LR A vs AH36 – Composition, Heat Treatment, Properties, and Applications

Table Of Content

Table Of Content

Introduction

Engineers, procurement managers, manufacturing planners, and naval architects frequently weigh LR A and AH36 when specifying structural steels for ships, offshore platforms, and heavy marine equipment. Typical trade‑offs in this choice include cost versus performance, weldability versus strength, and fabrication productivity versus in‑service toughness.

The primary technical distinction between these two grades lies in their design targets for yield strength: one is a more conventional mild/structural grade used for general fabrication, while the other is specified as a higher‑strength shipbuilding steel. This difference drives decisions on plate thickness, joining processes, and low‑temperature service capability, which is why LR A and AH36 are commonly compared in design and procurement discussions.

1. Standards and Designations

  • LR A
  • Origin: Lloyd’s Register classification system (commonly referenced as Grade A within several classification societies).
  • Typical standard context: Classification society rules and older shipbuilding specifications; sometimes cross‑referenced to national standards for general structural steel.
  • Steel type: Carbon/mild structural steel (plain carbon/low alloy depending on supplier practice).

  • AH36

  • Origin: ASTM/ABS/other classification systems for shipbuilding steels (commonly encountered as A Grade AH36 under standards like ASTM A131).
  • Typical standard context: Modern shipbuilding and offshore structural standards.
  • Steel type: HSLA (high‑strength low‑alloy) structural steel developed for ships and offshore structures.

Classification: LR A is conventionally a carbon/structural steel; AH36 is an HSLA structural steel designed for elevated yield strength and improved toughness.

2. Chemical Composition and Alloying Strategy

The following table summarizes the elemental emphasis for each grade. Exact compositions vary by supplier and applicable specification; entries describe typical alloying strategy rather than numeric limits.

Element LR A (typical) AH36 (typical)
C (Carbon) Low carbon — designed for basic structural strength and good weldability Low to moderate carbon — controlled to achieve higher yield while retaining weldability
Mn (Manganese) Moderate — deoxidizer and strengthener Moderate to higher than LR A — contributes to strength and hardenability
Si (Silicon) Present as deoxidizer (low) Present as deoxidizer (low)
P (Phosphorus) Controlled low levels for toughness Strictly controlled low levels for toughness
S (Sulfur) Low (controlled) Low (controlled)
Cr, Ni, Mo Typically absent or only trace Usually not primary alloying elements; sometimes trace levels for property consistency
V, Nb, Ti Generally not intentionally added (may be traces) May include microalloying (Nb, V, Ti) in some AH36 variants to improve strength and toughness
B Rarely used Rarely used; not typical in standard AH36
N (Nitrogen) Low Low; controlled to influence strength/toughness when microalloying present

How alloying affects properties: - Carbon and manganese are the principal strength contributors; higher Mn and slightly higher C increase yield and tensile strength but tend to reduce weldability and toughness if not properly controlled. - Microalloying elements (Nb, V, Ti) in AH36‑type steels refine grain size and enable higher strength without excessive carbon; they also improve toughness and resistance to brittle fracture. - Strict control of impurity elements (P, S) is essential in both grades to maintain impact toughness, particularly for marine service in low temperatures.

3. Microstructure and Heat Treatment Response

Typical microstructures and processing responses:

  • LR A
  • Microstructure: Predominantly ferrite with pearlite islands under standard hot‑rolled fabrication. Grain size tends to be coarser compared with microalloyed HSLA steels unless thermomechanical control is applied.
  • Heat treatment: Usually supplied as hot‑rolled, not commonly heat treated further; normalizing can refine grains but is less common for general hull plates.

  • AH36

  • Microstructure: Controlled ferrite‑pearlite with finer grain size compared with LR A; where microalloying and TMCP (thermo‑mechanical controlled processing) are used, a fine granular ferrite or bainitic‑ferrite mix is possible, enhancing strength and toughness.
  • Heat treatment/processing response: AH36 is typically supplied as thermomechanically processed or normalized plate to develop required yield and impact properties. Quenching and tempering is not a standard route for ship steels but could be used for specialty applications to further increase strength at the expense of cost.

Effect of processing: - Normalizing refines grains and increases toughness for both grades. - Thermo‑mechanical rolling (TMCP) used in AH36 variants provides higher strength with good toughness through grain refinement and precipitation control, without large increases in carbon content that would impair weldability. - Quench & tempering yields higher strengths but is not typical for standard LR A or AH36 product forms; it is used mainly where much higher strength or wear resistance is required.

4. Mechanical Properties

Below is a qualitative comparison of the key mechanical properties typically considered at the specification level. Actual properties should be verified against the applicable specification and mill certificates.

Property LR A AH36
Yield Strength Lower (general structural level) Higher (shipbuilding HSLA target)
Tensile Strength Lower to moderate Higher
Elongation (ductility) Good ductility for forming Comparable ductility; often sufficient despite higher strength due to microalloying
Impact Toughness Adequate at moderate temps; limited low‑temperature rating unless specified Higher, with specified Charpy impact requirements for low temps common
Hardness Lower Moderately higher due to higher strength

Interpretation: - AH36 is designed to provide a higher yield and tensile envelope than LR A while maintaining acceptable ductility and improved low‑temperature toughness. This is achieved mainly via composition control and processing, not by dramatically higher carbon. - LR A remains attractive where extreme strength is not required and where forming and welding simplicity are priorities.

5. Weldability

Weldability depends on carbon equivalent and microalloying. Two commonly used illustrative formulas are:

  • Carbon equivalent (IIW): $$CE_{IIW} = C + \frac{Mn}{6} + \frac{Cr+Mo+V}{5} + \frac{Ni+Cu}{15}$$

  • Pcm (weldability index for carbon steels): $$P_{cm} = C + \frac{Si}{30} + \frac{Mn+Cu}{20} + \frac{Cr+Mo+V}{10} + \frac{Ni}{40} + \frac{Nb}{50} + \frac{Ti}{30} + \frac{B}{1000}$$

Qualitative interpretation: - LR A, with generally lower carbon and minimal microalloying, presents excellent weldability with low preheat requirements and minimal risk of hydrogen‑induced cracking in typical fabrication conditions. - AH36 typically has a slightly higher effective hardenability due to controlled higher Mn and possible microalloying. This can increase the carbon equivalent modestly and may require controlled preheat or interpass temperatures and attention to consumables to manage HAZ toughness and avoid cold cracking, particularly on thicker plates or when through‑thickness restraint is high. - In practice, AH36 is engineered to be welded readily using common processes (SMAW, GMAW, SAW) with appropriate procedure qualification; however, welding procedures and often a formal WPS are more frequently required for AH36 than for LR A.

6. Corrosion and Surface Protection

  • Both LR A and AH36 are non‑stainless carbon/low‑alloy steels and require surface protection for corrosion resistance in marine environments.
  • Common protection methods: coatings (epoxy, polyurethane), cathodic protection, and galvanizing where appropriate for non‑immersed parts.
  • Stainless indices such as PREN are not applicable to these grades; for reference when stainless steels are considered: $$\text{PREN} = \text{Cr} + 3.3 \times \text{Mo} + 16 \times \text{N}$$
  • Selection guidance: AH36’s slightly different chemistry does not materially change corrosion resistance compared with LR A; selection should be driven by mechanical requirement and then by appropriate surface protection system design per service environment.

7. Fabrication, Machinability, and Formability

  • Forming and bending: LR A’s lower yield and lower strength make it easier to form and cold bend without springback control; AH36 will require higher forming forces and more attention to bend radii to avoid cracking, though modern AH36 grades with good ductility are formable within recommended limits.
  • Cutting and drilling: Both grades machine similarly using standard tooling; AH36 may be marginally more abrasive if microalloy precipitates are present.
  • Welding and fit‑up: LR A tolerates larger gap variation and faster weld travel speeds; AH36 benefits from controlled fit‑up and qualified procedures, particularly on thick plates.
  • Surface finishing: Both accept standard surface treatments; AH36 may require additional surface inspection if fatigue or brittle fracture risk is a concern.

8. Typical Applications

LR A (typical uses) AH36 (typical uses)
General ship structural components where high strength is not mandatory (secondary members, interiors) Hull plating, primary structural members, and areas requiring higher yield strength
Onshore structural steel for light to medium duty applications Offshore platform structures, deck and hull plating subject to higher stresses
Non‑critical brackets, fittings, and general fabrication Where weight savings or thickness reductions are desired through higher strength material

Selection rationale: - Choose LR A for applications emphasizing cost effectiveness, ease of fabrication, and where very high structural strength and low‑temperature toughness are not necessary. - Choose AH36 when higher yield strength, improved toughness (especially at low temperature), and the ability to reduce plate thickness/weight are important considerations.

9. Cost and Availability

  • Cost: LR A is generally less expensive on a per‑ton basis because it is a more conventional structural steel with lower processing demand. AH36 typically carries a premium due to tighter chemistry control, possible TMCP routes, and testing/certification requirements.
  • Availability: Both grades are widely available from plate mills serving the maritime and structural markets. AH36 is commonly stocked where shipbuilding or offshore fabrication is concentrated; LR A remains widely available for general fabrication.
  • Product forms: Both are supplied as hot‑rolled plate; AH36 may also be offered in thermomechanically controlled plate variants, which can affect lead time and cost.

10. Summary and Recommendation

Characteristic LR A AH36
Weldability Very good; simple procedures Good with qualified WPS and sometimes preheat control
Strength–Toughness balance Moderate strength, adequate toughness Higher strength with improved low‑temperature toughness
Cost Lower Higher

Recommendation: - Choose LR A if you need a cost‑effective, easy‑to‑fabricate structural steel for non‑critical ship or onshore applications where high yield strength and enhanced low‑temperature toughness are not required. - Choose AH36 if the component or structure demands higher yield and tensile strength, improved resistance to brittle fracture in low‑temperature marine service, or if reducing plate thickness (and therefore weight) is a project objective and the budget permits a higher material and fabrication control cost.

Final note: Always validate final selection against the project’s classification society rules, welding procedure qualifications, material mill certificates, and specific service temperature and fatigue requirements. When in doubt, request mill test reports and consult fabrication and welding specialists to define preheat, post‑weld heat treatments (if any), and quality assurance steps appropriate to the chosen grade.

Back to blog

Leave a comment