High-Strength Low-Alloy Structural Steel

ASTM A572 Grade 50 is a high-strength, low-alloy (HSLA) structural steel designed for superior strength-to-weight ratio and excellent weldability. This premium grade steel offers enhanced mechanical properties while maintaining excellent formability and corrosion resistance for demanding structural applications.

MetalZenith Manufacturing Excellence

As a leading steel manufacturer, MetalZenith produces ASTM A572 Grade 50 using state-of-the-art controlled rolling and thermomechanical processing technologies. Our advanced electric arc furnaces and continuous casting systems ensure precise chemical composition control and superior metallurgical properties. Our integrated quality management system guarantees consistent mechanical properties and dimensional accuracy across all product forms.

Key Applications

  • High-rise building construction and structural frameworks
  • Bridge construction and infrastructure projects
  • Heavy machinery and equipment manufacturing
  • Transportation and automotive structural components
  • Offshore and marine structural applications

Quality Assurance & Certifications

MetalZenith maintains ISO 9001:2015, ISO 14001, and OHSAS 18001 certifications. Every batch undergoes comprehensive testing including chemical analysis, mechanical property verification, ultrasonic testing, and dimensional inspection. Our products meet ASTM A572, EN 10025, and JIS G3106 international standards with full traceability documentation and mill test certificates.

عرض التفاصيل الكاملة

20 Years Experience | 1000+ Brand Partners | Full Customization

We have 20 years of industry experience, have partnered with over 1,000 brands, and support any customization needs.

Technical Specifications

Product Overview

Metallurgical Characteristics

ASTM A572 Grade 50 is a high-strength, low-alloy (HSLA) structural steel that achieves its superior mechanical properties through controlled rolling and microalloying techniques. The steel features a fine-grained ferrite-pearlite microstructure with precipitation strengthening from vanadium, niobium, and titanium carbides and nitrides. This metallurgical design provides an optimal balance of strength, toughness, and weldability.

Manufacturing Process

MetalZenith produces ASTM A572 Grade 50 using advanced electric arc furnace technology followed by ladle refining and continuous casting. The steel undergoes controlled rolling in the austenite recrystallization and non-recrystallization temperature ranges, followed by accelerated cooling to achieve optimal grain refinement. Our thermomechanical controlled processing (TMCP) ensures consistent mechanical properties and enhanced toughness while maintaining excellent weldability characteristics.

Heat Treatment Options

ASTM A572 Grade 50 is typically supplied in the as-rolled condition, providing optimal mechanical properties without additional heat treatment. For specific applications requiring stress relief, the steel can be heat treated at 580-650°C for 1-2 hours per 25mm of thickness. Normalizing at 900-950°C followed by air cooling can be performed to refine grain structure and improve toughness for critical applications.

Welding Characteristics

The steel exhibits excellent weldability with all common welding processes including SMAW, GMAW, FCAW, and SAW. The low carbon equivalent (CE ≤ 0.45) minimizes the risk of cold cracking and reduces preheating requirements. For sections thicker than 25mm, preheating to 100-150°C is recommended. Post-weld heat treatment is generally not required for most structural applications.

Quality Standards & Testing

MetalZenith maintains comprehensive quality control throughout the manufacturing process, including real-time chemical composition monitoring, mechanical property verification, and non-destructive testing. All products undergo ultrasonic testing, dimensional inspection, and surface quality assessment. Our quality management system complies with ISO 9001:2015, ISO 14001, and OHSAS 18001 standards, ensuring consistent product quality and full traceability documentation.

🧪 Chemical Composition

ElementComposition (%)Notes
Carbon (C)≤ 0.23Maximum
Manganese (Mn)1.35 maxStrength enhancement
Phosphorus (P)≤ 0.030Maximum
Sulfur (S)≤ 0.030Maximum
Silicon (Si)0.40 maxDeoxidizer
Copper (Cu)0.35 maxCorrosion resistance
Nickel (Ni)0.40 maxToughness improvement
Chromium (Cr)0.30 maxHardenability
Molybdenum (Mo)0.15 maxStrength enhancement
Vanadium (V)0.10 maxGrain refinement
Niobium (Nb)0.05 maxPrecipitation strengthening
Titanium (Ti)0.15 maxGrain refinement

⚙️ Mechanical Properties

PropertyValueTest Method
Yield Strength (0.2% offset)≥ 345 MPa (50 ksi)ASTM A370
Tensile Strength450-590 MPa (65-85 ksi)ASTM A370
Elongation in 200mm≥ 18%ASTM A370
Elongation in 50mm≥ 21%ASTM A370
Brinell Hardness170-220 HBASTM E10
Charpy V-Notch Impact (20°C)≥ 27 J (20 ft-lb)ASTM A370
Charpy V-Notch Impact (-40°C)≥ 20 J (15 ft-lb)ASTM A370
Fatigue Limit (10&sup7; cycles)160-180 MPaASTM D7791
Reduction of Area≥ 50%ASTM A370
Young's Modulus200-210 GPaASTM E111
Shear Modulus80-85 GPaASTM E143
Poisson's Ratio0.27-0.30ASTM E132

🔬 Physical Properties

PropertyValueTemperature
Density7.85 g/cm³20°C
Melting Point1510-1540°C-
Thermal Conductivity54 W/m·K20°C
Thermal Conductivity35 W/m·K500°C
Specific Heat Capacity500 J/kg·K20°C
Thermal Expansion Coefficient12×10-6/K20-100°C
Thermal Expansion Coefficient14×10-6/K20-500°C
Electrical Resistivity0.16 µΩ·m20°C
Magnetic PermeabilityFerromagnetic20°C
Curie Temperature770°C-
Thermal Diffusivity13.8 mm²/s20°C
Emissivity0.85-0.95Oxidized surface

📏 Product Specifications

SpecificationAvailable OptionsStandards
Product FormsPlates, Sheets, Bars, Beams, Channels, Angles, TubesASTM A572
Plate Thickness6-200mm (0.25-8 inches)ASTM A572
Sheet Thickness1.5-6mm (0.06-0.25 inches)ASTM A572
Bar Diameter10-300mm (0.4-12 inches)ASTM A572
Standard Widths1000-3000mm (40-120 inches)ASTM A6
Standard Lengths6000-12000mm (20-40 feet)ASTM A6
Surface FinishHot Rolled, Cold Rolled, Pickled, Shot BlastedASTM A6
Edge ConditionMill Edge, Slit Edge, Sheared EdgeASTM A6
Thickness Tolerance±0.3mm (±0.012 inches)ASTM A6
Width Tolerance±3mm (±0.125 inches)ASTM A6
Length Tolerance±6mm (±0.25 inches)ASTM A6
Flatness5mm/m maximum deviationASTM A6
International StandardsASTM A572, EN 10025-2 (S355), JIS G3106 (SM490)Multiple

Let Us Create Success for Your Project

Professional Team, Premium Products, Complete Service - Your Project Success is Our Mission

Our Advantages in Processing ASTM A572 Grade 50

Manufacturing Advantage 1

Advanced Thermomechanical Processing

MetalZenith employs cutting-edge controlled rolling and accelerated cooling technologies to achieve optimal grain refinement and precipitation strengthening. Our proprietary heat treatment processes ensure consistent mechanical properties and enhanced toughness while maintaining excellent weldability characteristics.

Comprehensive Quality Control System

Our integrated quality management system features real-time chemical composition monitoring, automated mechanical testing, and advanced non-destructive testing capabilities. Every product undergoes rigorous inspection protocols including ultrasonic testing, dimensional verification, and surface quality assessment to guarantee compliance with international standards.

Manufacturing Advantage 2
Manufacturing Advantage 3

Flexible Customization & Global Supply

MetalZenith offers extensive customization options including special dimensions, surface treatments, and mechanical property modifications. Our global distribution network and strategic inventory locations ensure rapid delivery worldwide, while our technical support team provides comprehensive engineering assistance for specific application requirements.

YOUR TRUSTED STEEL

MANUFACTURING PARTNER

20
Years Experience
Leading Steel Manufacturing & Distribution
1000+
Brand Partners
Trusted by Global Industry Leaders
Full
Customization
Tailored Solutions for Every Project
50M+
Tons Delivered
High-Quality Steel Products Worldwide
95%
Client Retention
Long-term Partnership Success
ISO 9001
Certified Quality
International Standards Compliance
20
Years Experience
Leading Steel Manufacturing & Distribution
1000+
Brand Partners
Trusted by Global Industry Leaders
Full
Customization
Tailored Solutions for Every Project
50M+
Tons Delivered
High-Quality Steel Products Worldwide
95%
Client Retention
Long-term Partnership Success
ISO 9001
Certified Quality
International Standards Compliance
GET IN TOUCH

Quick Inquiry

Industries We Serve

Professional steel solutions across major industries

Construction

High-rise Buildings • Infrastructure • Commercial Real Estate

Oil & Gas

Pipeline Systems • Storage Equipment • Refinery Facilities

Manufacturing

Precision Machinery • Industrial Equipment • Automation Systems

Automotive

Body Structure • Chassis Components • Engine Parts

Shipbuilding

Hull Structure • Marine Engineering • Port Equipment

Energy & Power

Power Generation • Transmission Towers • Renewable Energy

Aerospace

Aircraft Materials • Precision Components • Special Alloys

Railway

Track Systems • Vehicle Manufacturing • Infrastructure

Qualifications & Certifications

Client logo
Client logo
Client logo
Client logo
Client logo