EN L290 Pipeline Steel - Premium Quality from MetalZenith

EN L290 is a high-strength pipeline steel grade designed for oil and gas transmission systems, equivalent to API 5L X42. This low-carbon, microalloyed steel offers excellent weldability, formability, and resistance to sour service conditions. MetalZenith manufactures EN L290 using advanced controlled rolling and accelerated cooling technologies to achieve optimal mechanical properties and microstructural uniformity.

MetalZenith's Manufacturing Excellence

Our state-of-the-art production facilities utilize thermomechanical controlled processing (TMCP) and precise chemical composition control to produce EN L290 with superior mechanical properties and dimensional accuracy. Our advanced vacuum degassing and ladle refining processes ensure minimal inclusion content and exceptional cleanliness levels.

Key Applications

  • Oil and gas pipeline systems
  • Pressure vessels and storage tanks
  • Structural applications in harsh environments
  • Offshore platform construction
  • Petrochemical plant equipment

Quality Assurance

MetalZenith maintains ISO 9001:2015, API 5L, and EN 10208 certifications. Every batch undergoes comprehensive testing including chemical analysis, mechanical testing, non-destructive examination, and dimensional verification. Our quality management system ensures full traceability from raw materials to final delivery.

Lihat detail lengkap

20 Years Experience | 1000+ Brand Partners | Full Customization

We have 20 years of industry experience, have partnered with over 1,000 brands, and support any customization needs.

Technical Specifications

Product Overview

Metallurgical Characteristics

EN L290 is a low-carbon, microalloyed steel with a ferritic-pearlitic microstructure. The controlled addition of niobium, vanadium, and titanium provides grain refinement and precipitation strengthening, resulting in excellent strength-toughness balance. The fine-grained microstructure ensures superior low-temperature impact properties and resistance to brittle fracture.

Manufacturing Process

MetalZenith produces EN L290 through controlled rolling in the austenite recrystallization region followed by accelerated cooling. This thermomechanical controlled processing (TMCP) refines the grain structure and optimizes mechanical properties. Our continuous casting process ensures homogeneous chemical composition and minimal segregation. Advanced ladle metallurgy techniques including vacuum degassing and calcium treatment provide exceptional cleanliness levels.

Heat Treatment

EN L290 is typically supplied in the as-rolled condition with normalized microstructure. Optional heat treatments include stress relieving at 580-620°C for improved dimensional stability and normalized heat treatment at 900-950°C followed by air cooling for enhanced mechanical properties. Post-weld heat treatment may be applied at 580-620°C to relieve residual stresses.

Quality Standards

All EN L290 products manufactured by MetalZenith comply with EN 10208-2, API 5L PSL1 and PSL2, and ISO 3183 standards. Our quality management system includes 100% ultrasonic testing, hydrostatic pressure testing, dimensional inspection, and comprehensive mechanical testing. Chemical composition verification is performed using optical emission spectroscopy with certified reference materials. Impact testing is conducted according to EN 10045-1 using Charpy V-notch specimens at specified temperatures.

🧪 Chemical Composition

ElementComposition (%)
Carbon (C)≤ 0.28
Manganese (Mn)≤ 1.40
Silicon (Si)≤ 0.40
Phosphorus (P)≤ 0.030
Sulfur (S)≤ 0.030
Chromium (Cr)≤ 0.30
Nickel (Ni)≤ 0.30
Molybdenum (Mo)≤ 0.15
Copper (Cu)≤ 0.50
Niobium (Nb)≤ 0.05
Vanadium (V)≤ 0.10
Titanium (Ti)≤ 0.04
Aluminum (Al)≥ 0.015
Carbon Equivalent (CE)≤ 0.43

⚙️ Mechanical Properties

PropertyValue
Yield Strength (Rp0.2)290-440 MPa
Tensile Strength (Rm)415-565 MPa
Elongation (A)≥ 22%
Yield to Tensile Ratio≤ 0.93
Hardness (HV10)150-250
Impact Energy (KV2) at 0°C≥ 27 J
Impact Energy (KV2) at -20°C≥ 40 J
Impact Energy (KV2) at -40°C≥ 27 J
Fatigue Limit (10^7 cycles)180-220 MPa
Modulus of Elasticity210 GPa
Poisson's Ratio0.27-0.30
Shear Modulus80 GPa

🔬 Physical Properties

PropertyValue
Density7.85 g/cm³
Melting Point1510°C
Thermal Conductivity (20°C)54 W/m·K
Thermal Expansion Coefficient (20-100°C)12×10-6/K
Specific Heat Capacity500 J/kg·K
Electrical Resistivity (20°C)0.16 µΩ·m
Magnetic PermeabilityFerromagnetic
Curie Temperature770°C
Thermal Diffusivity13.7 mm²/s
Coefficient of Linear Expansion (0-100°C)11.5×10-6/K
Emissivity (oxidized surface)0.79

📏 Product Specifications

SpecificationDetails
Available FormsSeamless Pipes, Welded Pipes, Plates, Sheets, Coils, Bars
Pipe Outer Diameter21.3-1422 mm
Wall Thickness2.0-80 mm
Plate Thickness6-100 mm
Plate Width1500-4000 mm
Length6-18 m (or as required)
StandardsEN 10208-2, API 5L, ISO 3183, ASTM A333
Surface FinishBlack, Pickled, Oiled, Galvanized, Coated
End PreparationPlain End, Beveled End, Threaded
Dimensional Tolerance±0.5% (thickness), ±1% (width/diameter)
TestingHydrostatic, NDT, Chemical Analysis, Mechanical Testing
CertificationMill Test Certificate, Third Party Inspection Available

Let Us Create Success for Your Project

Professional Team, Premium Products, Complete Service - Your Project Success is Our Mission

Our Advantages in Processing EN L290

Manufacturing Advantage 1

Advanced TMCP Technology

MetalZenith employs thermomechanical controlled processing with precise temperature control and accelerated cooling to achieve fine-grained microstructure, ensuring superior mechanical properties and excellent low-temperature toughness in EN L290 steel.

Comprehensive Quality Control

Our integrated quality management system includes real-time chemical composition monitoring, automated mechanical testing, ultrasonic inspection, and dimensional verification, ensuring every EN L290 product meets or exceeds international standards.

Manufacturing Advantage 2
Manufacturing Advantage 3

Custom Processing Capabilities

MetalZenith offers extensive customization options including specialized heat treatments, precision machining, surface treatments, and cut-to-length services, delivering EN L290 products tailored to specific project requirements with global logistics support.

YOUR TRUSTED STEEL

MANUFACTURING PARTNER

20
Years Experience
Leading Steel Manufacturing & Distribution
1000+
Brand Partners
Trusted by Global Industry Leaders
Full
Customization
Tailored Solutions for Every Project
50M+
Tons Delivered
High-Quality Steel Products Worldwide
95%
Client Retention
Long-term Partnership Success
ISO 9001
Certified Quality
International Standards Compliance
20
Years Experience
Leading Steel Manufacturing & Distribution
1000+
Brand Partners
Trusted by Global Industry Leaders
Full
Customization
Tailored Solutions for Every Project
50M+
Tons Delivered
High-Quality Steel Products Worldwide
95%
Client Retention
Long-term Partnership Success
ISO 9001
Certified Quality
International Standards Compliance
GET IN TOUCH

Quick Inquiry

Industries We Serve

Professional steel solutions across major industries

Construction

High-rise Buildings • Infrastructure • Commercial Real Estate

Oil & Gas

Pipeline Systems • Storage Equipment • Refinery Facilities

Manufacturing

Precision Machinery • Industrial Equipment • Automation Systems

Automotive

Body Structure • Chassis Components • Engine Parts

Shipbuilding

Hull Structure • Marine Engineering • Port Equipment

Energy & Power

Power Generation • Transmission Towers • Renewable Energy

Aerospace

Aircraft Materials • Precision Components • Special Alloys

Railway

Track Systems • Vehicle Manufacturing • Infrastructure

Qualifications & Certifications

Client logo
Client logo
Client logo
Client logo
Client logo