SPCC vs SPCD – Composition, Heat Treatment, Properties, and Applications

Table Of Content

Table Of Content

Introduction

SPCC and SPCD are two closely related cold-rolled carbon steel grades commonly specified under JIS and used worldwide in sheet-metal fabrication. Engineers, procurement managers, and manufacturing planners routinely weigh trade-offs such as formability versus strength, weldability versus performance, and finishing versus cost when selecting between these grades. The practical selection dilemma is whether to prioritize higher ductility for deep drawing and complex stamping (typical of commercial cold-rolled grades) or to accept modestly higher strength with reduced elongation where load capacity and dimensional stability are more important.

The primary technical distinction between SPCC and SPCD lies in their cold-rolled chemistry and processing targets that produce different cold-forming ductility and tensile properties. This difference directly affects drawability, springback, and the heat-management strategies required for welding and subsequent processing.

1. Standards and Designations

  • Major international standards relevant to cold-rolled mild steels:
  • JIS (Japanese Industrial Standards) — original designations for SP-series cold-rolled steels (SPCC, SPCD, etc.)
  • ASTM/ASME — have analogous classes for cold-rolled carbon steels (commercial quality, drawing quality), though designations differ
  • EN (European norms) — EN 10130 family covers cold-rolled low-carbon steels for forming
  • GB (Chinese standards) — GB/T specifications for cold-rolled low-carbon steels
  • Classification: both SPCC and SPCD are plain carbon cold-rolled steels (carbon steels), not stainless, not tool steels, and not HSLA in the strict sense. They are designed primarily for forming and stamping applications rather than for high-temperature or high-hardness service.

2. Chemical Composition and Alloying Strategy

Element SPCC (typical specification style) SPCD (typical specification style)
C (Carbon) Low carbon, controlled for good formability Slightly higher carbon than SPCC, aimed at higher tensile strength
Mn (Manganese) Controlled level for deoxidation and strength Similar controlled Mn; contributes to strength and hardenability
Si (Silicon) Small amounts for deoxidation Similar small amounts
P (Phosphorus) Strictly limited (impurity) Strictly limited (impurity)
S (Sulfur) Low; may be controlled for machinability Low; typically similar control
Cr, Ni, Mo, V, Nb, Ti, B Generally absent or at trace/microalloying levels Generally absent or at trace/microalloying levels
N (Nitrogen) Trace; controlled where relevant Trace; controlled where relevant

Notes: - Both grades rely on a low-alloy, low-carbon chemistry; differences are subtle and achieved by slightly varying carbon and impurity control as well as cold-rolling and annealing schedules. - Alloying elements (Mn, Si) are kept low because the target property set emphasizes formability and paintability rather than hardenability or corrosion resistance. Microalloying (Nb, Ti, V) is not typical for these general cold-rolled grades; where present, it is used to control grain size and temper rolling behavior rather than to provide significant precipitation strengthening.

How alloying affects properties: - Carbon and manganese primarily raise strength and reduce ductility; small increases in carbon or Mn increase yield and tensile strengths but reduce elongation and increase susceptibility to martensitic transformation in HAZ during welding. - Silicon and manganese assist deoxidation; significant silicon can affect surface finish and coating adhesion. - Microalloying elements (if present at trace levels) refine grain size and may slightly increase strength without a large penalty to ductility.

3. Microstructure and Heat Treatment Response

  • Typical microstructures: both SPCC and SPCD are produced by cold rolling followed by annealing (recrystallization anneal) to restore ductility. The resulting microstructure is generally a fine ferrite-pearlite or predominantly ferritic matrix with dispersed pearlite, depending on carbon content.
  • SPCC: with slightly lower carbon, SPCC typically presents a more ferritic, softer matrix with fewer pearlitic regions, which favors higher uniform elongation and deep drawability.
  • SPCD: with modestly higher carbon content, SPCD may show a somewhat greater pearlite fraction or higher dislocation density after rolling, giving higher strength and slightly lower ductility.

Heat treatment response: - These grades are not designed for hardening by quench-and-temper; they respond to annealing (full or recrystallization) and temper rolling. Normalizing is not commonly applied to cold-rolled commercial steels targeted for forming. - Thermo-mechanical treatments are more relevant for HSLA steels than SP-series cold-rolled grades. Attempts to strengthen SPCC/SPCD by heat treatment produce limited gains because alloying is minimal; strength increases primarily through cold work or conversion to a higher carbon design.

4. Mechanical Properties

Property SPCC SPCD
Tensile strength Moderate (designed for forming) Higher than SPCC (designed for higher strength)
Yield strength Moderate Slightly higher
Elongation (ductility) Higher — better uniform and total elongation Lower — reduced formability compared with SPCC
Impact toughness Adequate for room-temperature forming; generally similar Comparable at room temperature; may be marginally lower in specific cases due to higher strength
Hardness Lower (softer) Slightly higher

Explanation: - SPCD typically achieves higher tensile and yield strength at the expense of elongation; this is consistent with its slightly higher carbon and cold work level. SPCC offers better ductility and is therefore preferred for deep drawing and complex-shaped stampings. - Toughness differences at ambient temperature are usually modest for both; neither is intended for low-temperature impact-critical applications.

5. Weldability

Weldability considerations center on carbon content, manganese, and any other hardenability-increasing elements. Higher carbon raises the carbon equivalent, increasing risk of HAZ hardening and cold cracking.

Useful carbon-equivalent and weldability indicators: - IIW carbon equivalent: $$CE_{IIW} = C + \frac{Mn}{6} + \frac{Cr+Mo+V}{5} + \frac{Ni+Cu}{15}$$ - Pcm (more conservative index for welding behavior): $$P_{cm} = C + \frac{Si}{30} + \frac{Mn+Cu}{20} + \frac{Cr+Mo+V}{10} + \frac{Ni}{40} + \frac{Nb}{50} + \frac{Ti}{30} + \frac{B}{1000}$$

Qualitative interpretation: - SPCC, with lower carbon, will have a lower $CE_{IIW}$ and $P_{cm}$, indicating generally easier welding with lower preheat requirements and lower susceptibility to HAZ cracking. - SPCD, with modestly higher carbon, increases $CE_{IIW}$ and $P_{cm}$ values. This requires more careful welding practice (preheat, controlled interpass temperature, appropriate filler metals) for thicker sections or hydrogen-prone environments. - For thin sheet work typical of these grades, conventional resistance spot welding and MIG/TIG butt welds are commonly used; process parameters must be tuned when using SPCD to avoid brittleness in the weld zone. - Post-weld stress relief is rarely applied to thin cold-rolled parts but may be considered for assemblies where higher residual stress combined with higher carbon increases cracking risk.

6. Corrosion and Surface Protection

  • Both SPCC and SPCD are non-stainless carbon steels and therefore rely on coatings and surface treatments for corrosion protection.
  • Common protection methods:
  • Hot-dip galvanizing (zinc coating)
  • Electro-galvanizing (for improved paintability)
  • Organic coatings: phosphate conversion coat + paint or powder coat
  • Passivation and oiling for temporary protection during storage
  • PREN (Pitting Resistance Equivalent Number): $$\text{PREN} = \text{Cr} + 3.3 \times \text{Mo} + 16 \times \text{N}$$
  • PREN is not applicable to SPCC/SPCD because these are not stainless steels and do not contain significant Cr, Mo, or N for passive film formation.
  • Selection of protective systems depends on end-use environment (indoor, outdoor, automotive underbody), cost, and adhesion/paintability requirements.

7. Fabrication, Machinability, and Formability

  • Formability:
  • SPCC: superior deep-drawing performance and stretch-forming; lower springback and more homogeneous deformation during stamping. Preferred for deep-drawn automotive outer panels and appliance shells.
  • SPCD: reduced drawability and higher springback; better when stronger sheet is required (shallow drawn parts, structural inner panels).
  • Cutting and blanking:
  • Both grades machine similarly; SPCD’s higher strength may require slightly greater tool forces and cause faster tool wear.
  • Bending and springback:
  • SPCD exhibits greater springback due to higher yield; forming dies and process parameters must compensate.
  • Machinability:
  • Both are conventional low-carbon steels and machine acceptably; higher strength in SPCD can reduce machining speeds and increase tooling stress.
  • Finishing and surface treatment:
  • Both accept painting and plating. Surface cleanliness and oxide control during annealing are important for consistent coating adhesion.

8. Typical Applications

SPCC (typical uses) SPCD (typical uses)
Automotive exterior panels, refrigerator shells, consumer appliance bodies, deep-drawn parts Automotive inner structural panels, parts requiring higher tensile strength or reduced deformation, shallow-drawn or stamped structural components
General-purpose stamped components, chassis covers, furniture panels Components where dimensional stability and higher strength are prioritized over maximum formability
Decorative and painted surfaces where surface finish is critical Applications that benefit from modest higher strength with similar surface finish requirements

Selection rationale: - Choose SPCC for complex forming operations, especially when maximal ductility and surface finish matter (outer panels, deep-drawn components). - Choose SPCD where slightly higher strength and reduced deformation under load are valuable, and where forming demands are less severe or can be accommodated by tooling adjustments.

9. Cost and Availability

  • Cost: SPCC is typically the lower-cost option because it targets mass-market commercial properties and has broad production volumes. SPCD may carry a modest premium because of slightly tighter chemical control or specific process targets.
  • Availability: Both grades are widely produced in regions with substantial automotive and appliance industries. SPCC is often more ubiquitous across multiple product forms (coils, cut-to-length, blanked sheets). SPCD availability may be slightly more limited depending on regional demand for higher-strength cold-rolled sheets.
  • Product forms: coils, cut sheets, pre-painted coil (for SPCC), and electro-galvanized coils are common. Lead times vary by coating and thickness.

10. Summary and Recommendation

Attribute SPCC SPCD
Weldability Very good (lower CE) Good but requires more care (higher CE)
Strength–Toughness balance Optimized for ductility and forming Higher strength with modest reduction in ductility
Cost Generally lower Slightly higher

Recommendations: - Choose SPCC if you need the best cold-forming ductility, deep-drawing performance, and a lower-cost general-purpose cold-rolled sheet for outer panels, decorative parts, or highly stamped components. - Choose SPCD if your design requires higher tensile or yield strength in the cold-rolled product and you can accept reduced elongation and increased forming force or compensate with tooling; also appropriate when dimensional stability and load-bearing in a thin-sheet application are prioritized.

Final note: SPCC and SPCD are close cousins in the cold-rolled carbon-steel family; the right choice is driven by the forming severity, required in-service loads, weld procedure constraints, surface-finishing route, and total part cost. Engineers should review supplier mill certificates and perform formability/weld trials with the selected coil lot to verify performance in the intended manufacturing process.