Ship Plate vs Offshore Plate – Composition, Heat Treatment, Properties, and Applications
Share
Table Of Content
Table Of Content
Introduction
Ship plate and offshore plate are two broad categories of structural steel used in maritime and hydrocarbon-industry construction. Engineers and procurement teams frequently balance trade-offs such as cost versus long-term durability, weldability versus strength, and fabrication speed versus service safety when selecting between them. Typical decision contexts include ship hull construction (where cost and formability are primary) versus offshore topsides and jacket/subsea structures (where extended corrosion exposure, low-temperature toughness, and stringent inspection are critical).
The key technical distinction is that offshore plates are specified and produced to meet additional service-driven requirements — enhanced toughness, stricter chemical controls, tighter non-destructive testing (NDT), and sometimes corrosion resistance — compared with conventional ship plates. These differences affect composition choices, thermomechanical processing, inspection, and ultimately lifecycle cost.
1. Standards and Designations
Major standards and common designations used for these two families include:
- International/Western:
- ASTM / ASME (e.g., ASTM A131 for shipbuilding; ASTM A572/A709/HPS and API 2H/2W for structural and offshore steels)
- EN (e.g., EN 10025 series for structural steels; NORSOK standards for offshore)
- DNV–GL (classification rules for ship and offshore)
- Asian:
- JIS (Japan Industrial Standards) — shipbuilding and structural steels
- GB (China National Standards) — ship and offshore plates
Classification by steel type: - Ship plate: typically plain carbon or low-alloy structural steels (mild steel / HSLA depending on grade). - Offshore plate: typically HSLA steels produced by thermomechanical controlled processing (TMCP), plus alloyed corrosion-resistant steels for specific locations; may include microalloyed grades (Nb, V, Ti) or low-alloy martensitic/quenched-tempered steels for high-strength applications.
2. Chemical Composition and Alloying Strategy
The following table summarizes the typical presence and role of key alloying elements in ship plate versus offshore plate (qualitative descriptors are used because specific compositions depend on standard and product grade).
| Element | Ship Plate (typical presence) | Offshore Plate (typical presence) |
|---|---|---|
| C (Carbon) | Low–Medium (balance of strength and weldability) | Low (kept lower to improve toughness and reduce cracking risk) |
| Mn (Manganese) | Medium (deoxidation and strengthening) | Medium–High (aids hardenability and strength control) |
| Si (Silicon) | Trace–Medium (deoxidizer) | Trace–Medium |
| P (Phosphorus) | Controlled low (impurity) | More tightly controlled low |
| S (Sulfur) | Controlled low | More tightly controlled low |
| Cr (Chromium) | Usually low/absent | Sometimes present for corrosion/strength in specific grades |
| Ni (Nickel) | Usually low/absent | May be present for toughness at low temperatures |
| Mo (Molybdenum) | Rare or low | May be present to improve hardenability and high-temperature strength |
| V (Vanadium) | Rare | Often present as microalloying to refine grain and strengthen |
| Nb (Niobium) | Rare | Common microalloying for grain refinement in TMCP grades |
| Ti (Titanium) | Rare | Sometimes used for stabilization / grain control |
| B (Boron) | Typically absent | May be used in minute amounts to increase hardenability in specific grades |
| N (Nitrogen) | Low | Controlled; nitrogen may be specified for certain stainless/duplex offshore alloys |
Alloying strategy summary: - Ship plate grades prioritize simple chemistries that are robust, formable, and economical. - Offshore plate chemistries are optimized to deliver high toughness, controlled hardenability, and fine-grained microstructures; hence, microalloying (Nb, V, Ti) and tighter impurity control are common. Additional alloying (Ni, Mo, Cr) appears where corrosion resistance or high strength is needed.
3. Microstructure and Heat Treatment Response
Typical microstructures: - Ship plate: Ferrite–pearlite microstructure is common in conventional ship plates produced by conventional rolling and controlled cooling. Where higher strength is required, bainitic structures may be present but still relatively coarse compared with TMCP steels. - Offshore plate: Modern offshore steels produced by TMCP exhibit refined ferrite and bainitic microstructures (acicular ferrite or fine-grained bainite) with dispersed microalloy precipitates. These microstructures provide better strength–toughness combinations and improved resistance to brittle fracture.
Heat treatment and processing effects: - Normalizing: Refines grain size and can improve toughness for both families but is more commonly specified for higher-grade offshore steels to meet impact requirements. - Quenching & tempering (Q&T): Used primarily for higher-strength, through-thickness critical applications where superior strength and toughness are required; less common for basic ship plates. - Thermomechanical Controlled Processing (TMCP): Widely used for offshore plates to produce a fine-grained structure, enhance yield strength, and improve low-temperature toughness without alloy-heavy chemistries. - PWHT (post-weld heat treatment): May be required for thick or quenched/tempered offshore steels; for ship plates, PWHT is less frequently specified except for specific welded assemblies.
4. Mechanical Properties
The mechanical property differences are driven by composition and processing. The table below provides qualitative comparisons (actual numeric specifications depend on grade, thickness, and standard).
| Property | Ship Plate | Offshore Plate |
|---|---|---|
| Tensile Strength | Moderate | Moderate–High (depending on grade) |
| Yield Strength | Moderate | Medium–High (HSLA grades often higher) |
| Elongation (%) | High (good ductility) | Good but may be lower than simple ship grades at equivalent thickness due to higher strength |
| Impact Toughness (Charpy) | Adequate at ambient | Higher, especially for low-temperature and critical offshore service |
| Hardness | Lower | Variable; can be higher for higher-strength or Q&T offshore steels |
Which is stronger/tougher/more ductile: - Offshore plates are often engineered to achieve a better strength–toughness balance, particularly at low temperatures; they may provide higher yield strength while maintaining acceptable ductility through fine microstructure and microalloying. - Ship plates prioritize ductility and formability, which can translate into higher elongation at the expense of lower yield strength.
5. Weldability
Weldability is a key differentiator and is influenced by carbon content, hardenability, and microalloying.
Important weldability indices (used for qualitative assessment): - Carbon Equivalent (IIW): $$CE_{IIW} = C + \frac{Mn}{6} + \frac{Cr+Mo+V}{5} + \frac{Ni+Cu}{15}$$ - Pcm (Sindo's formula): $$P_{cm} = C + \frac{Si}{30} + \frac{Mn+Cu}{20} + \frac{Cr+Mo+V}{10} + \frac{Ni}{40} + \frac{Nb}{50} + \frac{Ti}{30} + \frac{B}{1000}$$
Qualitative interpretation: - Lower $CE_{IIW}$ or $P_{cm}$ indicates easier weldability and lower susceptibility to hydrogen-induced cold cracking. - Ship plates typically have lower alloy content and moderate carbon, resulting in generally good weldability without stringent preheat or PWHT requirements for common thicknesses. - Offshore plates, despite lower carbon in many grades, can have increased hardenability due to Mn, Mo, Nb, V, or B; this raises crack risk in thick sections and may require controlled preheat, interpass temperature, and, in some cases, PWHT. Higher-strength or quenched-and-tempered offshore steels will often have stricter weld procedures and qualification requirements.
Practical considerations: - Thickness, joint design, and local heat input dominate real-world weldability issues. - NDT regimes for offshore structures may be more rigorous (radiography, ultrasonic), and welding procedures must be qualified to higher standards.
6. Corrosion and Surface Protection
Non-stainless steels (most ship and many offshore structural plates) rely on coatings and cathodic protection: - Typical measures: surface preparation, primers, high-performance paints, hot-dip galvanizing (where feasible), and impressed current or sacrificial anode systems for submerged components. - Offshore service often demands advanced coatings (multi-layer, abrasion- and UV-resistant) and cathodic protection design; coating longevity and inspection are critical cost drivers.
When stainless or duplex steels are used offshore, use PREN to assess pitting resistance: $$\text{PREN} = \text{Cr} + 3.3 \times \text{Mo} + 16 \times \text{N}$$ - PREN is not applicable to plain carbon or HSLA ship plates. - Offshore environments (splash zone, splash-to-submerged interfaces) may require stainless or duplex materials with high PREN, driven by chloride-induced pitting risk.
7. Fabrication, Machinability, and Formability
- Cutting: Both families are typically cut by oxy-fuel, plasma, or laser; higher-strength offshore plates may require consideration of cutting heat input and edge condition for subsequent welding.
- Bending/forming: Ship plates, being more ductile, are easier to bend and form. Offshore HSLA plates maintain reasonable formability but may require larger bend radii and greater force due to higher yield strength.
- Machinability: Higher-strength microalloyed steels can be tougher to machine and may reduce tool life compared with low-carbon ship steels. Preheat and cutting-fluid strategies can mitigate this.
- Surface finishing: Offshore plates may receive additional mill or post-fabrication treatments (e.g., stress-relief, pickling/passivation for stainless grades) to meet inspection criteria.
8. Typical Applications
| Ship Plate (typical uses) | Offshore Plate (typical uses) |
|---|---|
| Hull plating, deck plating, internal stiffeners for merchant ships and tugs | Jacket members, topside structural members, braces, platform decks for offshore oil & gas |
| Bulkheads, hatch covers, general structural elements where formability and cost are priorities | Subsea structural components, riser supports, and splash zone parts requiring higher toughness/corrosion control |
| Non-critical superstructure where economy and painting are primary | High-integrity welded joints, load-bearing braces, and cold-service components where NDT and low-temperature performance are required |
Selection rationale: - Choose ship plate when fabrication speed, bending/formability, and lower material cost are primary. - Choose offshore plate when service environment (chilling temperatures, cyclic loading, aggressive corrosion) demands higher toughness, stricter inspection, and longer design life.
9. Cost and Availability
- Cost: Ship plates are generally less expensive per tonne than specialized offshore plates because of simpler chemistry, less processing, and broader supplier base. Offshore plates (TMCP, microalloyed, or higher-spec corrosion-resistant steels) command a premium due to tighter controls and additional processing.
- Availability: Standard ship plates are widely available from many mills in standard thicknesses and lengths. Offshore plates to specific standards or with tight Z-profile/low-S/R guarantees may have longer lead times and limited suppliers, especially for large thicknesses or specialty corrosion-resistant alloys.
- Procurement advice: Early engagement with suppliers and specifying critical parameters (impact requirements, thickness ranges, NDT) reduces delivery risk and cost escalation.
10. Summary and Recommendation
| Attribute | Ship Plate | Offshore Plate |
|---|---|---|
| Weldability | Generally good; simpler procedures | Good with controls; may need preheat/PWHT for higher-strength grades |
| Strength–Toughness balance | Moderate strength, high ductility | Optimized for higher strength with improved low-temperature toughness |
| Cost | Lower | Higher (processing, alloying, inspection) |
Choose ship plate if: - The project emphasizes low procurement cost, extensive forming/bending operations, and the service environment is less demanding (e.g., non-submerged hull areas with regular maintenance and coatings). - Inspection and traceability requirements are moderate and standard shipbuilding grades meet fitness-for-service criteria.
Choose offshore plate if: - The application requires higher low-temperature toughness, tighter chemistry and mechanical-property control, enhanced through-thickness properties, or more rigorous NDT and documentation. - The structure will operate in harsh marine environments, face cyclic or extreme loading, or have long maintenance intervals where lifecycle risk reduction justifies higher material and fabrication cost.
Concluding note: Selection should be driven by a combination of design loads, environmental exposure, fabrication plan, inspection regime, and lifecycle cost modeling. Collaborate with class societies, material suppliers, and welding specialists early in the design process to confirm the appropriate grade, processing route, and welding procedures for either ship or offshore plate applications.