316LN Stainless Steel: Properties and Key Applications
Share
Table Of Content
Table Of Content
316LN stainless steel is a low-carbon, nitrogen-enhanced version of the 316 stainless steel grade, classified as an austenitic stainless steel. It is primarily composed of iron, chromium, nickel, and molybdenum, with the addition of nitrogen to enhance its mechanical properties. The typical composition of 316LN includes approximately 16-18% chromium, 10-14% nickel, and 2-3% molybdenum, with nitrogen levels around 0.1-0.2%. This unique combination of alloying elements contributes to its excellent corrosion resistance, high strength, and good weldability.
Characteristics and Properties
316LN stainless steel is known for its superior resistance to pitting and crevice corrosion, especially in chloride environments. Its low carbon content minimizes the risk of carbide precipitation during welding, making it suitable for applications requiring high strength and corrosion resistance. The addition of nitrogen improves tensile strength and yield strength, making it a preferred choice in demanding applications.
Advantages (Pros):
- Excellent corrosion resistance, particularly in marine and chemical environments.
- High strength and toughness at elevated temperatures.
- Good weldability and formability.
- Low risk of sensitization due to low carbon content.
Limitations (Cons):
- Higher cost compared to standard stainless steels.
- Not as readily available as more common grades like 304 or 316.
- Limited resistance to certain reducing acids.
Historically, 316LN has been significant in industries such as petrochemical, marine, and pharmaceutical, where its corrosion resistance and mechanical properties are critical.
Alternative Names, Standards, and Equivalents
| Standard Organization | Designation/Grade | Country/Region of Origin | Notes/Remarks |
|---|---|---|---|
| UNS | S31653 | USA | Closest equivalent to 316L with enhanced nitrogen content. |
| AISI/SAE | 316LN | USA | Low carbon variant of 316 with improved strength. |
| ASTM | A240/A240M | USA | Standard specification for chromium and chromium-nickel stainless steel plates. |
| EN | 1.4406 | Europe | Equivalent to 316LN with similar properties. |
| JIS | SUS316LN | Japan | Japanese standard equivalent with minor compositional differences. |
The differences between 316LN and its equivalents often lie in the nitrogen content and specific mechanical properties, which can affect performance in certain applications. For instance, while 316L is known for its excellent weldability, 316LN offers enhanced strength, making it more suitable for high-stress environments.
Key Properties
Chemical Composition
| Element (Symbol and Name) | Percentage Range (%) |
|---|---|
| Fe (Iron) | Balance |
| Cr (Chromium) | 16.0 - 18.0 |
| Ni (Nickel) | 10.0 - 14.0 |
| Mo (Molybdenum) | 2.0 - 3.0 |
| N (Nitrogen) | 0.1 - 0.2 |
| C (Carbon) | ≤ 0.03 |
The primary role of chromium is to enhance corrosion resistance, while nickel improves toughness and ductility. Molybdenum provides additional resistance to pitting and crevice corrosion, particularly in chloride environments. Nitrogen enhances strength and improves resistance to stress corrosion cracking.
Mechanical Properties
| Property | Condition/Temper | Typical Value/Range (Metric) | Typical Value/Range (Imperial) | Reference Standard for Test Method |
|---|---|---|---|---|
| Tensile Strength | Annealed | 520 - 720 MPa | 75 - 104 ksi | ASTM E8 |
| Yield Strength (0.2% offset) | Annealed | 205 - 310 MPa | 30 - 45 ksi | ASTM E8 |
| Elongation | Annealed | 40 - 50% | 40 - 50% | ASTM E8 |
| Hardness (Rockwell B) | Annealed | 70 - 90 HRB | 70 - 90 HRB | ASTM E18 |
| Impact Strength | -20°C | 40 J | 29.5 ft-lbf | ASTM E23 |
The combination of high tensile and yield strength, along with good elongation, makes 316LN suitable for applications requiring structural integrity under mechanical loading. Its impact strength at low temperatures ensures performance in cryogenic environments.
Physical Properties
| Property | Condition/Temperature | Value (Metric) | Value (Imperial) |
|---|---|---|---|
| Density | Room Temperature | 8.0 g/cm³ | 0.289 lb/in³ |
| Melting Point/Range | - | 1375 - 1400 °C | 2500 - 2550 °F |
| Thermal Conductivity | Room Temperature | 16 W/m·K | 92 BTU·in/ft²·h·°F |
| Specific Heat Capacity | Room Temperature | 500 J/kg·K | 0.12 BTU/lb·°F |
| Electrical Resistivity | Room Temperature | 0.72 µΩ·m | 0.00000072 Ω·m |
| Coefficient of Thermal Expansion | 20 - 100 °C | 16.0 x 10⁻⁶ /K | 8.9 x 10⁻⁶ /°F |
The density and melting point indicate that 316LN can withstand high-temperature applications, while its thermal conductivity and specific heat capacity make it suitable for heat exchangers. The low electrical resistivity is beneficial in applications requiring electrical conductivity.
Corrosion Resistance
| Corrosive Agent | Concentration (%) | Temperature (°C/°F) | Resistance Rating | Notes |
|---|---|---|---|---|
| Chlorides | 3-10% | 20-60°C / 68-140°F | Excellent | Risk of pitting corrosion. |
| Sulfuric Acid | 10-20% | 20-50°C / 68-122°F | Good | Limited resistance, especially at higher temperatures. |
| Hydrochloric Acid | 5-10% | 20-40°C / 68-104°F | Fair | Not recommended for prolonged exposure. |
| Sea Water | - | Ambient | Excellent | Highly resistant to marine environments. |
316LN exhibits excellent resistance to a variety of corrosive agents, particularly in marine environments where chlorides are prevalent. However, it is less resistant to strong acids like hydrochloric acid, where alternative materials may be more suitable. Compared to 304 and 316 stainless steels, 316LN offers superior resistance to pitting and stress corrosion cracking, making it a preferred choice in aggressive environments.
Heat Resistance
| Property/Limit | Temperature (°C) | Temperature (°F) | Remarks |
|---|---|---|---|
| Max Continuous Service Temp | 925 °C | 1700 °F | Suitable for high-temperature applications. |
| Max Intermittent Service Temp | 870 °C | 1600 °F | Can withstand short-term exposure to higher temperatures. |
| Scaling Temperature | 800 °C | 1470 °F | Risk of oxidation above this temperature. |
| Creep Strength considerations | 600 °C | 1112 °F | Creep resistance begins to decline above this temperature. |
316LN maintains its strength and corrosion resistance at elevated temperatures, making it suitable for applications such as heat exchangers and pressure vessels. However, care must be taken to avoid oxidation and scaling at high temperatures.
Fabrication Properties
Weldability
| Welding Process | Recommended Filler Metal (AWS Classification) | Typical Shielding Gas/Flux | Notes |
|---|---|---|---|
| TIG | ER316L | Argon | Excellent for thin sections. |
| MIG | ER316L | Argon + 2% CO2 | Good for thicker sections. |
| SMAW | E316L | - | Suitable for field applications. |
316LN is highly weldable, with the recommended filler metals ensuring compatibility and maintaining corrosion resistance. Pre- and post-weld heat treatments are often not necessary due to its low carbon content, reducing the risk of sensitization.
Machinability
| Machining Parameter | 316LN | AISI 1212 | Notes/Tips |
|---|---|---|---|
| Relative Machinability Index | 45% | 100% | 316LN is more challenging to machine. |
| Typical Cutting Speed (Turning) | 25-30 m/min | 50-60 m/min | Use carbide tools for best results. |
Machining 316LN requires careful consideration of cutting speeds and tooling due to its work-hardening characteristics. Carbide tools are recommended to achieve optimal results.
Formability
316LN exhibits good formability, allowing for cold and hot forming processes. However, it is important to note that excessive cold working can lead to increased hardness and reduced ductility. Recommended bend radii should be adhered to in order to prevent cracking during forming operations.
Heat Treatment
| Treatment Process | Temperature Range (°C/°F) | Typical Soaking Time | Cooling Method | Primary Purpose / Expected Result |
|---|---|---|---|---|
| Solution Annealing | 1000 - 1100 °C / 1832 - 2012 °F | 30 minutes | Air or Water | Dissolve carbides, improve corrosion resistance. |
| Stress Relief | 400 - 600 °C / 752 - 1112 °F | 1 hour | Air | Reduce residual stresses. |
During heat treatment, 316LN undergoes metallurgical transformations that enhance its microstructure, improving its mechanical properties and corrosion resistance. Solution annealing is particularly effective in restoring ductility after cold working.
Typical Applications and End Uses
| Industry/Sector | Specific Application Example | Key Steel Properties Utilized in this Application | Reason for Selection (Brief) |
|---|---|---|---|
| Marine | Shipbuilding | Corrosion resistance, strength | Exposure to seawater. |
| Chemical | Process piping | Corrosion resistance, weldability | Handling aggressive chemicals. |
| Pharmaceutical | Equipment fabrication | Cleanliness, corrosion resistance | Compliance with sanitary standards. |
| Oil & Gas | Offshore platforms | Strength, toughness, corrosion resistance | Harsh environmental conditions. |
Other applications include:
* Food processing equipment
* Heat exchangers
* Pressure vessels
* Valves and fittings
316LN is chosen for these applications due to its excellent corrosion resistance and mechanical properties, which are critical in environments where hygiene and structural integrity are paramount.
Important Considerations, Selection Criteria, and Further Insights
| Feature/Property | 316LN | 304 | 321 | Brief Pro/Con or Trade-off Note |
|---|---|---|---|---|
| Key Mechanical Property | High strength | Moderate strength | High strength | 316LN offers better corrosion resistance than 304. |
| Key Corrosion Aspect | Excellent | Good | Good | 316LN is superior in chloride environments. |
| Weldability | Good | Excellent | Good | 316LN requires careful welding practices. |
| Machinability | Moderate | Good | Moderate | 316LN is harder to machine than 304. |
| Formability | Good | Excellent | Good | 316LN has slightly reduced formability. |
| Approx. Relative Cost | Higher | Lower | Higher | Cost considerations may affect selection. |
| Typical Availability | Moderate | High | Moderate | 304 is more commonly available. |
When selecting 316LN, considerations include cost-effectiveness, availability, and specific application requirements. Its unique properties make it suitable for niche applications where performance is critical, despite its higher cost compared to more common grades like 304. Additionally, its low magnetic permeability makes it suitable for applications in sensitive environments.
In conclusion, 316LN stainless steel is a versatile and high-performance material that excels in demanding environments, offering a balance of strength, corrosion resistance, and fabricability. Its unique properties make it a preferred choice in various industries, ensuring reliability and longevity in applications where failure is not an option.