20 Years Experience | 1000+ Brand Partners | Full Customization
We have 20 years of industry experience, have partnered with over 1,000 brands, and support any customization needs.
Technical Specifications
Product Overview
Metallurgical Characteristics
RHA Steel features a tempered martensitic microstructure achieved through controlled quenching and tempering processes. The optimized alloy composition with chromium, nickel, and molybdenum additions provides exceptional strength-to-weight ratio and superior impact resistance. The fine-grained microstructure ensures uniform mechanical properties and excellent through-thickness performance critical for structural applications.
Heat Treatment Process
MetalZenith employs precision austenitizing at 870-900°C followed by controlled quenching in oil or polymer solutions to achieve optimal hardness. Subsequent tempering at 200-250°C ensures the desired strength-toughness balance while maintaining dimensional stability and stress relief throughout the material cross-section.
Manufacturing Excellence
Our advanced manufacturing process includes vacuum degassing, controlled rolling, and precise heat treatment cycles with continuous monitoring of temperature profiles and cooling rates. MetalZenith's state-of-the-art facilities ensure consistent quality and traceability throughout production, meeting the most stringent structural engineering requirements.
Specialized Quality Testing
RHA Steel undergoes comprehensive testing including welding performance evaluation using standard procedures, forming capability assessment through bend tests, fatigue strength analysis under cyclic loading, and atmospheric corrosion resistance testing in various environmental conditions. Additional ballistic testing and impact resistance verification ensure superior performance in demanding applications.
Application Engineering Considerations
For building structures and bridge engineering, RHA Steel provides exceptional load-bearing capacity and seismic resistance. In mechanical manufacturing, its high strength enables weight reduction while maintaining structural integrity. Vehicle manufacturing benefits from superior crash resistance and durability. General engineering applications leverage its excellent machinability and welding characteristics for complex fabrications requiring high-performance materials.
🧪 Chemical Composition
Element | Composition (%) |
---|---|
Carbon (C) | 0.28 - 0.33 |
Manganese (Mn) | 0.70 - 1.00 |
Silicon (Si) | 0.20 - 0.35 |
Phosphorus (P) | ≤ 0.035 |
Sulfur (S) | ≤ 0.040 |
Chromium (Cr) | 0.70 - 1.20 |
Nickel (Ni) | 0.40 - 0.70 |
Molybdenum (Mo) | 0.15 - 0.25 |
⚙️ Mechanical Properties
Property | Value |
---|---|
Yield Strength (MPa) | ≥ 1275 |
Tensile Strength (MPa) | 1450 - 1750 |
Elongation (%) | ≥ 8 |
Impact Energy at 20°C (J) | ≥ 20 |
Hardness (HB) | 477 - 534 |
Fatigue Strength (MPa) | 580 - 650 |
🔬 Physical Properties
Property | Value |
---|---|
Density (g/cm3) | 7.85 |
Melting Point (°C) | 1480 - 1520 |
Thermal Conductivity (W/m·K) | 42.7 |
Thermal Expansion (×10??/K) | 11.9 |
Elastic Modulus (GPa) | 210 |
Poisson's Ratio | 0.27 - 0.30 |
📏 Product Specifications
Specification | Details |
---|---|
Available Forms | Plates, Sheets, Bars, Forgings, Custom Shapes |
Thickness Range | 12.7 - 152mm |
Width Range | 1200 - 3000mm |
Length Range | 6000 - 12000mm |
Standards Compliance | MIL-DTL-12560, ASTM A514, EN 10025-6 |
Heat Treatment Condition | Quenched and Tempered |
Surface Finish | Hot Rolled, Shot Blasted, Machined |
Let Us Create Success for Your Project
Professional Team, Premium Products, Complete Service - Your Project Success is Our Mission
Our Advantages in Processing RHA Steel

Advanced Heat Treatment Technology
MetalZenith utilizes precision-controlled quenching and tempering processes with real-time monitoring to achieve optimal hardness distribution and microstructural refinement. Our advanced heat treatment ensures consistent mechanical properties and enhanced structural performance throughout the material cross-section.
Comprehensive Performance Testing
Our RHA Steel undergoes extensive testing including welding performance evaluation, forming capability assessment, fatigue strength analysis, and atmospheric corrosion resistance testing. MetalZenith's quality assurance program ensures superior performance in structural applications with comprehensive ballistic and impact testing protocols.


Custom Engineering Solutions
MetalZenith provides tailored processing solutions including custom heat treatment cycles, precision machining, and specialized forming operations. Our technical team offers comprehensive support for structural design optimization and application-specific material modifications to meet unique project requirements.
YOUR TRUSTED STEEL
MANUFACTURING PARTNER
Quick Inquiry
Industries We Serve
Professional steel solutions across major industries