Q235A vs Q235B – Composition, Heat Treatment, Properties, and Applications

Table Of Content

Table Of Content

Introduction

Q235A and Q235B are two commonly specified grades from the Q235 family of carbon structural steels under the Chinese GB/T 700 standard. Engineers, procurement managers, and manufacturing planners frequently choose between them for structural components, plates, and rolled sections where baseline strength, weldability, and cost are important. Typical selection scenarios balance weldability and forming ease against notch toughness and suitability for lower-temperature service.

The principal practical distinction between these two grades is toughness control and the attendant steelmaking practice: one grade is produced and supplied without an imposed low-temperature impact requirement and therefore can be manufactured with less stringent deoxidation/oxygen-control practices; the other is specified to demonstrate a minimum impact energy at a defined temperature, which drives both melt/deoxidation control and inspection. Because of that difference, Q235B is generally treated to achieve more consistent toughness than Q235A and is preferred where impact resistance is required.

1. Standards and Designations

  • Major standards and cross-references:
  • GB/T 700 — Chinese national standard for hot-rolled low carbon structural steel (defines Q235 series).
  • Common international analogues for general understanding: ASTM A36 (structural), EN S235 (structural steels), JIS G3101 SS400 (Japan). Note: these are approximate functional equivalents, not direct chemical/mechanical identity matches.
  • Material classification:
  • Q235A and Q235B are plain low-carbon structural steels (non-alloy carbon steels). They are neither stainless nor HSLA in the modern high-strength low-alloy sense, nor tool steels.

2. Chemical Composition and Alloying Strategy

Element Typical control (GB/T 700 guidance; consult mill certificate)
C (carbon) ≤ 0.22 (nominal low-carbon content; primary strength contributor)
Mn (manganese) ≤ 1.40 (strength and deoxidation aid; limits on brittle behavior)
Si (silicon) small (deoxidizer; typical trace to a few tenths percent)
P (phosphorus) ≤ 0.045 (impurity—kept low to avoid embrittlement)
S (sulfur) ≤ 0.045 (impurity—controlled to preserve toughness and machinability)
Cr, Ni, Mo, V, Nb, Ti, B Not intentionally alloyed in standard Q235 grades; typically present only as trace residuals (mill-specific)
N (nitrogen) Controlled at low levels; not a deliberate alloying element

Notes: - The Q235 family is designed to be a low-carbon, low-alloy structural steel. Alloying is deliberately minimal to keep cost low and to preserve good weldability and formability. - The presence of manganese and silicon at controlled levels supports tensile strength and deoxidation. Microalloying (V, Nb, Ti) is not a feature of Q235—if present in commercial material they are usually at residual levels. - For any project, always confirm the actual chemical certificate from the mill because values vary with product form and producer.

How alloying affects properties: - Carbon increases strength but reduces weldability and ductility as content rises; Q235’s low carbon keeps a good balance. - Manganese increases hardenability and tensile strength but excessive Mn can increase crack susceptibility. - Deoxidizers (Si, Al, Mn) and the deoxidation route (rimmed, semi-killed, killed) influence inclusion population and internal porosity; these in turn influence impact toughness and welding performance.

3. Microstructure and Heat Treatment Response

  • Typical microstructure: As-rolled Q235 steels produce a predominantly ferritic matrix with polygonal ferrite and some pearlite, reflecting their low carbon content. The microstructure is forgiving to common cold-forming and welding operations.
  • Effects of processing:
  • Normalizing: Produces a more uniform ferrite–pearlite structure, modestly refining grain size and improving toughness consistency. Not commonly required for standard Q235.
  • Quenching & tempering: Not typical or economical for Q235; these steels are not designed for heat-treatment to increase strength.
  • Thermo-mechanical processing: Controlled rolling and accelerated cooling can refine grain structure and increase toughness; such approaches shift the material toward higher-strength structural steel families, not typical Q235 practice.
  • Grade-specific microstructural implications:
  • Q235A: With looser toughness requirements and potentially less rigorous deoxidation, it can display more variation in inclusion content and localized toughness.
  • Q235B: Produced to meet an impact energy requirement at 0°C, so mills commonly employ killed or low-oxygen practices and process control to achieve consistent microstructure and fewer detrimental defects, yielding better notch toughness.

4. Mechanical Properties

Property Q235A (typical) Q235B (typical)
Yield strength (nominal) 235 MPa (design basis for grade name) 235 MPa
Tensile strength (typical) ~370–500 MPa (depends on thickness/process) ~370–500 MPa (similar range)
Elongation (A%) ~20–26% (varies with thickness) ~20–26% (similar or slightly better at low temperature)
Impact toughness Not specified by standard for A; varies by mill Specified at 0°C (commonly a Charpy V-notch minimum, e.g., ~27 J)
Hardness Typical mild-steel hardness range; not a primary spec Similar to Q235A under like processing

Explanation: - Both grades have the same nominal yield-strength target (235 MPa). Tensile and elongation are strongly affected by thickness and rolling practices rather than the A/B suffix alone. - Q235B is required to meet a minimum impact energy at a specified temperature (commonly 0°C). That testing requirement causes Q235B material to have more consistent notch toughness than Q235A. - Q235A may be mechanically equivalent in static loading but is less controlled for low-temperature impact resistance.

5. Weldability

Weldability for low-carbon steels is generally good; both Q235A and Q235B are considered easily weldable with standard filler metals and common welding processes. Key considerations:

  • Carbon content is low (C ≤ 0.22), which favors good weldability and low preheat requirements for typical thicknesses.
  • Hardenability is low; therefore, risk of hard, brittle heat-affected zones is limited compared with higher-carbon steels.
  • Deoxidation and residuals influence hydrogen uptake and inclusion content; Q235B’s production controls to meet impact testing tend to reduce inclusion size and oxygen-related defects, which can meaningfully improve weldability in terms of cracking resistance and HAZ toughness.

Useful weldability indices (interpret qualitatively): - Carbon equivalent for IIW: $$CE_{IIW} = C + \frac{Mn}{6} + \frac{Cr+Mo+V}{5} + \frac{Ni+Cu}{15}$$ - Lower $CE_{IIW}$ implies easier weldability with reduced need for preheat/postheat. - International parameter $P_{cm}$: $$P_{cm} = C + \frac{Si}{30} + \frac{Mn+Cu}{20} + \frac{Cr+Mo+V}{10} + \frac{Ni}{40} + \frac{Nb}{50} + \frac{Ti}{30} + \frac{B}{1000}$$ - $P_{cm}$ is used to assess susceptibility to cold cracking; typical Q235 grades give low values and are not prone to hydrogen-assisted cold cracking under normal practices.

Interpretation: Both grades generally give low $CE_{IIW}$ and $P_{cm}$ values because they are low-carbon and minimally alloyed. Q235B’s lower residual oxygen and smaller inclusions can yield slightly better HAZ toughness and lower susceptibility to weld-induced brittleness, particularly in constrained or low-temperature service.

6. Corrosion and Surface Protection

  • Q235A and Q235B are plain carbon steels (non-stainless). They rely on coatings and design measures for corrosion protection.
  • Typical protective strategies:
  • Hot-dip galvanizing for long-term outdoor exposure.
  • Protective paints and primers (epoxy, polyurethane) in industrial environments.
  • Surface treatments (cold-rolled/shot-blasting) to improve coating adhesion.
  • Stainless-steel corrosion indices such as PREN are not applicable to Q235 grades because they contain negligible chromium, molybdenum, or nitrogen for passive film formation. $$\text{PREN} = \text{Cr} + 3.3 \times \text{Mo} + 16 \times \text{N}$$
  • This index is relevant only for stainless alloys and therefore not meaningful for Q235.

7. Fabrication, Machinability, and Formability

  • Formability: Low-carbon content and a ductile ferritic matrix make both grades easy to bend, roll, and form for plates and sections. Q235B’s better notch toughness can reduce edge-cracking risk when forming tight radii or when working at lower temperatures.
  • Machinability: Q235 steels machine well with standard tooling; machinability grades vary little between A and B unless specific residual elements are present. Cutting speeds and feeds should match mild-steel practice.
  • Finishing: Surface quality is governed by rolling and pickling. Q235B’s production practices to meet impact testing may yield marginally better internal soundness and surface consistency for welding and finishing.

8. Typical Applications

Q235A – Typical Uses Q235B – Typical Uses
General structural components where impact risk is low: non-critical brackets, frames, building sections, light machinery parts Structural members requiring minimum low-temperature toughness or where impact testing is specified: certain bridge components, guard rails, welded frames exposed to cooler climates
Sheet and plate for fabrication where cost is primary driver and impact exposure is limited Welded structural assemblies where predictable notch toughness is important (specifying engineers call for tested material)
General-purpose low-cost rolled sections and profiles Structural plates and profiles where purchaser requires Charpy V-notch acceptance at 0°C

Selection rationale: - Choose Q235A where cost and availability dominate and service conditions do not impose low-temperature impact requirements. - Choose Q235B where code or application requires a demonstrated impact-energy level (commonly at 0°C) or where improved toughness is desired due to potential impact or notch stress.

9. Cost and Availability

  • Cost: Both grades are economically priced compared with alloy steels. Q235A is typically the least expensive because it avoids the additional processing and testing needed to guarantee impact performance. Q235B carries a modest premium to reflect controlled deoxidation, processing, and impact testing.
  • Availability by product form: Plates, hot-rolled coils, sheets, and structural sections in Q235 are widely available from domestic and international suppliers. Q235B may be slightly less ubiquitous in some product thicknesses or finishes due to testing constraints, but it remains readily obtainable from major mills.
  • Lead times: Additional testing and certification for Q235B can add minor lead time versus Q235A—account for this in procurement schedules when impact certification is required.

10. Summary and Recommendation

Attribute Q235A Q235B
Weldability Excellent (standard low-carbon) Excellent; slightly improved HAZ toughness due to deoxidation practice
Strength–Toughness balance Good for general use; consistent static properties Better controlled notch toughness; same nominal yield
Cost Lower (fewer process controls/tests) Moderate premium for testing and processing

Recommendations: - Choose Q235A if your application is general structural work where impact resistance at low temperature is not required, you need the most cost-effective material, and standard weldability and formability are sufficient. - Choose Q235B if the design or code requires minimum impact energy at approximately 0°C or when you want tighter assurance of notch toughness and internal soundness (for welded structures, components subject to moderate impact, or service in cooler climates).

Final note: Q235A and Q235B share the same base chemistry and nominal strength level, but differ in toughness verification and associated steelmaking controls. Always specify the required impact test temperature and energy (or accept the supplier’s certification) and confirm chemical and mechanical test reports from the mill before procurement or critical fabrication.

Back to blog