Q390 vs Q420 – Composition, Heat Treatment, Properties, and Applications
แบ่งปัน
Table Of Content
Table Of Content
Introduction
Q390 and Q420 are two commonly specified high‑strength structural steels used across construction, heavy machinery, and fabrication industries. Engineers and procurement teams frequently choose between them when balancing strength requirements, fabrication complexity, and lifecycle cost: for example, selecting a lower‑cost grade with easier weldability versus a higher‑strength grade that reduces section size and weight.
The principal technical distinction is that Q420 is specified for a higher minimum yield strength than Q390, and achieving that higher yield typically involves tighter composition control and stronger microalloying/hardenability strategies, which can affect weldability and forming behavior. These two grades are therefore compared when designers must trade off higher strength (and potential weight savings) against fabrication ease and toughness performance.
1. Standards and Designations
- Common standards referencing these grades include:
- Chinese standard GB/T 1591 — high‑strength low‑alloy structural steels (where the Q‑designation originates).
- Regional equivalents/analogs may be specified in project documentation, but Q390/Q420 are GB style yield‑based designations rather than ASTM names.
- Classification:
- Both Q390 and Q420 are HSLA (high‑strength low‑alloy) carbon steels designed primarily for structural applications (not stainless or tool steels).
- They are not stainless steels; they are carbon‑based structural steels with microalloying and controlled chemistry.
2. Chemical Composition and Alloying Strategy
- Both grades use a low‑carbon base with controlled alloying and may include microalloying elements (V, Nb, Ti, B) or small additions of Cr/Mo in some supplied variants. Exact limits vary by standard edition and producer; mill certificates should always be consulted.
| Element | Typical role and presence in Q390 / Q420 |
|---|---|
| C (Carbon) | Low carbon content to preserve weldability and toughness; both grades rely on controlled C rather than high C for strength. |
| Mn (Manganese) | Principal strengthening element and deoxidizer; present in modest amounts to increase hardenability and tensile properties. |
| Si (Silicon) | Deoxidation and strength contribution; kept moderate to avoid weldability issues. |
| P (Phosphorus) | Kept low as an impurity to avoid embrittlement and loss of toughness. |
| S (Sulfur) | Minimized; may be present as trace amounts — controlled for machinability but reduced for toughness. |
| Cr (Chromium) | Usually low or absent; small amounts may be used in specific variants to improve hardenability. |
| Ni (Nickel) | Not typical in standard Q grades; may appear only in special variants for toughness. |
| Mo (Molybdenum) | Occasionally added in small amounts in specially specified steels to improve hardenability. |
| V (Vanadium) | Common microalloying element for precipitation strengthening and grain refinement. |
| Nb (Niobium) | Used for grain refinement and strengthening via microalloying (common in TMCP products). |
| Ti (Titanium) | Present as a deoxidizer and to control N via TiN; contributes to fine grain sizes when used. |
| B (Boron) | Very small quantities, when used, greatly increase hardenability; tightly controlled. |
| N (Nitrogen) | Controlled; interacts with Ti/Nb to form stable nitrides which affect grain size and toughness. |
Explanation: The main alloying strategy for Q390 and Q420 is to maintain low carbon and utilize microalloying (V, Nb, Ti, and occasionally B) combined with thermo‑mechanical processing to obtain the required yield strength with favorable toughness and weldability. Q420 variants designed to meet the higher yield requirement may rely slightly more on microalloying or thermomechanical control, which can increase hardenability relative to Q390.
3. Microstructure and Heat Treatment Response
- Typical microstructures:
- As‑rolled or TMCP (thermo‑mechanical controlled processing) products: fine ferrite‑pearlite or ferrite with controlled bainitic fractions depending on cooling rates and microalloy additions.
- Q390 often achieves the required strength with a predominantly fine ferritic microstructure and dispersed precipitates from Nb/V/Ti.
- Q420 may include a higher fraction of low‑temperature transformation products (fine bainite or tempered martensite islands) in some processing routes to reach the higher yield.
- Heat treatment response:
- Normalizing: refines prior austenite grain size and can improve toughness; both grades respond to normalizing with improved uniformity, but gains depend on thickness and composition.
- Quenching & tempering: not typically used for standard commodity Q‑grades (cost and distortion concerns), but subcritical tempering/controlled cooling can produce higher strength and toughness if required.
- TMCP: the most common route — controlled rolling followed by accelerated cooling produces fine grain structures and dispersion strengthening; it is effective for both grades but Q420 heat‑treatment schedules are optimized to secure the higher yield without sacrificing impact toughness.
4. Mechanical Properties
Note: Mechanical properties depend on thickness, processing (TMCP, normalized), and testing temperature. The yield value in the grade name denotes the guaranteed minimum yield strength in MPa under specified test conditions.
| Property | Q390 (typical) | Q420 (typical) |
|---|---|---|
| Minimum Yield Strength (MPa) | 390 (specified) | 420 (specified) |
| Tensile Strength (MPa) | Moderate; margin above yield varies with processing (common ranges depend on mill spec and thickness) | Higher overall tensile range required to maintain ductility at higher yield |
| Elongation (%) | Generally good ductility for structural steels (depends on thickness) | Slightly reduced ductility relative to Q390 for equivalent processing, if higher strength achieved by microalloying/hardenability |
| Impact Toughness (J at given temperature) | Good when TMCP and low C are used; retains toughness at common service temperatures | Similar or slightly lower if higher hardenability increases susceptibility to brittle microstructures unless specifically processed for toughness |
| Hardness (HB, typical) | Lower than Q420 for similar processing | Higher due to higher yield; affects machinability and indentation resistance |
Interpretation: Q420 is deliberately stronger by specification, and when strength is achieved mainly through microalloying and controlled processing, toughness can remain acceptable. However, the higher strength target narrows the processing window: achieving Q420 can increase hardenability, which may reduce intrinsic weldability and ductility if not compensated by careful alloy design and heat treatment.
5. Weldability
- Weldability considerations center on carbon content, carbon equivalent, and the presence of microalloying or hardenability‑increasing elements.
- Useful indices:
- Carbon equivalent (IIW): $$CE_{IIW} = C + \frac{Mn}{6} + \frac{Cr+Mo+V}{5} + \frac{Ni+Cu}{15}$$
- Pcm (weldability parameter): $$P_{cm} = C + \frac{Si}{30} + \frac{Mn+Cu}{20} + \frac{Cr+Mo+V}{10} + \frac{Ni}{40} + \frac{Nb}{50} + \frac{Ti}{30} + \frac{B}{1000}$$
- Qualitative interpretation:
- Lower carbon and lower CE values indicate easier weldability with lower preheat and reduced risk of cold cracks.
- Q390, designed with slightly lower required strength, often has a lower CE compared with Q420 variants produced with additional microalloying or higher Mn, making Q390 generally easier to weld with less preheat.
- Q420 can be welded successfully, but may require more conservative preheat/interpass temperatures, hydrogen control, and post‑weld heat treatment (PWHT) on thick sections to avoid hard martensitic zones and hydrogen cold cracking.
- Practical recommendations:
- Use low‑hydrogen consumables and preheat as necessary based on thickness and calculated CE/Pcm.
- For critical applications, request mill weldability data and consider qualification weld procedures on representative thicknesses.
6. Corrosion and Surface Protection
- These are carbon HSLA steels — not corrosion resistant in the way stainless steels are.
- Typical protection methods: hot‑dip galvanizing, zinc electroplating (where appropriate), organic coatings (primers/topcoats), and specialized coatings for marine or aggressive industrial atmospheres.
- PREN (pitting resistance equivalent number) is not applicable to Q grades because they are not stainless steels: $$\text{PREN} = \text{Cr} + 3.3 \times \text{Mo} + 16 \times \text{N}$$
- This index applies only for stainless alloys containing significant Cr, Mo, and N; it should not be used for Q390/Q420.
- Selection point: if corrosion resistance is a project driver, specify protective systems or consider stainless/duplex alloys rather than relying on base‑steel chemistry.
7. Fabrication, Machinability, and Formability
- Machinability:
- Both grades are machinable with standard practices; higher strength (Q420) typically increases tool wear and may require adjusted feeds/speeds.
- Formability and bending:
- Lower yield steels (Q390) are generally easier to form and bend to tight radii without cracking; Q420 may require larger bend radii or controlled forming methods.
- Cutting and thermal processes:
- Thermal cutting (plasma/oxy‑fuel) is similar for both grades, but post‑cut edge conditions and heat‑affected zones should be considered for downstream fatigue or welds.
- Surface finishing:
- For paint or plating, surface cleanliness and pre‑treatment are the same; hard surfaces on Q420 may influence abrasive finishing.
8. Typical Applications
| Q390 — Common uses | Q420 — Common uses |
|---|---|
| General structural steelwork where moderate high strength and good weldability are needed (building frames, non‑critical bridges, platforms) | Heavier structural applications where weight saving is important (long‑span bridges, heavy cranes, large earthmoving equipment) |
| Structural components where fabrication speed and ease of welding are priorities | Components requiring greater section modulus for the same load (reducing plate thickness while maintaining capacity) |
| Secondary structural members, general fabrication | Primary load‑bearing members, high‑capacity structural members, and specialized welded structures |
Selection rationale: Choose Q390 when fabrication ease, lower cost, and good toughness are primary. Choose Q420 when higher strength per unit area and weight/space savings are required, and when the fabrication plan accommodates slightly more rigorous welding/forming controls.
9. Cost and Availability
- Relative cost:
- Q420 typically commands a modest premium over Q390 due to the higher guaranteed yield and possibly tighter composition/processing controls.
- Availability:
- Both grades are widely produced in plate and coil by major mills in regions where GB standards are common. Availability by product form (plate, coil, section) can vary by market and thickness.
- Procurement note:
- For large projects, specify required delivery standard, mechanical property acceptance criteria, and supply form early to secure best lead times and pricing.
10. Summary and Recommendation
| Criterion | Q390 | Q420 |
|---|---|---|
| Weldability | Better (generally lower CE) | Good but may require more preheat/controls |
| Strength–Toughness balance | Good, favorable toughness for many TMCP products | Higher strength; toughness achievable but requires tighter control |
| Cost | Lower | Higher (modest premium) |
Conclusion: - Choose Q390 if you prioritize easier fabrication and welding, good toughness with a slightly lower material cost, and when section sizing allows for the lower minimum yield. - Choose Q420 if you need higher design yield to reduce section size or weight and can accommodate more disciplined welding, forming, and thermal control during fabrication.
Practical final note: Always request the supplier’s mill certificate, heat‑treatment record, and weldability guidance for the supplied lot. For critical structures, require qualification welding on representative thickness and processing conditions, and consider specifying impact energy and toughness limits at the service temperature to ensure field performance.