446 Stainless Steel: Properties and Key Applications

Table Of Content

Table Of Content

446 stainless steel is classified as an austenitic stainless steel, notable for its high chromium content and the addition of molybdenum, which enhances its resistance to oxidation and corrosion. This steel grade is primarily composed of chromium (24-27%) and nickel (19-22%), with molybdenum (up to 1.5%) as a significant alloying element. The high chromium content provides excellent resistance to oxidation and high-temperature environments, while nickel contributes to its toughness and ductility.

Comprehensive Overview

446 stainless steel is particularly recognized for its exceptional high-temperature strength and oxidation resistance, making it suitable for applications in environments where other stainless steels may fail. Its ability to maintain mechanical properties at elevated temperatures, combined with good weldability and formability, makes it a preferred choice in various industrial applications, especially in the petrochemical and power generation sectors.

Advantages:
- High-Temperature Resistance: Capable of withstanding temperatures up to 1200°C (2192°F) without significant degradation.
- Corrosion Resistance: Excellent resistance to oxidation and scaling in high-temperature environments.
- Durability: Good mechanical properties, including strength and ductility, contribute to its longevity in service.

Limitations:
- Cost: Higher alloy content can lead to increased material costs compared to lower-grade stainless steels.
- Weldability Challenges: While it can be welded, care must be taken to avoid issues such as hot cracking.
- Limited Availability: Not as commonly stocked as other stainless steel grades, which may affect lead times.

446 stainless steel has a strong market position in specialized applications, particularly where high-temperature performance is critical. Its historical significance lies in its development for use in furnace components, heat exchangers, and other high-temperature applications.

Alternative Names, Standards, and Equivalents

Standard Organization Designation/Grade Country/Region of Origin Notes/Remarks
UNS S44600 USA Closest equivalent to EN 1.4762
AISI/SAE 446 USA Commonly used designation
ASTM A240 USA Standard specification for stainless steel plates
EN 1.4762 Europe Minor compositional differences to be aware of
JIS SUS446 Japan Equivalent grade with similar properties
GB 00Cr25Ni20 China Comparable grade with slight variations

The differences between these equivalent grades often lie in minor compositional variations that can affect performance in specific environments. For instance, while both UNS S44600 and EN 1.4762 offer similar high-temperature resistance, the specific alloying elements and their percentages can influence corrosion resistance and mechanical properties.

Key Properties

Chemical Composition

Element (Symbol and Name) Percentage Range (%)
Cr (Chromium) 24.0 - 27.0
Ni (Nickel) 19.0 - 22.0
Mo (Molybdenum) 0.5 - 1.5
C (Carbon) ≤ 0.03
Mn (Manganese) ≤ 1.0
Si (Silicon) ≤ 1.0
P (Phosphorus) ≤ 0.045
S (Sulfur) ≤ 0.03

The primary role of chromium in 446 stainless steel is to enhance corrosion resistance and oxidation resistance at elevated temperatures. Nickel contributes to the steel's toughness and ductility, while molybdenum improves resistance to pitting and crevice corrosion, particularly in chloride environments.

Mechanical Properties

Property Condition/Temper Typical Value/Range (Metric - SI Units) Typical Value/Range (Imperial Units) Reference Standard for Test Method
Tensile Strength Annealed 515 - 690 MPa 75 - 100 ksi ASTM E8
Yield Strength (0.2% offset) Annealed 205 - 310 MPa 30 - 45 ksi ASTM E8
Elongation Annealed 40 - 50% 40 - 50% ASTM E8
Hardness (Rockwell B) Annealed 85 - 95 HRB 85 - 95 HRB ASTM E18
Impact Strength (Charpy V-notch) -20°C 40 J 30 ft-lbf ASTM E23

The combination of high tensile and yield strength, along with good elongation, makes 446 stainless steel suitable for applications that require structural integrity under mechanical loading. Its impact strength at low temperatures also ensures reliability in colder environments.

Physical Properties

Property Condition/Temperature Value (Metric - SI Units) Value (Imperial Units)
Density Room Temperature 7.8 g/cm³ 0.283 lb/in³
Melting Point/Range - 1400 - 1450 °C 2552 - 2642 °F
Thermal Conductivity Room Temperature 25 W/m·K 17.3 BTU·in/(hr·ft²·°F)
Specific Heat Capacity Room Temperature 500 J/kg·K 0.119 BTU/lb·°F
Electrical Resistivity Room Temperature 0.73 µΩ·m 0.0000013 Ω·in
Coefficient of Thermal Expansion 20 - 100 °C 16.5 x 10⁻⁶ /K 9.2 x 10⁻⁶ /°F

The density of 446 stainless steel indicates its robustness, while its melting point signifies its suitability for high-temperature applications. The thermal conductivity and specific heat capacity are critical for applications involving heat exchangers, where efficient heat transfer is essential.

Corrosion Resistance

Corrosive Agent Concentration (%) Temperature (°C/°F) Resistance Rating Notes
Sulfuric Acid 10-20 25/77 Fair Risk of pitting
Chlorides 3-5 60/140 Good Susceptible to pitting
Sea Water - 25/77 Excellent Good resistance
Hydrochloric Acid 5-10 25/77 Poor Not recommended

446 stainless steel exhibits excellent resistance to various corrosive environments, particularly in high-temperature applications. Its performance in chloride-rich environments is noteworthy, although it is susceptible to pitting corrosion. Compared to grades like 304 and 316 stainless steel, 446 offers superior oxidation resistance but may not perform as well in reducing environments or in the presence of strong acids.

Heat Resistance

Property/Limit Temperature (°C) Temperature (°F) Remarks
Max Continuous Service Temp 1200 2192 Optimal for high-temperature applications
Max Intermittent Service Temp 1300 2372 Short-term exposure only
Scaling Temperature 1150 2102 Begins to oxidize significantly
Creep Strength Considerations Begin 800 1472 Creep may become a concern

446 stainless steel maintains its mechanical properties at elevated temperatures, making it ideal for applications such as furnace components and heat exchangers. Its oxidation resistance allows it to perform well in environments where other steels may fail due to scaling or oxidation.

Fabrication Properties

Weldability

Welding Process Recommended Filler Metal (AWS Classification) Typical Shielding Gas/Flux Notes
TIG ER446 Argon Preheat recommended
MIG ER446 Argon + 2% O₂ Good for thin sections
Stick E446 - Requires careful control

Weldability of 446 stainless steel is generally good, but it requires careful attention to avoid hot cracking. Preheating before welding can help mitigate this risk, and post-weld heat treatment may be necessary to relieve stresses.

Machinability

Machining Parameter [446 Stainless Steel] Benchmark Steel (AISI 1212) Notes/Tips
Relative Machinability Index 30% 100% Requires slower speeds
Typical Cutting Speed (Turning) 20 m/min 60 m/min Use carbide tools

Machinability of 446 stainless steel is lower than that of more common grades like AISI 1212. It is advisable to use carbide tooling and slower cutting speeds to achieve optimal results.

Formability

446 stainless steel exhibits moderate formability. Cold forming is possible, but care must be taken to avoid work hardening. Hot forming is preferred for complex shapes, and recommended bend radii should be adhered to in fabrication.

Heat Treatment

Treatment Process Temperature Range (°C/°F) Typical Soaking Time Cooling Method Primary Purpose / Expected Result
Annealing 1050 - 1150 / 1922 - 2102 1 - 2 hours Air Relieve stresses, improve ductility
Solution Treatment 1000 - 1100 / 1832 - 2012 1 hour Water Enhance corrosion resistance

During heat treatment, 446 stainless steel undergoes metallurgical transformations that enhance its microstructure, improving its mechanical properties and corrosion resistance.

Typical Applications and End Uses

Industry/Sector Specific Application Example Key Steel Properties Utilized in this Application Reason for Selection (Brief)
Power Generation Boiler Tubes High-temperature strength, oxidation resistance Essential for high-efficiency systems
Petrochemical Furnace Components Corrosion resistance, durability Critical for long-term operation
Aerospace Exhaust Systems High-temperature performance Required for extreme conditions

Other applications include:
* Heat exchangers
* Industrial furnaces
* Chemical processing equipment

The selection of 446 stainless steel for these applications is primarily due to its ability to withstand high temperatures and corrosive environments, ensuring reliability and longevity.

Important Considerations, Selection Criteria, and Further Insights

Feature/Property 446 Stainless Steel 304 Stainless Steel 316 Stainless Steel Brief Pro/Con or Trade-off Note
Key Mechanical Property High tensile strength Moderate tensile strength Moderate tensile strength 446 offers superior high-temp performance
Key Corrosion Aspect Excellent oxidation resistance Good general corrosion resistance Better resistance to chlorides 446 is less effective in reducing environments
Weldability Moderate Good Good 446 requires more care during welding
Machinability Moderate Good Good 446 is harder to machine than 304/316
Formability Moderate Good Good 446 is less formable than 304/316
Approx. Relative Cost Higher Lower Moderate Cost can be a deciding factor in selection
Typical Availability Limited Widely available Widely available Availability may affect project timelines

When selecting 446 stainless steel, considerations such as cost-effectiveness, availability, and specific application requirements must be taken into account. Its unique properties make it suitable for niche applications where high-temperature performance is critical, but its higher cost and limited availability may necessitate careful planning and sourcing strategies.

In summary, 446 stainless steel is a high-performance material that excels in demanding environments, making it a valuable choice for industries requiring durability and reliability under extreme conditions.


Data Sources & Verification

Chemical composition and mechanical property values on this page are compiled from published material standards and cross-referenced against the equivalent designations listed above (UNS S44600, ASTM A240, EN 1.4762, JIS SUS446, GB 00Cr25Ni20). Values are typical or nominal and vary with product form, thickness, and heat treatment; confirm against the governing standard and mill test certificate before design or procurement use.

Design tools: Working with this grade structurally? Use our free Load Capacity Calculator, Span Calculator, and Steel Beam Calculator. Estimate material weight with our steel weight calculators.

Technically reviewed by Dr. Zhang Zhiwei — former Senior Technical Specialist, Baosteel Group; member, Chinese Society for Metals. How we compile our data · spotted an error? Tell us and we will review it.

Back to blog

12 comments

“Great article on 446 stainless steel! The high chromium content makes it particularly interesting for high-temperature applications. I’m currently researching materials for an industrial furnace project – does anyone have experience with its weldability compared to 304L grades?

Also, for those working with specialized industrial materials marketing, I came across this performance marketing agency https://collaba.digital/performance-agency that seems to focus on technical B2B sectors. Has anyone worked with them for promoting niche steel products? Would be curious to hear about real-world experiences with both the material and marketing such specialized industrial offerings."

Henry

“Great article on 446 stainless steel! The high-temperature resistance properties are particularly impressive. I’m currently researching materials for an industrial furnace project and this seems like a perfect fit. Does anyone have experience with sourcing this grade in Europe?

Also, for those considering marketing strategies for similar industrial products, I found this comprehensive guide on digital marketing approaches quite helpful: https://collaba.digital/compleksny_marketing_agency. They seem to specialize in technical industries – has anyone worked with them before? Would be curious to hear about real-world experiences with both the material and marketing such specialized products."

Matt

Leave a comment