SPCC vs SPCE – Composition, Heat Treatment, Properties, and Applications

Table Of Content

Table Of Content

Introduction

SPCC and SPCE are two widely used JIS-designated cold-rolled carbon steel grades frequently specified in sheet and coil form for manufacturing, automotive, appliance, and general fabrication work. Engineers, procurement managers, and manufacturing planners often weigh trade-offs between cost, formability, and strength when selecting between them: SPCC is a general-purpose cold-rolled commercial-quality steel, while SPCE is tailored for enhanced deep-drawing performance and higher ductility. The principal distinction lies in the mechanical behavior associated with tensile and forming performance — SPCE is optimized for stretchability and uniform elongation, whereas SPCC is optimized for economical production and moderate strength. Because both are cold-rolled, low-alloy carbon steels, they are commonly compared during material selection for sheet-metal forming, stamping, and welded assemblies.

1. Standards and Designations

  • JIS: Primary designation where both grades originate
  • SPCC — Cold-reduced commercial quality steel sheet and strip (JIS G3141)
  • SPCE — Cold-reduced deep-drawing steel sheet and strip (JIS G3141)
  • International equivalents/near-equivalents (by function, not direct one-to-one chemical match):
  • EN/ISO: cold-rolled mild steels (e.g., DC01/DC03 type families)
  • ASTM/ASME: broadly comparable to low-carbon cold-rolled steels (e.g., A366/A611 family for commercial steels; actual equivalence requires supplier MTC)
  • GB (China): similar commercial and deep-drawing designations exist but check exact chemical/microstructure requirements
  • Classification: Both SPCC and SPCE are plain low-carbon cold-rolled carbon steels (not alloy steels, not stainless, and not HSLA).

2. Chemical Composition and Alloying Strategy

Table: Relative presence of alloying and impurity elements (qualitative; verify mill test certificate for exact values).

Element SPCC (commercial cold-rolled) SPCE (deep-drawing cold-rolled) Notes
C (Carbon) Moderate (higher than SPCE) Lower (reduced carbon to improve ductility) C controls strength and hardenability; lower C improves formability.
Mn (Manganese) Controlled (strength and deoxidation) Controlled (similar levels; optimized for ductility) Mn provides strength but excessive Mn increases hardenability.
Si (Silicon) Low (deoxidation) Low (kept low to aid drawability) Si largely serves as deoxidizer; high Si can reduce surface quality.
P (Phosphorus) Trace (kept minimal) Trace (kept minimal) P increases strength but can reduce ductility and cause brittleness.
S (Sulfur) Trace (controlled; may be slightly higher for machinability grades) Trace (kept low for formability) S improves machinability but harms drawability and surface quality.
Cr, Ni, Mo, V, Nb, Ti, B Generally absent or present only as trace microalloying Generally absent or trace microalloying These are not characteristic alloying elements for SPCC/SPCE; some suppliers may add trace elements for specific applications.
N (Nitrogen) Trace Trace Nitrogen is typically controlled to avoid embrittlement; not a design feature here.

Alloying strategy: Both grades use low overall alloy content. The emphasis for SPCE is on reduced carbon and tighter control of P/S to maximize uniform elongation and avoid surface defects during deep drawing. SPCC allows slightly higher carbon and relaxed impurity tolerances consistent with general commercial use and lower cost.

3. Microstructure and Heat Treatment Response

  • Typical microstructures:
  • Both SPCC and SPCE are manufactured by cold rolling followed by annealing. The dominant microstructure after appropriate annealing is ferritic with a low fraction of pearlite or stress-relief conditions depending on processing.
  • SPCE, due to lower carbon and optimized anneal cycles, tends to have a more uniform, equiaxed ferrite grain structure with fewer hard phases, supporting better stretchability and reduced tendency for localized necking.
  • Heat treatment response and processing:
  • Annealing (recrystallization anneal) is the standard treatment for both grades to restore ductility after cold reduction. Annealing temperature and time are chosen to achieve desirable grain size and to relieve work hardening.
  • Thermo-mechanical processing and controlled atmosphere anneals are used by some mills to refine texture and enhance deep-drawing properties, particularly for SPCE.
  • Quenching and tempering or hardening treatments are not typical for these grades because they are low-carbon cold-rolled steels intended for ductile sheet applications rather than heat-treated structural parts.
  • Effect of processing:
  • Higher cold reduction increases strength by work hardening; subsequent anneal restores ductility. SPCE is processed to achieve a balance favoring elongation and uniform deformation rather than maximum tensile strength.

4. Mechanical Properties

Table: Qualitative comparison of common mechanical attributes (specific values vary with temper, thickness, and supplier—consult MTC).

Property SPCC SPCE Practical implication
Tensile Strength Moderate Similar or slightly lower SPCC may exhibit marginally higher tensile strength in the same temper due to marginally higher C or work-hardening response.
Yield Strength Moderate Slightly lower SPCE priority is lower yield to allow deeper stretching before the onset of permanent localized deformation.
Elongation (Uniform and Total) Good Higher (better drawability) SPCE provides improved total and uniform elongation—critical for deep drawing and complex stamping.
Impact Toughness Adequate for sheet applications Adequate; similar or slightly better at room temperature Both are intended for sheet forming; neither is optimized for low-temperature impact service.
Hardness Moderate (slightly higher) Slightly lower (softer) Hardness correlates with strength; softer SPCE enables better formability.

Interpretation: SPCE is engineered to provide superior ductility and stretchability at the expense of a small reduction in strength and hardness compared with SPCC. For applications requiring deeper draw radii, complex geometry, or minimized springback, SPCE is typically preferred. SPCC is chosen when cost and adequate strength for simple forming are primary concerns.

5. Weldability

  • General remarks:
  • Both SPCC and SPCE are low-carbon steels and are broadly weldable with standard fusion and resistance welding methods. Their low alloying content reduces risk of hard, untempered martensite in the heat-affected zone (HAZ).
  • Weldability depends on carbon-equivalent measures and on the presence of residual alloying/microalloying.
  • Carbon-equivalent and weldability indices:
  • A commonly used index for qualitative assessment of weldability is: $$CE_{IIW} = C + \frac{Mn}{6} + \frac{Cr+Mo+V}{5} + \frac{Ni+Cu}{15}$$ Lower $CE_{IIW}$ values indicate better weldability in terms of reduced cold-cracking risk.
  • A more detailed predictive formula is: $$P_{cm} = C + \frac{Si}{30} + \frac{Mn+Cu}{20} + \frac{Cr+Mo+V}{10} + \frac{Ni}{40} + \frac{Nb}{50} + \frac{Ti}{30} + \frac{B}{1000}$$ $P_{cm}$ is used in some standards to judge preheat and weldability requirements.
  • Qualitative interpretation:
  • Because SPCE typically has slightly lower carbon and tightly controlled impurities, it often exhibits marginally better weldability in terms of susceptibility to cold cracking and need for preheat. In practice, for thin sheet applications and common welding processes (MIG/MAG, TIG, resistance spot welding), both grades weld satisfactorily without special precautions, provided proper joint design, fit-up, and welding parameters are used.
  • For heavy gauge, multi-pass welds, or when microalloying elements are present, evaluate $CE_{IIW}$ and $P_{cm}$ and follow preheat/postheat recommendations.

6. Corrosion and Surface Protection

  • Both SPCC and SPCE are non-stainless carbon steels; inherent corrosion resistance is limited. Typical protection strategies:
  • Hot-dip galvanizing (GI), electro-galvanizing (EG), or pre-treatment with conversion coatings before painting.
  • Paint systems (epoxy, polyester) and powder coatings for atmospheric environments.
  • OEMs often specify surface treatments (zinc, organic coatings) depending on outdoor exposure and required service life.
  • Stainless indices:
  • PREN (Pitting Resistance Equivalent Number) is not applicable to these grades because they are not stainless steels; thus: $$\text{PREN} = \text{Cr} + 3.3 \times \text{Mo} + 16 \times \text{N}$$ is irrelevant to SPCC/SPCE as their Cr, Mo, and N contents are negligible.
  • Practical note: For forming operations that produce bare cuts or exposed edges, consider post-forming coatings or edge-sealing treatments to avoid localized corrosion.

7. Fabrication, Machinability, and Formability

  • Formability:
  • SPCE excels in deep drawing, complex stamping, and operations that require high uniform elongation and minimal earing. It is selected when tight drawing radii, high reductions in area, or bakery-shaped parts are required.
  • SPCC handles general forming tasks—bending, mild stamping, and panel work—where extreme drawability is not required.
  • Machinability:
  • Cold-rolled low-carbon steels are generally machinable with standard tooling; SPCC may machine marginally better if sulfur or machinability-enhancing elements are present, but such additions are uncommon for quality cold-rolled sheet.
  • Bending and springback:
  • SPCE's lower yield strength and higher ductility can reduce springback in some cases, but process setup must still consider thickness and tool geometry.
  • Surface finish and post-processing:
  • Both offer good surface quality for painting and plating after appropriate cleaning and pre-treatment. SPCE is often produced with tighter surface quality controls for visible or painted components.

8. Typical Applications

Table: Common applications by grade

SPCC (commercial cold-rolled) SPCE (deep-drawing cold-rolled)
General panels, housings, simple stamped parts, furniture components, chassis panels Automotive inner panels, fuel tanks (where formability matters), complex deep-drawn kitchenware, recessed lighting housings
Appliance bodies and non-critical stamped components Complex stamped and stretched components requiring high uniform elongation (e.g., automotive inner doors, complex shells)
Structural sheet where cost is a driver and forming is simple High-draw components with tight aesthetic or dimensional tolerances after forming

Selection rationale: Choose SPCE when geometry demands high uniform elongation and minimal localized thinning; choose SPCC for cost-sensitive, less severe forming tasks or where slightly higher as-formed strength is beneficial.

9. Cost and Availability

  • Cost:
  • SPCC is typically the more economical option due to broader production volumes and less stringent composition controls.
  • SPCE may carry a modest premium because of tighter chemical control and processing to achieve superior drawability.
  • Availability by product form:
  • Both grades are widely available in coils and cut-to-length cold-rolled sheets. Availability varies by region and by supplier inventory; SPCC is more commonly stocked as a general-purpose grade.
  • Lead time and procurement tips:
  • For high-volume production, negotiating coil batches with consistent mill test certificates (MTCs) reduces variability. For deep-draw production, request supplier data and forming trials to ensure consistent performance.

10. Summary and Recommendation

Table: Quick comparison

Attribute SPCC SPCE
Weldability Good Slightly better or comparable
Strength–Toughness balance Moderate strength with adequate toughness Lower yield/higher ductility—better toughness in forming
Cost Lower (economical) Slightly higher (premium for formability)

Recommendations: - Choose SPCE if: - Your application requires deep drawing, high uniform elongation, complex stamping with tight radii, or minimal localized thinning. - You prioritize formability and consistent stretchability over marginal increases in as-formed tensile strength. - Choose SPCC if: - Your application involves simpler forming operations, cost sensitivity, and general-purpose stamped or formed parts where moderate strength is sufficient. - You need widely available sheet material with good surface quality for painting or plating at lower cost.

Final note: SPCC and SPCE are close cousins in the cold-rolled, low-carbon steel family. The decisive factor in selection is forming behavior driven by tensile and elongation performance. For any critical design, always request the supplier’s mill test certificate and, when possible, conduct forming trials and weldability tests with the exact temper and thickness to confirm behavior under your specific process conditions.