ASTM E8 |
Yield Strength (0.2% offset) | Quenched & Tempered | Room Temp | 1800 - 2000 MPa | 261 - 290 ksi | ASTM E8 |
Elongation | Quenched & Tempered | Room Temp | 3 - 5% | 3 - 5% | ASTM E8 |
Hardness (HRC) | Quenched & Tempered | Room Temp | 58 - 62 HRC | 58 - 62 HRC | ASTM E18 |
Impact Strength (Charpy) | Quenched & Tempered | -20 °C | 20 - 30 J | 15 - 22 ft-lbf | ASTM E23 |
The combination of high tensile and yield strength, along with excellent hardness, makes CPM 10V suitable for applications requiring high mechanical loading and structural integrity, such as cutting tools and dies.
Physical Properties
Property | Condition/Temperature | Value (Metric) | Value (Imperial) |
---|---|---|---|
Density | Room Temp | 7.85 g/cm³ | 0.284 lb/in³ |
Melting Point/Range | - | 1420 - 1450 °C | 2590 - 2640 °F |
Thermal Conductivity | Room Temp | 25 W/m·K | 14.5 BTU·in/h·ft²·°F |
Specific Heat Capacity | Room Temp | 460 J/kg·K | 0.11 BTU/lb·°F |
Electrical Resistivity | Room Temp | 0.00001 Ω·m | 0.00001 Ω·in |
The density and melting point of CPM 10V indicate its robustness, while its thermal conductivity and specific heat capacity are crucial for applications involving thermal cycling or heat treatment processes.
Corrosion Resistance
Corrosive Agent | Concentration (%) | Temperature (°C) | Resistance Rating | Notes |
---|---|---|---|---|
Chlorides | 3 - 10 | 20 - 60 | Fair | Risk of pitting corrosion |
Acids | 1 - 5 | 20 - 40 | Poor | Not recommended |
Alkaline Solutions | 1 - 10 | 20 - 60 | Fair | Susceptible to stress corrosion cracking |
Atmospheric | - | - | Good | Performs well in dry conditions |
CPM 10V exhibits moderate corrosion resistance, particularly in atmospheric conditions. However, it is susceptible to pitting in chloride environments and should be avoided in acidic or highly alkaline conditions. Compared to other tool steels like D2, which has lower corrosion resistance, CPM 10V performs better in applications where wear resistance is critical, but care must be taken in corrosive environments.
Heat Resistance
Property/Limit | Temperature (°C) | Temperature (°F) | Remarks |
---|---|---|---|
Max Continuous Service Temp | 400 °C | 752 °F | Suitable for high-temperature applications |
Max Intermittent Service Temp | 500 °C | 932 °F | Short-term exposure only |
Scaling Temperature | 600 °C | 1112 °F | Risk of oxidation beyond this point |
Creep Strength considerations | 400 °C | 752 °F | Creep resistance begins to decline |
At elevated temperatures, CPM 10V maintains its hardness and wear resistance, but oxidation can become a concern if not properly protected. The steel's performance in high-temperature applications is generally good, making it suitable for hot work tooling.
Fabrication Properties
Weldability
Welding Process | Recommended Filler Metal (AWS Classification) | Typical Shielding Gas/Flux | Notes |
---|---|---|---|
TIG | ER80S-D2 | Argon | Preheat recommended |
MIG | ER80S-D2 | Argon + CO2 mix | Requires post-weld heat treatment |
Stick | E7018 | - | Not recommended for thick sections |
Welding CPM 10V can be challenging due to its high hardness. Preheating is often recommended to reduce the risk of cracking, and post-weld heat treatment is essential to restore toughness.
Machinability
Machining Parameter | CPM 10V | AISI 1212 | Notes/Tips |
---|---|---|---|
Relative Machinability Index | 50 | 100 | More difficult to machine |
Typical Cutting Speed (m/min) | 15 - 25 | 40 - 60 | Use carbide tools for best results |
Machining CPM 10V requires specialized tools and techniques due to its hardness. Carbide tooling is recommended, and slower cutting speeds may be necessary to achieve optimal results.
Formability
CPM 10V is not particularly suited for forming operations due to its high hardness and brittleness. Cold forming is generally not recommended, while hot forming may be possible with careful control of temperature and strain rates.
Heat Treatment
Treatment Process | Temperature Range (°C) | Typical Soaking Time | Cooling Method | Primary Purpose / Expected Result |
---|---|---|---|---|
Annealing | 800 - 850 | 1 - 2 hours | Air | Reduce hardness, improve machinability |
Hardening | 1000 - 1100 | 30 - 60 minutes | Oil/Water | Achieve maximum hardness |
Tempering | 500 - 600 | 1 hour | Air | Reduce brittleness, enhance toughness |
The heat treatment process significantly affects the microstructure of CPM 10V, transforming it into a martensitic structure that provides its characteristic hardness and wear resistance. Proper heat treatment is crucial for achieving the desired balance of hardness and toughness.
Typical Applications and End Uses
Industry/Sector | Specific Application Example | Key Steel Properties Utilized in this Application | Reason for Selection |
---|---|---|---|
Tool Manufacturing | Cutting Tools | High wear resistance, toughness | Long-lasting edge retention |
Aerospace | Aircraft Components | High strength-to-weight ratio | Durability under stress |
Automotive | Engine Components | High-temperature performance | Reliability in harsh conditions |
Medical Devices | Surgical Instruments | Corrosion resistance, sharpness | Precision and safety |
Other applications include:
* Knives and blades for industrial use
* Dies and molds for metal forming
* High-performance wear parts in machinery
CPM 10V is chosen for these applications due to its unique combination of hardness, wear resistance, and toughness, making it ideal for tools that require prolonged use under demanding conditions.
Important Considerations, Selection Criteria, and Further Insights
Feature/Property | CPM 10V | AISI D2 | M2 Tool Steel | Brief Pro/Con or Trade-off Note |
---|---|---|---|---|
Key Mechanical Property | High hardness | Good wear resistance | High toughness | CPM 10V offers superior wear resistance |
Key Corrosion Aspect | Moderate | Fair | Poor | CPM 10V performs better in corrosive environments |
Weldability | Challenging | Moderate | Good | Requires preheat and post-weld treatment |
Machinability | Difficult | Moderate | Good | CPM 10V is harder to machine than D2 |
Formability | Poor | Fair | Good | Limited forming capability |
Approx. Relative Cost | High | Moderate | Moderate | Higher cost due to advanced processing |
Typical Availability | Moderate | High | High | CPM 10V may be less readily available |
When selecting CPM 10V, considerations include its cost-effectiveness for specific applications, availability in the market, and the need for specialized machining and welding techniques. Its unique properties make it suitable for niche applications where performance is critical, despite the challenges in fabrication and higher costs compared to other tool steels.
In summary, CPM 10V steel is a high-performance tool steel that excels in wear resistance and toughness, making it ideal for demanding applications in various industries. Its advanced properties, however, come with challenges in machining and welding, necessitating careful consideration during the selection process.