SA106B vs SA106C – Composition, Heat Treatment, Properties, and Applications

Table Of Content

Table Of Content

Introduction

ASTM A106 Grade B (SA106B) and Grade C (SA106C) are two common seamless carbon-steel pipe grades specified for high-temperature service and pressure applications. Engineers, procurement managers, and manufacturing planners typically weigh trade-offs such as strength versus formability, cost versus allowable working pressure, and weldability versus hardenability when selecting between them.

The principal technical distinction between SA106B and SA106C is that Grade C is specified for higher strength and pressure-temperature ratings than Grade B, achieved primarily through a modestly higher carbon/alloy content and tighter mechanical property requirements. Because they share the same standard and production routes, these grades are often compared directly in piping design, fabrication planning, and material purchase specifications.

1. Standards and Designations

  • Primary standard: ASTM A106 / ASME SA106 — “Seamless Carbon Steel Pipe for High-Temperature Service.”
  • Other regional references: equivalent product forms exist in EN, JIS, and GB standards for carbon steel pipe, but direct grade-to-grade equivalence varies; specification and mechanical requirements must be confirmed case-by-case.
  • Classification: both SA106B and SA106C are carbon steels intended for high-temperature service (not stainless, not HSLA in the modern sense, and not tool steel).

2. Chemical Composition and Alloying Strategy

Element SA106B (typical specification character) SA106C (typical specification character)
C (Carbon) Lower carbon level compared to C; controlled to balance strength and weldability Slightly higher carbon than B to achieve higher yield/tensile and pressure ratings
Mn (Manganese) Present to provide tensile strength and deoxidation control; similar range in both grades Similar to B; used to support strength as carbon increases
Si (Silicon) Deoxidizer; amounts controlled and similar in both grades Same role; generally not a strengthening alloy in these grades
P (Phosphorus) Kept low as an impurity to preserve toughness Kept low; similar impurity limits
S (Sulfur) Kept low; can be present in small quantities Kept low; similar limits
Cr, Ni, Mo Not purposely alloyed in significant quantities; typically present only as trace impurities Often traces only; not a primary alloying strategy
V, Nb, Ti Not regularly added as microalloying elements for A106; modern mills may use microalloying in specific runs Typically not specified; if present it may be incidental or for special lots
B, N Not relevant as defining alloying elements; nitrogen controlled for impact properties Same as B

Notes: - ASTM A106 defines chemical limits and mechanical requirements rather than prescribing significant alloying additions like Cr or Mo; these are carbon-steel grades with compositions controlled for consistent high-temperature strength and weldability. - The design strategy for Grade C centers on modestly increased carbon/Mn and stricter mechanical testing to raise allowable stresses at temperature; Grade B aims for a balance of strength and fabrication friendliness.

3. Microstructure and Heat Treatment Response

  • Typical microstructure: both grades are produced as seamless pipes with microstructures dominated by ferrite and pearlite in normalized or as-rolled condition. The ferrite/pearlite balance depends on carbon and cooling rates.
  • Grade B: with its lower carbon content, the microstructure tends toward a finer, more ductile ferrite–pearlite mix with relatively lower pearlite fraction than Grade C under similar thermal history.
  • Grade C: higher carbon and manganese increase the pearlite fraction and raise hardenability slightly, shifting the balance toward higher strength and modestly reduced ductility.
  • Heat treatment response:
  • Normalizing (reheating above critical temperature and air cooling) refines grain size, improves toughness, and produces a consistent ferrite–pearlite microstructure for both grades.
  • Quenching and tempering are possible but are not typical mill-supply conditions for standard A106 pipe; applying these processes will increase strength and toughness depending on parameters, with Grade C responding with higher achievable strength due to its composition.
  • Thermo-mechanical processing (controlled rolling) can refine grain structure and improve strength–toughness combinations; Grade C’s slightly higher hardenability allows achieving higher strengths with similar processing intensity.

4. Mechanical Properties

Property SA106B SA106C
Tensile strength Moderate — meets Grade B requirements Higher — meets Grade C higher tensile requirements
Yield strength Lower than C — allows more plastic deformation before yielding Higher than B — allows higher allowable stresses at temperature
Elongation (ductility) Typically higher ductility than C Slightly reduced elongation relative to B due to higher carbon/pearlite
Impact toughness Good at standard test temperatures; maintained by low impurity levels Comparable but may require attention at very low temperatures; toughness can be maintained by processing
Hardness Lower to moderate Slightly higher (reflecting higher strength)

Interpretation: - SA106C achieves greater tensile and yield strength than SA106B; the trade-off is a modest reduction in ductility and potentially higher susceptibility to hardening in the HAZ during welding. For pressure-vessel and high-temperature piping, the higher allowable stresses for C can permit thinner walls or higher operating pressures, but weld procedures and preheat must be considered.

5. Weldability

  • General: both grades are considered weldable by common methods (SMAW, GTAW, GMAW, FCAW). Weldability depends primarily on carbon content, carbon equivalent (CE), and presence of microalloying elements.
  • As carbon increases, susceptibility to hydrogen-assisted cracking in the heat-affected zone (HAZ) increases; Grade C typically requires more careful welding controls (preheat, interpass temperature, controlled heat input) than Grade B.
  • Common weldability indices:
  • $$CE_{IIW} = C + \frac{Mn}{6} + \frac{Cr+Mo+V}{5} + \frac{Ni+Cu}{15}$$
  • $$P_{cm} = C + \frac{Si}{30} + \frac{Mn+Cu}{20} + \frac{Cr+Mo+V}{10} + \frac{Ni}{40} + \frac{Nb}{50} + \frac{Ti}{30} + \frac{B}{1000}$$
  • Interpretation:
  • Higher $CE_{IIW}$ or $P_{cm}$ indicates higher hardenability and a greater risk of HAZ cracking; while SA106 grades generally have modest CE values, Grade C will typically register a slightly higher CE than Grade B.
  • For both grades, low sulfur and phosphorus and limited alloy additions maintain good weldability. When specifying SA106C for thicker-wall or critical welds, plan appropriate preheat and qualifying welding procedures to avoid HAZ cracking.

6. Corrosion and Surface Protection

  • Both SA106B and SA106C are carbon steels (non-stainless) and are not inherently corrosion-resistant in atmospheric, soil, or marine environments.
  • Common protective measures:
  • External coatings: painting, epoxy, or fusion-bonded epoxy (FBE).
  • Metallic coatings: hot-dip galvanizing for certain service conditions (consider temperature limitations and coating compatibility with elevated-temperature service).
  • Internal linings: cement mortar, epoxy, or other linings for corrosive fluids.
  • PREN relevance: the PREN index is used for stainless alloys (pitting resistance), so it is not applicable to SA106 carbon steels. If a service requires pitting-corrosion resistance, a stainless or alloyed material should be selected.
  • For contrast, the PREN formula for stainless alloys is: $$\text{PREN} = \text{Cr} + 3.3 \times \text{Mo} + 16 \times \text{N}$$
  • Clarification: Because A106 grades have minimal chromium and molybdenum, corrosion mitigation is achieved via coatings, cathodic protection, and material selection rather than inherent alloy resistance.

7. Fabrication, Machinability, and Formability

  • Cutting: both grades are readily cut with oxy-fuel, plasma, or mechanical cutting. Grade C may generate slightly harder chips due to higher carbon, but differences are modest.
  • Machinability: similar for both; higher carbon in Grade C can make tool wear marginally more pronounced under aggressive conditions.
  • Formability and bending: Grade B’s slightly greater ductility makes it marginally easier to cold-form or bend without cracking; Grade C may require larger bend radii or heat-assisted forming for tight-radius work.
  • Threading and joining: standard pipe-threading and flange fabrication are comparable. Welding filler selection should match base metal chemistry and service temperature; low-alloy filler metal may be appropriate for high-temperature service.

8. Typical Applications

SA106B — Typical Uses SA106C — Typical Uses
Boiler tubes, moderate-temperature process piping, general-purpose high-temperature service where moderate strength and good ductility are prioritized High-temperature service and piping systems where higher allowable stresses or higher pressure-temperature ratings are required
Low- to medium-pressure steam lines, heat exchangers with moderate design pressures Power plant piping, higher-pressure steam and feedwater lines where code allowable stresses mandate higher grade
General plant piping, conveying non-corrosive fluids at elevated temperatures Applications that allow wall-thickness optimization by using higher-strength material to meet stress limits

Selection rationale: - Choose the grade that meets the required allowable stress at operating temperature with the smallest wall thickness and lowest life-cycle cost, while ensuring fabrication and welding controls are feasible for the site and contractor.

9. Cost and Availability

  • Cost: SA106B is typically less expensive than SA106C because of lower mechanical requirements and slightly simpler processing targets. However, market pricing fluctuates with steel mill practices, commodity prices, and regional supply.
  • Availability: both grades are widely available globally in a range of diameters and wall thicknesses. For large-diameter or heavy-wall sections, lead times may increase; Grade B often has broader immediate availability for common sizes.
  • Product forms: seamless pipe is standard under A106; availability can vary by supplier (seamless versus welded variants under other standards).

10. Summary and Recommendation

Category SA106B SA106C
Weldability Better (easier welding and lower preheat requirements) Good, but typically requires more welding control (preheat/interpass)
Strength–Toughness balance Lower strength, higher ductility Higher strength, slightly lower ductility but higher allowable stresses
Cost Generally lower Generally higher

Conclusions and recommendations: - Choose SA106B if: - Your application prioritizes easier fabrication and welding, higher ductility, and lower material cost. - The design pressure/temperature envelope and code allowable stresses are satisfied by Grade B without excessive wall thickness. - Field welding conditions are constrained and you prefer minimal preheat/interpass requirements.

  • Choose SA106C if:
  • The project requires higher allowable stresses, thinner wall sections for the same pressure/temperature rating, or higher tensile/yield margins.
  • You can control welding procedures (preheat, qualified procedures) and fabrication practices to accommodate the slightly higher hardenability.
  • The life-cycle or weight savings from reduced wall thickness offset the higher material cost and fabrication controls.

Final note: The ASTM A106 standard contains the exact chemical and mechanical requirements and should be consulted when preparing purchase specifications or engineering calculations. For critical or high-risk services, perform supplier qualification, request mill test reports, and verify heat-treatment and NDT requirements to ensure compliance with design and safety objectives.

Back to blog