320 Stainless Steel: Properties and Key Applications

Table Of Content

Table Of Content

320 Stainless Steel is classified as an austenitic stainless steel, primarily composed of iron, chromium, and nickel, with a low carbon content. This specific grade typically contains around 18% chromium and 8% nickel, which contribute significantly to its corrosion resistance and mechanical properties. The low carbon content enhances its weldability and reduces the risk of carbide precipitation during welding, making it suitable for various applications in industries where high corrosion resistance and formability are essential.

Comprehensive Overview

320 Stainless Steel is known for its excellent resistance to oxidation and corrosion, particularly in high-temperature environments. Its austenitic structure provides good ductility and toughness, making it a preferred choice for applications that require both strength and flexibility. The primary alloying elements, chromium and nickel, play crucial roles in enhancing the steel's resistance to corrosive environments, while the low carbon content minimizes the risk of intergranular corrosion.

Advantages:
- Corrosion Resistance: Exceptional resistance to a wide range of corrosive environments, including acidic and alkaline conditions.
- High-Temperature Stability: Maintains strength and oxidation resistance at elevated temperatures.
- Weldability: Low carbon content allows for easy welding without significant risk of weld decay.

Limitations:
- Cost: Generally more expensive than carbon steels due to alloying elements.
- Work Hardening: Can become hard and brittle when subjected to extensive cold working, which may require careful handling during fabrication.

Historically, 320 Stainless Steel has been utilized in various applications, particularly in the food processing, chemical, and petrochemical industries, where its unique properties are highly valued. Its market position is strong, with a consistent demand for its use in environments that challenge other materials.

Alternative Names, Standards, and Equivalents

Standard Organization Designation/Grade Country/Region of Origin Notes/Remarks
UNS S32000 USA Closest equivalent to AISI 304 with minor compositional differences.
AISI/SAE 320 USA Similar to 316 but with different alloying elements.
ASTM A240 USA Standard specification for stainless steel plates.
EN 1.4301 Europe Equivalent to AISI 304, but with different mechanical properties.
JIS SUS 304 Japan Closely related, with similar corrosion resistance.

The subtle differences between these grades can significantly affect performance in specific applications. For instance, while 320 and 304 stainless steels share many properties, 320's enhanced resistance to certain corrosive agents makes it more suitable for specific environments.

Key Properties

Chemical Composition

Element (Symbol and Name) Percentage Range (%)
Fe (Iron) Balance
Cr (Chromium) 18.0 - 20.0
Ni (Nickel) 8.0 - 10.0
C (Carbon) ≤ 0.08
Mn (Manganese) 2.0 - 2.5
Si (Silicon) ≤ 1.0

The primary alloying elements in 320 Stainless Steel include chromium, which enhances corrosion resistance and oxidation stability, and nickel, which contributes to its toughness and ductility. The low carbon content is crucial for maintaining the steel's weldability and preventing carbide precipitation, which can lead to intergranular corrosion.

Mechanical Properties

Property Condition/Temper Typical Value/Range (Metric - SI Units) Typical Value/Range (Imperial Units) Reference Standard for Test Method
Tensile Strength Annealed 520 - 720 MPa 75 - 104 ksi ASTM E8
Yield Strength (0.2% offset) Annealed 205 - 310 MPa 30 - 45 ksi ASTM E8
Elongation Annealed 40 - 50% 40 - 50% ASTM E8
Hardness Annealed 160 - 190 HB 90 - 100 HB ASTM E10
Impact Strength -40°C 40 J 30 ft-lbf ASTM E23

The mechanical properties of 320 Stainless Steel make it suitable for applications requiring high strength and ductility. Its tensile strength and yield strength indicate its ability to withstand significant loads, while its elongation percentage reflects its capacity for deformation without fracture, making it ideal for structural applications.

Physical Properties

Property Condition/Temperature Value (Metric - SI Units) Value (Imperial Units)
Density - 7.93 g/cm³ 0.286 lb/in³
Melting Point/Range - 1400 - 1450 °C 2552 - 2642 °F
Thermal Conductivity 20°C 16 W/m·K 92 BTU·in/(hr·ft²·°F)
Specific Heat Capacity 20°C 500 J/kg·K 0.12 BTU/lb·°F
Electrical Resistivity 20°C 0.73 µΩ·m 0.0000013 Ω·in

The density of 320 Stainless Steel indicates its substantial mass, which contributes to its strength. Its thermal conductivity is moderate, making it suitable for applications where heat transfer is necessary but not excessive. The specific heat capacity is relatively high, allowing it to absorb and retain heat, which is beneficial in high-temperature applications.

Corrosion Resistance

Corrosive Agent Concentration (%) Temperature (°C/°F) Resistance Rating Notes
Chlorides 3-10 20-60 / 68-140 Good Risk of pitting corrosion.
Sulfuric Acid 10-30 20-50 / 68-122 Fair Susceptible to stress corrosion cracking.
Acetic Acid 5-20 20-60 / 68-140 Good Generally resistant.
Alkaline Solutions 5-30 20-60 / 68-140 Excellent Very resistant.

320 Stainless Steel exhibits excellent resistance to a variety of corrosive environments, particularly in alkaline solutions and organic acids. However, it is susceptible to pitting corrosion in chloride environments and stress corrosion cracking in sulfuric acid. Compared to 316 stainless steel, which has molybdenum added for enhanced pitting resistance, 320 may not perform as well in chloride-rich environments but offers better resistance in alkaline conditions.

Heat Resistance

Property/Limit Temperature (°C) Temperature (°F) Remarks
Max Continuous Service Temp 800 1472 Suitable for high-temperature applications.
Max Intermittent Service Temp 900 1652 Can withstand short-term exposure to higher temperatures.
Scaling Temperature 1000 1832 Begins to oxidize significantly above this temperature.

At elevated temperatures, 320 Stainless Steel maintains its strength and oxidation resistance, making it suitable for applications in high-temperature environments. However, prolonged exposure to temperatures above 800 °C (1472 °F) can lead to oxidation and scaling, which may compromise its structural integrity.

Fabrication Properties

Weldability

Welding Process Recommended Filler Metal (AWS Classification) Typical Shielding Gas/Flux Notes
TIG ER308L Argon Excellent for thin sections.
MIG ER308L Argon + CO2 Good for thicker sections.
Stick E308L - Suitable for outdoor applications.

320 Stainless Steel is highly weldable due to its low carbon content, which minimizes the risk of carbide precipitation during welding. Pre-heat treatment is generally not required, but post-weld heat treatment may be beneficial to relieve stresses and improve corrosion resistance.

Machinability

Machining Parameter 320 Stainless Steel AISI 1212 Notes/Tips
Relative Machinability Index 40 100 More challenging to machine.
Typical Cutting Speed (Turning) 25 m/min 50 m/min Use carbide tools for best results.

Machining 320 Stainless Steel can be more challenging compared to carbon steels due to its work hardening characteristics. It is advisable to use high-speed steel or carbide tools and to maintain adequate cutting speeds and coolant application to prevent overheating.

Formability

320 Stainless Steel exhibits good formability, allowing for cold and hot forming processes. However, it is essential to consider the work hardening effect during cold forming, which may require additional force and can lead to reduced ductility. The minimum bend radius should be carefully calculated to avoid cracking.

Heat Treatment

Treatment Process Temperature Range (°C/°F) Typical Soaking Time Cooling Method Primary Purpose / Expected Result
Annealing 1000 - 1100 / 1832 - 2012 1 - 2 hours Air Relieve stresses and improve ductility.
Solution Treatment 1000 - 1100 / 1832 - 2012 30 minutes Water Dissolve carbides and improve corrosion resistance.

Heat treatment processes such as annealing and solution treatment are critical for optimizing the microstructure of 320 Stainless Steel. These treatments enhance ductility and corrosion resistance by dissolving carbides and relieving internal stresses.

Typical Applications and End Uses

Industry/Sector Specific Application Example Key Steel Properties Utilized in this Application Reason for Selection (Brief)
Food Processing Equipment and piping Corrosion resistance, ease of cleaning Hygiene and durability
Chemical Processing Reactors and storage tanks High-temperature stability, corrosion resistance Safety and longevity
Oil and Gas Pipeline components Strength, weldability, and corrosion resistance Reliability in harsh environments

Other applications include:
- Pharmaceutical equipment
- Marine environments
- Architectural structures

The selection of 320 Stainless Steel for these applications is primarily due to its excellent corrosion resistance and mechanical properties, which ensure safety and longevity in demanding environments.

Important Considerations, Selection Criteria, and Further Insights

Feature/Property 320 Stainless Steel AISI 316 Stainless Steel AISI 304 Stainless Steel Brief Pro/Con or Trade-off Note
Key Mechanical Property High tensile strength Excellent corrosion resistance Good ductility 320 offers a balance of strength and corrosion resistance.
Key Corrosion Aspect Good in alkaline solutions Best in chloride environments Moderate resistance 316 is superior in chloride environments.
Weldability Excellent Good Good All grades are weldable, but 320 has an edge due to low carbon.
Machinability Moderate Good Excellent 320 is harder to machine than 304 and 316.
Approx. Relative Cost Moderate Higher Lower 320 is generally more cost-effective than 316.
Typical Availability Moderate High High 304 is the most commonly available stainless steel.

When selecting 320 Stainless Steel, considerations include its cost-effectiveness, availability, and specific performance requirements in corrosive environments. Its unique properties make it suitable for niche applications where other grades may not perform as well. Additionally, safety considerations in high-stress environments must be taken into account, ensuring that the selected material meets all regulatory and performance standards.


Data Sources & Verification

Chemical composition and mechanical property values on this page are compiled from published material standards and cross-referenced against the equivalent designations listed above (UNS S32000, ASTM A240, EN 1.4301, JIS SUS 304). Values are typical or nominal and vary with product form, thickness, and heat treatment; confirm against the governing standard and mill test certificate before design or procurement use.

Design tools: Working with this grade structurally? Use our free Load Capacity Calculator, Span Calculator, and Steel Beam Calculator. Estimate material weight with our steel weight calculators.

Technically reviewed by Dr. Zhang Zhiwei — former Senior Technical Specialist, Baosteel Group; member, Chinese Society for Metals. How we compile our data · spotted an error? Tell us and we will review it.

Back to blog

1 comment

Thanks for the detailed breakdown of the 320 grade properties. I’m currently evaluating this specific steel for a food processing project we’re looking to launch in Spain, as the alkaline resistance you mentioned is exactly what we need for our cleaning protocols. Since we are in the early stages of setting up our local operations and navigating the bureaucracy, I was wondering if you have any insights on how the current supply chain for 320 stainless plate looks in the Catalonia region? Also, for our foreign engineering team coming over to oversee the installation, we’ve been looking into the administrative requirements like https://e-residence.com/fr/nie-spain-online/barcelona/ to get everything compliant — do you happen to know if there are specific industry-related permits required for international contractors working with high-pressure vessel steel in that area?

Deez

Leave a comment