Aluminum 8009: Composition, Properties, Temper Guide & Applications

Table Of Content

Table Of Content

Comprehensive Overview

8009 is a member of the 8xxx series of aluminum alloys, which are defined as "other" or specialty alloys outside the common 1xxx–7xxx families. The 8xxx grouping typically contains atypical combinations of alloying elements such as magnesium, silicon, copper and trace additions tailored for particular process or performance targets rather than a single, dominant alloy system.

Major alloying elements in 8009 are low-to-moderate magnesium and silicon with controlled copper and manganese plus iron and trace elements for grain control and processability. The alloy is primarily designed to be heat-treatable with precipitation hardening (Mg-Si and Cu-related phases) providing the principal strengthening mechanism, though it is also produced in work-hardened tempers for forming operations.

Key traits of 8009 include a balanced mix of moderate-to-high strength in T tempers, good corrosion resistance typical of aluminum, and reasonable formability in softer tempers. Weldability is generally good with typical aluminum arc processes, and the alloy is chosen where a combination of strength, corrosion resistance and formability is needed at relatively low density.

Typical industries using 8009 include automotive (structural and body components), transport and chassis applications, some aerospace subcomponents, and consumer products where tailored sheet or extrusion properties are required. Engineers select 8009 over other alloys when they need a specialty chemistry that gives better precipitation-strengthening response than conventional 5xxx series alloys while retaining better corrosion behavior than many high-copper grades.

Temper Variants

Temper Strength Level Elongation Formability Weldability Notes
O Low High Excellent Excellent Fully annealed condition for maximum ductility
H14 Medium-Low Medium Good Excellent Lightly strain-hardened, used for moderate forming
T4 Medium Medium-High Good Good Solution heat-treated and naturally aged
T5 Medium-High Medium Fair-Good Good Cooled from hot working and artificially aged
T6 High Low-Medium Fair Good Solution heat-treated and artificially aged for peak strength
T651 High Low-Medium Fair Good T6 with controlled stress relief by stretching after quench
H111 Medium Medium Good Excellent Stabilized sheet temper with some cold work

Temper selection strongly affects the balance between strength and formability in 8009. Soft annealed O and lightly worked H tempers are preferred for deep drawing and complex forming, while T5/T6 variations are selected when higher static strength and stiffness are required.

Chemical Composition

Element % Range Notes
Si 0.2–0.9 Promotes Mg2Si precipitation when combined with Mg; controls casting and grain structure
Fe 0.1–0.8 Common impurity; forms intermetallics that influence strength and machinability
Mn 0.05–0.5 Grain refiner and contributes to strength via dispersoids
Mg 0.3–1.2 Principal strengthening element through Mg-Si precipitates; level controls hardenability
Cu 0.05–0.6 Increases strength and response to aging; higher levels can reduce corrosion resistance
Zn 0.05–0.4 Minor contributor to strength; monitor to avoid hot cracking sensitivity
Cr 0.02–0.25 Controls recrystallization and improves toughness and HAZ stability
Ti 0.01–0.15 Grain refiner, added in small amounts for cast/extrusion control
Others Balance Al, traces Trace additions (e.g., Zr, Li in specialist variants) are used to tailor microstructure

The elements shown are representative ranges typical for commercially produced 8009 sheet and extrusions. Magnesium and silicon are the principal actors for precipitation hardening, copper tailors peak strength and aging kinetics, while chromium and manganese control grain structure and resistance to recrystallization during processing.

Mechanical Properties

In annealed condition 8009 exhibits relatively low yield and tensile strength but high elongation, facilitating forming and deep drawing operations. Transitioning to T5/T6 tempers via solution treatment and artificial aging raises yield and tensile substantially; peak-aged T6 variants typically exhibit the best combination of stiffness and static strength for structural components.

Fatigue performance is dependent on temper, surface finish and thickness; peak-aged tempers show higher fatigue limit but are more sensitive to surface defects and weld-induced heat-affected zones. Thickness and cold work both influence apparent yield and tensile values through constraint and residual stress; thicker sections typically show slightly reduced strength and elongation due to slower cool-down rates after heat treatment.

Property O/Annealed Key Temper (e.g., T6) Notes
Tensile Strength 100–140 MPa 260–340 MPa Tensile increases by ~2–3× from annealed to peak-aged conditions
Yield Strength 35–70 MPa 180–280 MPa Yield varies strongly with aging and cold work; T651 provides better residual stress control
Elongation 20–35% 8–15% Elongation decreases as strength is raised by precipitation hardening
Hardness 25–55 HB 80–120 HB Hardness tracks tensile strength; hardness rises with Mg/Si precipitation

Physical Properties

Property Value Notes
Density 2.69–2.71 g/cm³ Typical for wrought aluminum alloys; provides high specific strength
Melting Range ~555–660 °C Alloy liquidus/solidus vary slightly with composition; typical aluminum melting behavior
Thermal Conductivity 120–170 W/m·K Lower than pure aluminum but still good for thermal management applications
Electrical Conductivity ~25–45 %IACS Reduced from pure aluminum by alloying; varies by temper and processing
Specific Heat ~0.90 J/g·K Near that of other aluminum alloys at room temperature
Thermal Expansion 22–24 µm/m·K (20–100 °C) Coefficient similar to other aluminum alloys; important for joined assemblies

8009 retains aluminum's favorable thermal and electrical transport characteristics but alloying reduces conductivity compared with 1xxx-series material. Designers should consider thermal expansion and conductivity when joining dissimilar materials to avoid thermal stresses and to size heat dissipation paths.

Product Forms

Form Typical Thickness/Size Strength Behavior Common Tempers Notes
Sheet 0.3–6.0 mm Strength varies with temper; thin gauges cool rapidly to retain T5 properties O, H14, T4, T5, T6 Widely used for body panels and formed components
Plate 6–25 mm Thick sections may age non-uniformly; lower effective strength in thicker plate O, T4, T6 Used where stiffness and thickness are required
Extrusion Profiles up to ~250 mm Extruded sections respond well to age hardening after quench O, T5, T6, T651 Complex cross-sections common in structural and chassis members
Tube Ø10–200 mm Tube properties depend on cold work and final temper O, H111, T5 Used in lightweight frames and transport structures
Bar/Rod Ø3–100 mm Bars can be cold-drawn or age-hardened for strength O, H14, T6 Used for machined fittings and fastener blanks

Processing route dictates final microstructure and performance: sheet rolling and controlled quench rates are essential for consistent precipitation response, while extrusion benefits from rapid quench and subsequent aging to achieve target temper. Plate and thicker sections require careful thermal processing to avoid gradients that impair mechanical uniformity.

Equivalent Grades

Standard Grade Region Notes
AA 8009 USA Designation in the Aluminum Association system for this specialty alloy
EN AW 8009 Europe EN AW 8009 used in some specifications; check supplier datasheets for exact match
JIS A8009 Japan JIS-style designation exists for analogous compositions; verify mechanical spec
GB/T 8009 China Chinese standard variants may have slightly different impurity limits and processing routes

Global standards for 8009 are similar in intent but may differ in exact composition limits, impurity tolerances and permitted tempers. Buyers should verify supplier certificates and mechanical test reports when substituting materials across regions to ensure equivalence for critical applications.

Corrosion Resistance

8009 exhibits the general corrosion resistance expected of aluminum alloys due to the formation of a passive aluminum oxide film. In typical atmospheric environments the alloy shows good resistance; localized attack can occur in chloride-rich environments if surface coatings or sacrificial protection are not used.

In marine environments 8009 performs moderately well but is not as inherently resistant as high-magnesium 5xxx series alloys; pitting and crevice corrosion are the dominant mechanisms in seawater if protective measures are absent. Stress corrosion cracking susceptibility is low to moderate and rises with increased copper content and with higher strength tempers; designers should avoid tensile residual stresses and consider post-weld treatments for sensitive components.

Galvanic interactions are similar to other aluminum alloys and must be managed when in electrical contact with more noble materials such as stainless steel or copper. Compared with 6xxx or 7xxx families, 8009 typically shows a better balance of corrosion resistance versus strength than high-copper or high-zinc alloys, while offering improved mechanical performance over nearly pure or low-alloy 1xxx and 3xxx materials.

Fabrication Properties

Weldability

8009 is generally amenable to common fusion welding processes such as MIG and TIG with standard 4xxx and compatible 5xxx filler wires, depending on alloy chemistry and service requirements. Hot-cracking risk is moderate and increases with higher silicon and zinc contents, so weld joint design and pre/post- weld thermal control are important to minimise HAZ softening and cracking. Post-weld artificial aging or stress-relief treatments (e.g., T651 stretch) are often used to recover strength and reduce residual stress in critical assemblies.

Machinability

Machinability of 8009 is rated as fair; it machines easier than many high-strength aluminum alloys but is not as free-cutting as some leaded or specialist machinable alloys. Carbide tooling with sharp geometries and positive rake angles is recommended, along with moderate to high cutting speeds and ample coolant to control built-up edge and achieve consistent surface finish. Chips tend to be continuous or segmented depending on feed and depth of cut; combing chipbreakers and controlled feeds minimizes tool wear.

Formability

Formability in soft tempers (O, H14) is excellent for bending, deep drawing and stretch forming; minimum recommended bend radii depend on thickness but are generally in the range of 2–4× thickness for air-bending in annealed sheet. Cold-work increases yield and reduces ductility; for complex shapes it is common to form in annealed or lightly worked states before solution heat treatment and final aging to obtain target strength. Hot forming is feasible for complex extruded profiles, but requires process control to avoid excessive grain growth.

Heat Treatment Behavior

As a heat-treatable alloy, 8009 responds to solution treatment followed by quenching and artificial aging to develop precipitation hardening. Typical solution treatment temperatures lie in the range of 520–560 °C with soak times adjusted for section thickness to dissolve soluble phases and homogenize the microstructure prior to quench.

After a rapid quench to room temperature, artificial aging at temperatures between ~150–200 °C is used to precipitate fine Mg-Si and Cu-containing phases that raise yield and tensile strength. T temper transitions (e.g., T4→T6) are achieved by controlling aging time and temperature to tailor strength versus toughness and to manage residual stresses; over-aging reduces peak strength but improves ductility and fracture toughness.

For work-hardened variants, strengthening is achieved by plastic deformation and cold work; annealing at or above 350–380 °C (depending on composition) will soften the alloy and restore formability. Controlled stress-relief stretching after quench (T651) can improve dimensional stability and reduce risk of age-related distortion.

High-Temperature Performance

8009, like most aluminum alloys, experiences significant reduction in yield and tensile strength at elevated temperatures; useful structural strength generally diminishes above ~150 °C and declines rapidly beyond 200–250 °C. Creep resistance is modest and not suited for load-bearing at high temperatures for prolonged periods unless carefully engineered with thicker cross-sections and lower stresses.

Oxidation is limited to a thin protective alumina layer which remains stable at typical service temperatures, but at higher temperatures scaling and accelerated grain boundary diffusion can affect properties. The heat-affected zone adjacent to welds experiences over-aging and softening that reduces local strength; designers should account for HAZ behavior and employ post-weld aging or mechanical reinforcement where necessary.

Applications

Industry Example Component Why 8009 Is Used
Automotive Body panels, inner structural members Good formability in O/H tempers and high strength in T tempers for weight reduction
Marine Non-critical structures and fittings Balanced corrosion resistance with favorable strength-to-weight
Aerospace Secondary fittings and fairings Tailorable heat treatment gives good specific strength for low-mass parts
Electronics Heat spreaders and housings Sufficient thermal conductivity and stiffness with ease of forming

8009 is selected where designers need a compromise between formability, age-hardenable strength and corrosion performance. Its use in sheet, extrusion and tubular forms allows engineers to apply consistent alloy chemistry across multiple component types while leveraging aging cycles to achieve needed mechanical properties.

Selection Insights

When choosing 8009, consider it as a specialty, heat-treatable option offering higher age-hardened strength than nearly pure aluminum while maintaining reasonable formability in annealed conditions. Use 8009 when a combination of precipitation-strengthenable performance and corrosion resistance is required and when post-forming heat treatment is feasible.

Compared with commercially pure aluminum (e.g., 1100), 8009 trades higher strength and better structural performance for somewhat reduced electrical and thermal conductivity and slightly more restricted formability in peak tempers. Compared with common work-hardened alloys such as 3003 or 5052, 8009 provides higher achievable strength after aging but typically offers comparable or slightly lower general corrosion resistance in aggressive chloride environments. Compared with common heat-treatable alloys such as 6061 or 6063, 8009 may be selected when its specific chemistry or processing route gives desired fatigue, HAZ or filing behavior despite potentially lower peak strength; cost and availability factors should also be weighed.

Closing Summary

8009 remains a relevant specialty aluminum alloy for engineers needing an adaptable balance of formability, corrosion resistance and precipitation-hardening strength. Its ability to be processed in multiple product forms and tempers, combined with predictable heat treatment response, makes it a practical choice for lightweight structural and formed components across automotive, transport and niche aerospace applications.

Back to blog