DX51D+Z vs DX51D+ZF – Composition, Heat Treatment, Properties, and Applications

Table Of Content

Table Of Content

Introduction

DX51D+Z and DX51D+ZF are closely related cold-rolled low‑carbon steels widely used for coated flat products in automotive, appliance, and construction industries. The practical selection dilemma for engineers and procurement teams typically centers on balancing corrosion resistance and paintability against formability and cost, and on choosing the coating chemistry that best suits joining and finishing processes. Both notations identify the same DX51D substrate grade; the critical distinction lies in the type and metallurgical character of the zinc-based coating applied to the sheet.

This article compares the two options across standards, composition, microstructure and heat‑treatment response, mechanical properties, weldability, corrosion performance, fabrication behavior, typical applications, and procurement considerations to support informed selection decisions.

1. Standards and Designations

  • EN: DX51D is defined as a substrate grade in EN 10346 (continuously hot-dip coated steel flat products) and related EN standards for cold-rolled products used as bases for coating.
  • JIS/ASTM/ASME/GB: Equivalent low-carbon cold-rolled grades exist in other standards (for example, DC01/DC03 families in EN/ISO nomenclature or mild cold-rolled steels in JIS/ASTM), but DX51D calls out the specific EN coating designations.
  • Coating designators:
  • +Z denotes a metallic zinc coating (hot‑dip galvanized zinc layer).
  • +ZF denotes a zinc‑iron alloy coating (a zinc-iron intermetallic-rich surface layer produced via alloying/diffusion during the hot-dip process, commonly referred to as a zinc‑iron coating).
  • Classification: DX51D substrate is a low‑carbon, cold‑rolled carbon steel (not stainless, not HSLA, not tool steel).

2. Chemical Composition and Alloying Strategy

The DX51D substrate is a low‑carbon, low‑alloy cold‑rolled steel engineered for good formability and adequate strength after coating. Typical composition ranges are intentionally low in alloy content; exact values depend on producer and strip thickness. The following table summarizes representative typical ranges rather than strict limits — always verify supplier material certificates for exact numbers.

Element Typical (wt%) — DX51D substrate (representative)
C up to ~0.12 (typically 0.03–0.12)
Mn ~0.20–0.80
Si trace to ~0.30 (often 0.01–0.30)
P trace, ≤0.04 (typically ≤0.035)
S trace, ≤0.03–0.04
Cr not intentionally added (trace)
Ni not intentionally added (trace)
Mo not intentionally added (trace)
V not intentionally added (trace)
Nb not intentionally added (trace)
Ti not intentionally added (trace)
B not intentionally added (trace)
N low, controlled (ppm levels)

Notes: - DX51D is deliberately low in alloying elements; its mechanical performance comes primarily from cold reduction, strain hardening, and coating/annealing cycles rather than significant alloy additions. - Coating chemistry differs: the +Z product carries a primarily metallic zinc layer; the +ZF product carries a zinc‑iron alloy layer formed by diffusion/annealing after hot‑dip galvanizing. Coating microchemistry (Zn vs Zn–Fe intermetallics) is the central metallurgical difference and strongly influences surface hardness, adhesion, and post‑processing behavior.

How alloying affects properties: - Carbon and manganese control base steel strength and hardenability; keeping carbon low preserves formability and weldability. - Silicon and phosphorus affect surface deoxidation and yield behavior; controlled low levels help avoid embrittlement. - The absence of strong alloying reduces hardenability; these steels are readily weldable and formable but have limited potential for through‑thickness strength increases via heat treatment.

3. Microstructure and Heat Treatment Response

Microstructure (typical): - As‑cold‑rolled DX51D: ferritic matrix with dispersed elongated grains and work‑hardened dislocation structure. After continuous annealing (common for coated sheet), the microstructure is largely recrystallized ferrite with fine grain size tuned for ductility. - Coating influence: The hot‑dip process deposits a coating and, in the +ZF case, a subsequent alloying/annealing step promotes diffusion between zinc and iron to form Zn–Fe intermetallics (e.g., zeta, delta phases) at the coating/substrate interface.

Heat treatment/processing effects: - Recrystallization anneal: restores ductility in the substrate and affects coating adherence; standard continuous anneals used prior to coating produce a soft, ductile ferrite. - Normalizing/quenching & tempering: not typical for DX51D; the low alloy content limits hardenability, so conventional HT routes used for HSLA or quenched steels are not generally applied. - Thermo‑mechanical processing: modifications in cold reduction and anneal profiles can adjust yield/tensile combinations and r‑values (plastic strain ratios) important for forming performance, but the substrate remains a low‑alloy ferritic steel.

4. Mechanical Properties

Mechanical properties of coated DX51D depend on thickness, cold reduction, and final anneal. The coating itself contributes minimally to bulk mechanical values but does affect surface-related responses (e.g., coating cracking during forming). Typical property ranges are given as representative; check mill certificates for production lots.

Property Typical range (DX51D substrates, representative)
Tensile strength (Rp0.2–Rm interplay) ~270–410 MPa
Yield strength (Rp0.2) ~140–300 MPa
Elongation (A%) ~20–35%
Impact toughness (room temp) Not standardized; generally good for mild steel; dependent on thickness and microstructure
Hardness Low to moderate; typical HV values correlate with tensile range and cold work

Which is stronger/tougher/more ductile: - The base DX51D substrate determines the mechanical envelope; +Z and +ZF coatings do not materially change bulk tensile or yield values. - Ductility and formability are effectively the same for the substrate — differences in practical formability are driven by coating ductility and adhesion. Pure zinc coatings (+Z) are generally more ductile during severe forming operations than iron‑rich alloyed coatings (+ZF), which can be slightly harder and more prone to coating fragmentation on extreme deformation.

5. Weldability

Weldability depends primarily on the substrate carbon equivalent and on the coating behavior during welding.

Common weldability indices: - Carbon equivalent (IIW): $$CE_{IIW} = C + \frac{Mn}{6} + \frac{Cr+Mo+V}{5} + \frac{Ni+Cu}{15}$$ - Pcm (welding crack sensitivity): $$P_{cm} = C + \frac{Si}{30} + \frac{Mn+Cu}{20} + \frac{Cr+Mo+V}{10} + \frac{Ni}{40} + \frac{Nb}{50} + \frac{Ti}{30} + \frac{B}{1000}$$

Qualitative interpretation: - DX51D substrate has low carbon and low alloy content, producing low $CE_{IIW}$ and $P_{cm}$ values — hence the substrate itself is readily weldable by standard fusion and resistance methods. - Coating effects: - +Z (zinc) vaporizes and can cause zinc fumes, porosity, and undercut if not removed locally or if welding parameters are not adjusted; ventilation and fume controls are required. - +ZF (zinc‑iron alloy) coatings tend to be more iron‑rich and adhere more strongly; they produce less fuming and are easier to weld without pre‑strip, and they often reduce porosity compared with pure zinc coatings. - Resistance welding: Coating electrical resistance affects spot weldability. Zinc coatings can reduce electrode life and alter welding currents. Galvannealed or ZF coatings usually give more consistent spot welding behavior because of a more stable surface condition. - Pre‑weld preparation (stripping or using adapted parameters) mitigates coating-related welding issues.

6. Corrosion and Surface Protection

  • Neither DX51D+Z nor DX51D+ZF is stainless steel; corrosion protection depends on the coating type and thickness.
  • +Z (zinc): provides sacrificial galvanic protection — zinc corrodes preferentially, protecting exposed steel at scratches and cut edges. Pure zinc layers are generally more ductile and provide robust sacrificial protection.
  • +ZF (zinc‑iron alloy): the alloyed layer offers good barrier protection and improved paint adherence due to a more oxide‑active surface and rougher topography; it is usually better for over‑painting and baking durability.
  • PREN formula (stainless use-case): $$\text{PREN} = \text{Cr} + 3.3 \times \text{Mo} + 16 \times \text{N}$$
  • This index is not applicable to DX51D products because they are non‑stainless low‑carbon steels.
  • Practical implications:
  • For bare or cut‑edge corrosion resistance, +Z is often superior due to sacrificial behavior.
  • For painted/coated systems where long paint life and bakeability matter, +ZF often yields better paint adhesion and lower risk of flaking, improving system longevity.

7. Fabrication, Machinability, and Formability

  • Forming:
  • +Z coatings (metallic zinc) are typically more forgiving in deep drawing and severe forming because the coating is softer and more ductile; less risk of visible coating fractures.
  • +ZF coatings are harder and more brittle at the surface and can develop fine coating cracks during tight bends or stretch forming; however, these cracks are often tightly bonded and less visible after painting.
  • Cutting and shearing: coating type slightly affects burr formation and tool wear. +ZF coatings may increase tool abrasion compared to +Z.
  • Machinability: both behave like mild steel; coatings need to be considered for chip adhesion and tool fouling.
  • Finishing: +ZF offers better paint adhesion and compatibility with electrocoat and high‑temperature bake cycles; +Z may require specific pretreatments for optimal paint performance.
  • Handling and storage: both require standard precautions to avoid mechanical damage to the coating; +Z may show more visible scratches (but sacrificial protection retains corrosion performance), whereas +ZF damage can appear darker and more adherent.

8. Typical Applications

DX51D+Z (zinc) DX51D+ZF (zinc‑iron alloy)
Building cladding, roofing, gutters (good cut‑edge protection) Automotive outer panels where paint adhesion and bakeability are critical
General structural sheet for outdoor use, fencing Appliance bodies and components that undergo painting and baking
Agricultural equipment, exposed components where sacrificial protection desirable Automotive inner panels, parts requiring reliable spot welds and coating adhesion
HVAC ducts and conduit Pre‑painted coil where a consistent paint transfer and adhesion are required

Selection rationale: - Choose +Z when sacrificial corrosion protection and deep formability are prioritized and when cost sensitivity is important. - Choose +ZF when subsequent painting, bake cycles, and weld consistency are important; +ZF supports robust paint systems and often yields better resistance to paint flaking during forming.

9. Cost and Availability

  • Cost: In most markets, DX51D+Z is typically slightly less expensive than DX51D+ZF because the latter requires an additional alloying/annealing step to form the zinc‑iron layer. Exact price spreads depend on zinc market prices and processor capacities.
  • Availability: Both coatings are standard commercial products available from major coil coaters and steel mills in a wide range of thicknesses and coil weights. Lead times are generally short for common gauges; specialty coatings or required paint pretreatments can extend procurement time.

10. Summary and Recommendation

Criterion DX51D+Z DX51D+ZF
Weldability (practical, coating‑related) Moderate — caution for fume/porosity Better — less fume, more consistent spot welds
Strength–Toughness (substrate) Same (substrate controlled) Same (substrate controlled)
Formability (severe drawing) Better (more ductile coating) Slightly reduced (coating harder)
Paintability / Bakeability Good with pretreatment Superior (better adhesion, less flaking)
Cost Lower (generally) Slightly higher (processing add)

Concluding guidance: - Choose DX51D+Z if you need cost‑effective galvanized sheet with strong sacrificial corrosion protection and superior ductile coating behavior for deep drawing or exposed structural components. - Choose DX51D+ZF if your priority is paint adhesion, consistent welding (especially resistance welding), and long‑term painted performance — common demands in automotive outer/inner panels and pre‑painted coil applications.

Final note: Because the substrate (DX51D) chemistry and processing condition determine mechanical behavior, and because coating parameters vary by supplier, always request mill test certificates, coating weights/thicknesses, and perform representative forming/welding/paint trials with your chosen supplier before full production acceptance.

กลับไปยังบล็อก