SS400 vs Q235 – Composition, Heat Treatment, Properties, and Applications

Table Of Content

Table Of Content

Introduction

SS400 and Q235 are two of the most commonly specified plain-carbon structural steels used worldwide for general fabrication, construction, and machinery. Engineers, procurement managers, and manufacturing planners frequently weigh trade-offs such as cost vs. assured mechanical performance, weldability vs. strength, and local availability vs. standard compliance when choosing between them. Typical decision contexts include structural framing, welded fabrications, and general machinery parts where predictable yield and reasonable ductility are required.

Although both grades are low‑carbon structural steels with broadly similar uses, they originate from different national standards systems and therefore have slightly different guaranteed chemical ranges and property limits. That difference in standards and test practice—not a fundamental metallurgical gulf—is why these two grades are often compared in design and procurement conversations.

1. Standards and Designations

  • SS400: Japanese Industrial Standards (JIS) designation commonly used for general structural steel (JIS G3101 / JIS G3131 family historically). Classified as plain carbon structural steel.
  • Q235: Chinese GB/T 700 series designation for carbon structural steel (several subgrades Q235A/B/C/D/E). Classified as plain carbon structural steel.
  • Comparable international equivalents:
  • ASTM/ASME: ASTM A36 (commonly used as a rough Western equivalent for general structural use, though not identical).
  • EN: S235 (European structural steel with similar application space; different guaranteed values and testing).
  • Category: Both SS400 and Q235 are plain carbon (mild) structural steels — not stainless, not tool or high‑strength low‑alloy (HSLA) steels. Some product forms may include microalloyed or thermomechanically processed variants, but the grades themselves are defined as carbon structural steels.

2. Chemical Composition and Alloying Strategy

Below are representative composition ranges (wt%). Values reflect typical maximums and common ranges from the respective standards and common practice; exact values must be validated on each mill certificate because subgrades and thickness limits can change limits.

Element SS400 (representative, wt%) Q235 (representative, wt%)
C ≤ 0.25 (typical range 0.05–0.25) ≤ 0.22 (typical range 0.05–0.22)
Mn ≤ 1.60 (commonly 0.3–1.6) ≤ 1.40 (commonly 0.3–1.4)
Si ≤ 0.50 (often ≤ 0.35) ≤ 0.35
P ≤ 0.050 ≤ 0.045
S ≤ 0.050 ≤ 0.045
Cr trace / not specified (≤0.30 typical impurity) trace / not specified
Ni trace / not specified trace / not specified
Mo trace / not specified trace / not specified
V, Nb, Ti, B, N generally trace / not specified generally trace / not specified

Notes: - Standards define maximum concentrations and acceptance criteria; both grades are intentionally low in hardenability alloying elements. Significant additions of Cr, Ni, Mo, V, or Nb are not part of typical SS400/Q235 compositions. - The primary strengthening elements are carbon and manganese; silicon is controlled for deoxidation and may affect toughness when present in higher amounts. - Small differences in maximums (e.g., slightly higher allowable Mn or Si in SS400) mean SS400 can appear marginally different in some mill lots, but both are engineered to be weldable, ductile structural steels.

How alloying affects performance: - Carbon increases strength and hardenability but reduces weldability and ductility as it rises. - Manganese increases strength and hardenability and helps deoxidize; moderate Mn improves toughness. - Silicon is a deoxidizer and increases strength slightly but can influence weld bead properties. - Phosphorus and sulfur are controlled because they reduce toughness and cause embrittlement and machining issues at elevated levels.

3. Microstructure and Heat Treatment Response

  • Typical microstructures: Under normal hot‑rolled or recrystallized conditions, both SS400 and Q235 present ferrite–pearlite microstructures. Grain size and pearlite morphology depend on rolling and cooling rates.
  • Normal processing: Hot rolling followed by controlled cooling typically yields a fine ferrite-pearlite structure offering a balance of strength and ductility.
  • Response to heat treatment:
  • Annealing/normalizing: Both steels respond to annealing and normalizing by refining grain size and improving toughness. Normalizing is used to homogenize and refine the microstructure for improved mechanical properties.
  • Quenching & tempering: These grades are not intended for hardening by quench & tempering; they lack the alloying content to develop high hardened martensite without excessive cracking risk. If heat-treated aggressively, the steels can form martensite in thin sections, but tensile and toughness behavior will be unpredictable.
  • Thermo‑mechanical processing: For both steels, tighter control of rolling and accelerated cooling can slightly increase strength and toughness; however, they remain in the mild/low-medium strength regime compared with HSLA or quenched & tempered steels.

4. Mechanical Properties

Representative mechanical property ranges (verify on material certificates; properties depend on thickness, testing method, and subgrade):

Property SS400 (typical) Q235 (typical)
Tensile Strength (MPa) 400–510 (depends on thickness) 370–500
Yield Strength (MPa) ≈ 245 (commonly reported for many thicknesses) 235 (nominal design yield — the “Q235” designation)
Elongation (% in 50 mm or 65 mm) 20–26% 20–26%
Charpy Impact Toughness Not universally specified; subgrades may specify values (improved by normalizing) Not universally specified; some subgrades/test conditions specify values
Hardness (HB) ~120–170 HB (hot-rolled condition typical) ~120–170 HB

Interpretation: - Q235 is named for a nominal minimum yield of 235 MPa; SS400 often has a similar or slightly higher guaranteed yield depending on thickness and product. In many product forms the practical strength differences are modest. - Ductility and toughness in both are sufficient for general structural use; improved toughness is achieved by specifying normalized or tested impact properties. - Neither grade is designed for high hardness or high-temperature service.

5. Weldability

Weldability is driven mainly by carbon content, carbon equivalents (hardenability), and residuals of alloying elements.

Common carbon equivalent formulas used to assess weldability: - IIW carbon equivalent: $$CE_{IIW} = C + \frac{Mn}{6} + \frac{Cr+Mo+V}{5} + \frac{Ni+Cu}{15}$$ - International Pcm: $$P_{cm} = C + \frac{Si}{30} + \frac{Mn+Cu}{20} + \frac{Cr+Mo+V}{10} + \frac{Ni}{40} + \frac{Nb}{50} + \frac{Ti}{30} + \frac{B}{1000}$$

Qualitative interpretation: - Both SS400 and Q235 are low‑carbon and have low concentrations of hardenability elements, so their $CE_{IIW}$ and $P_{cm}$ values are low compared with alloy or high‑strength steels. This translates to generally good weldability with common arc processes (SMAW, MIG/MAG, TIG). - Because Q235 often has slightly lower maximum carbon, it can be marginally easier to weld without preheat; however, actual weld procedure qualifications should use mill certificate chemistries, section thickness, and joint design to set preheat/interpass temperatures. - Microalloying or higher Mn/Si in a particular mill lot can increase hardenability slightly; for thick sections, preheat and controlled interpass temperatures are prudent to avoid cold cracking and hydrogen cracking.

6. Corrosion and Surface Protection

  • Both SS400 and Q235 are non‑stainless carbon steels; corrosion resistance is limited and depends on environment and exposure.
  • Protection strategies:
  • Barrier coatings (paints), hot‑dip galvanizing, zinc electroplating, and polymer coatings are standard protections for outdoor or corrosive environments.
  • Cathodic protection is used for buried or submerged structures.
  • PREN (Pitting Resistance Equivalent Number) is not applicable to these non‑stainless steels. For reference: $$\text{PREN} = \text{Cr} + 3.3 \times \text{Mo} + 16 \times \text{N}$$ applies to stainless alloys and is not meaningful for plain carbon steels like SS400 or Q235.

7. Fabrication, Machinability, and Formability

  • Formability/bendability: Both grades form and bend well in hot‑rolled condition. Minimum bend radii depend on thickness and specified ductility; Q235 and SS400 behave similarly.
  • Cutting and machining: Machinability is moderate. Lower carbon varieties and controlled sulfur improve machinability; neither grade is optimized for high-speed machining.
  • Surface finishing: Hot‑rolled surfaces are acceptable for many structural uses; shot blasting, grinding, or pickling is applied before painting or welding as appropriate.
  • Cold forming: Both can be cold‑formed; springback and residual stress depend on thickness and exact chemistry.

8. Typical Applications

SS400 Typical Uses Q235 Typical Uses
Structural beams, columns and girders manufactured to JIS requirements; construction steel for building frames General structural components, welded assemblies and profiles in China; construction and light machinery
Rolled shapes, plates and sheets for mechanical fabrication where JIS compliance is required Plates, coils, bars, and sections for general fabrication under GB standards
Welded bridges, cranes, and platforms when JIS standard acceptance and testing are specified General-purpose frames, supports, containers and commercial structures where cost and local availability are key

Selection rationale: - Choose based on required design code, the standard called out in the contract, local supply chain, and any specified mechanical or impact test requirements. For example, projects specifying JIS standards will typically call SS400; projects using GB standards will call Q235.

9. Cost and Availability

  • Relative cost: Both grades are commodity carbon steels and are priced close to one another; local market dynamics, tariffs, and logistics determine final cost. Q235 may be less expensive in regions with strong Chinese mill supply; SS400 may be more easily sourced where JIS product lines are established.
  • Availability by product form: Both are widely available in plates, coils, sheets, bars, and structural shapes. Lead times are generally short for standard sizes; specialty thicknesses or certified mill test reports may increase lead time.

10. Summary and Recommendation

Summary table (qualitative):

Attribute SS400 Q235
Weldability Very good (low C, low alloying) Very good (slightly lower C; low alloying)
Strength–Toughness balance Good; often slightly higher guaranteed tensile/yield in some product forms Good; designed for 235 MPa nominal yield
Cost & availability Widely available where JIS products are stocked; prices vary by region Widely available in China and regions with Chinese supply; often cost-competitive

Conclusions: - Choose Q235 if: - Your project specifies GB/T standards or is procurement‑constrained to local Chinese material supply. - You need a cost‑competitive general structural steel with nominal yield ≈ 235 MPa and good weldability for common welded fabrications. - Choose SS400 if: - Your design, contract, or client specifies JIS standards, or you require the particular product forms and test practices associated with JIS compliance. - You need the slightly different guaranteed mechanical limits offered under JIS for certain thicknesses, or you prefer suppliers and certificates tied to the JIS ecosystem.

Final note: SS400 and Q235 are broadly interchangeable for many general structural applications, but they are governed by different standards. Always verify specific mill certificates, thickness‑dependent guarantees, and any required impact testing or special processing before final selection.

Back to blog