15-5 PH Stainless Steel: Properties and Key Applications
Share
Table Of Content
Table Of Content
15-5 PH Stainless Steel is a precipitation-hardening stainless steel that combines high strength and corrosion resistance with good fabricability. Classified as a martensitic stainless steel, it contains significant amounts of chromium and nickel, along with copper, which enhances its hardening response. The primary alloying elements include:
- Chromium (Cr): Provides corrosion resistance and contributes to the steel's hardness.
- Nickel (Ni): Enhances toughness and ductility, improving the steel's overall performance.
- Copper (Cu): Aids in precipitation hardening, increasing strength without compromising corrosion resistance.
Characteristics and Properties
15-5 PH exhibits several notable characteristics:
- High Strength: Achieves high tensile and yield strength, making it suitable for demanding applications.
- Corrosion Resistance: Offers excellent resistance to a variety of corrosive environments, including atmospheric conditions and some acidic environments.
- Good Fabricability: Can be easily machined and welded, which is advantageous in manufacturing processes.
Advantages and Limitations
Pros | Cons |
---|---|
High strength-to-weight ratio | Limited high-temperature performance |
Excellent corrosion resistance | May require post-weld heat treatment |
Good machinability and weldability | Higher cost compared to some other stainless steels |
Historically, 15-5 PH has been widely used in aerospace, chemical processing, and other industries where high strength and corrosion resistance are critical. Its market position is strong, particularly in applications requiring a combination of mechanical properties and resistance to harsh environments.
Alternative Names, Standards, and Equivalents
Standard Organization | Designation/Grade | Country/Region of Origin | Notes/Remarks |
---|---|---|---|
UNS | S15500 | USA | Closest equivalent to AISI 630 |
AISI/SAE | 15-5 PH | USA | Precipitation hardening grade |
ASTM | A564 | USA | Specification for precipitation hardening stainless steels |
EN | 1.4545 | Europe | Similar properties but may have slight compositional differences |
JIS | SUS630 | Japan | Comparable grade with minor differences |
The differences between these equivalent grades often lie in their specific compositions and mechanical properties, which can affect their performance in particular applications. For instance, while UNS S15500 and AISI 630 are similar, slight variations in nickel and copper content can influence corrosion resistance and strength.
Key Properties
Chemical Composition
Element (Symbol and Name) | Percentage Range (%) |
---|---|
Chromium (Cr) | 15.0 - 17.5 |
Nickel (Ni) | 3.0 - 5.0 |
Copper (Cu) | 3.0 - 5.0 |
Manganese (Mn) | 1.0 max |
Silicon (Si) | 1.0 max |
Carbon (C) | 0.07 max |
Phosphorus (P) | 0.04 max |
Sulfur (S) | 0.03 max |
The primary role of chromium is to enhance corrosion resistance, while nickel improves toughness and ductility. Copper plays a crucial role in the precipitation hardening process, significantly increasing the strength of the steel without compromising its corrosion resistance.
Mechanical Properties
Property | Condition/Temper | Test Temperature | Typical Value/Range (Metric - SI Units) | Typical Value/Range (Imperial Units) | Reference Standard for Test Method |
---|---|---|---|---|---|
Tensile Strength | Annealed | Room Temp | 930 - 1,100 MPa | 135 - 160 ksi | ASTM E8 |
Yield Strength (0.2% offset) | Annealed | Room Temp | 620 - 850 MPa | 90 - 123 ksi | ASTM E8 |
Elongation | Annealed | Room Temp | 10 - 15% | 10 - 15% | ASTM E8 |
Hardness (Rockwell) | Annealed | Room Temp | 30 - 40 HRC | 30 - 40 HRC | ASTM E18 |
Impact Strength | Quenched & Tempered | -40°C | 40 J | 29.5 ft-lbf | ASTM E23 |
The combination of high tensile and yield strength makes 15-5 PH suitable for applications that require structural integrity under mechanical loading. Its good elongation values indicate that it can withstand deformation without fracturing, which is essential in dynamic applications.
Physical Properties
Property | Condition/Temperature | Value (Metric - SI Units) | Value (Imperial Units) |
---|---|---|---|
Density | Room Temp | 7.8 g/cm³ | 0.283 lb/in³ |
Melting Point | - | 1,400 - 1,500 °C | 2,552 - 2,732 °F |
Thermal Conductivity | Room Temp | 16 W/m·K | 92 BTU·in/ft²·h·°F |
Specific Heat Capacity | Room Temp | 500 J/kg·K | 0.12 BTU/lb·°F |
Electrical Resistivity | Room Temp | 0.73 µΩ·m | 0.0000013 Ω·in |
The density of 15-5 PH makes it a lightweight option for applications where weight savings are critical. Its thermal conductivity is moderate, which is beneficial in applications where heat dissipation is necessary, while its specific heat capacity indicates good thermal stability.
Corrosion Resistance
Corrosive Agent | Concentration (%) | Temperature (°C/°F) | Resistance Rating | Notes |
---|---|---|---|---|
Chlorides | 3.5% | 25°C/77°F | Good | Risk of pitting |
Sulfuric Acid | 10% | 25°C/77°F | Fair | Susceptible to stress corrosion cracking |
Acetic Acid | 5% | 25°C/77°F | Excellent | Resistant to localized corrosion |
Atmospheric | - | - | Excellent | Good for outdoor applications |
15-5 PH exhibits excellent resistance to atmospheric corrosion and is suitable for marine environments. However, it is susceptible to pitting in chloride-rich environments and stress corrosion cracking in the presence of sulfuric acid. Compared to grades like 304 and 316 stainless steels, 15-5 PH offers superior strength but may have lower resistance to certain corrosive agents, particularly in high-chloride environments.
Heat Resistance
Property/Limit | Temperature (°C) | Temperature (°F) | Remarks |
---|---|---|---|
Max Continuous Service Temp | 300°C | 572°F | Suitable for high-temperature applications |
Max Intermittent Service Temp | 400°C | 752°F | Can withstand short-term exposure to higher temperatures |
Scaling Temperature | 600°C | 1,112°F | Begins to lose mechanical properties |
At elevated temperatures, 15-5 PH maintains good oxidation resistance but may experience a reduction in mechanical properties. Care should be taken in applications involving prolonged exposure to high temperatures, as this can lead to decreased strength and potential scaling.
Fabrication Properties
Weldability
Welding Process | Recommended Filler Metal (AWS Classification) | Typical Shielding Gas/Flux | Notes |
---|---|---|---|
TIG | ER 630 | Argon | Preheat recommended |
MIG | ER 630 | Argon | Post-weld heat treatment may be required |
15-5 PH is generally considered weldable, but preheating and post-weld heat treatment are often necessary to avoid cracking and ensure optimal mechanical properties. The use of appropriate filler metals is crucial to maintain corrosion resistance and strength in the weld area.
Machinability
Machining Parameter | [15-5 PH] | [AISI 1212] | Notes/Tips |
---|---|---|---|
Relative Machinability Index | 60% | 100% | Requires slower cutting speeds |
Typical Cutting Speed (Turning) | 30 m/min | 50 m/min | Use carbide tools for best results |
Machinability is moderate, and while it can be machined effectively, slower cutting speeds and specialized tooling are recommended to achieve optimal results and prevent tool wear.
Formability
15-5 PH can be cold formed, but its work hardening characteristics may limit the extent of deformation. Hot forming is also possible, but care must be taken to avoid excessive temperatures that could lead to loss of mechanical properties.
Heat Treatment
Treatment Process | Temperature Range (°C/°F) | Typical Soaking Time | Cooling Method | Primary Purpose / Expected Result |
---|---|---|---|---|
Solution Annealing | 1,000 - 1,100°C / 1,832 - 2,012°F | 1 hour | Air cool | Dissolves precipitates |
Aging | 480 - 620°C / 896 - 1,148°F | 4 - 8 hours | Air cool | Increases strength through precipitation hardening |
The heat treatment process involves solution annealing followed by aging, which enhances the steel's strength through the formation of fine precipitates. This process significantly alters the microstructure, leading to improved mechanical properties.
Typical Applications and End Uses
Industry/Sector | Specific Application Example | Key Steel Properties Utilized in this Application | Reason for Selection (Brief) |
---|---|---|---|
Aerospace | Aircraft components | High strength, corrosion resistance | Critical for safety and performance |
Chemical Processing | Valve bodies | Corrosion resistance | Essential for harsh environments |
Oil & Gas | Pump shafts | High strength, toughness | Required for demanding conditions |
Medical Devices | Surgical instruments | Biocompatibility, corrosion resistance | Safety and reliability are paramount |
Other applications include:
-
- Marine hardware
-
- Food processing equipment
-
- Automotive components
15-5 PH is chosen for applications requiring a combination of high strength and corrosion resistance, particularly in environments where mechanical integrity is critical.
Important Considerations, Selection Criteria, and Further Insights
Feature/Property | [15-5 PH] | [AISI 304] | [AISI 316] | Brief Pro/Con or Trade-off Note |
---|---|---|---|---|
Key Mechanical Property | High strength | Moderate strength | Moderate strength | 15-5 PH offers superior strength |
Key Corrosion Aspect | Good in many environments | Excellent in most | Excellent in chlorides | 15-5 PH may corrode in chlorides |
Weldability | Moderate | Good | Good | 15-5 PH requires careful handling |
Machinability | Moderate | Good | Good | 15-5 PH is less machinable |
Formability | Moderate | Good | Good | 15-5 PH is less formable |
Approx. Relative Cost | Higher | Moderate | Moderate | Cost reflects performance benefits |
Typical Availability | Moderate | High | High | 15-5 PH is less common |
When selecting 15-5 PH, considerations include its cost-effectiveness, availability, and specific performance requirements. While it may be more expensive than other stainless steels, its unique combination of properties often justifies the investment, especially in high-performance applications. Safety and reliability are paramount in industries like aerospace and medical, where 15-5 PH's properties can significantly impact performance and durability.
In summary, 15-5 PH stainless steel is a versatile material that excels in applications requiring high strength and corrosion resistance, making it a preferred choice in demanding environments.