Aluminum 5251: Composition, Properties, Temper Guide & Applications

Table Of Content

Table Of Content

Comprehensive Overview

5251 is a member of the 5xxx series aluminum alloys, which are magnesium-based, non-heat-treatable alloys offering a balance of strength and corrosion resistance. Its chemistry places it among the Al-Mg(-Mn) alloys where magnesium is the principal strengthening solute and manganese provides secondary grain-structure control.

Strength in 5251 is obtained primarily through solid-solution strengthening and strain hardening; the alloy cannot be significantly strengthened by precipitation heat treatment. Key traits include moderate-to-high strength for a non-heat-treatable alloy, good atmospheric and marine corrosion resistance, excellent formability in the annealed condition, and good weldability with typical aluminum fusion processes.

Typical industries using 5251 include automotive interior and exterior panels, marine structural components, architectural and building systems, and certain transport and general engineering applications. Engineers select 5251 when designers need a corrosion-resistant alloy with better strength than commercially pure aluminum and superior formability compared with many heat-treatable alloys.

5251 is chosen over other alloys when a combination of cold-forming capability, moderate strength, and durable surface performance is required while keeping fabrication costs low and avoiding age-hardening cycles. Its service profile often makes it preferable to alloys that sacrifice corrosion resistance for higher peak strength.

Temper Variants

Temper Strength Level Elongation Formability Weldability Notes
O Low High (18–30%) Excellent Excellent Fully annealed; best for deep drawing and complex forming
H12 Low–Medium Moderate (12–20%) Very good Very good Lightly cold-worked for slight strengthening
H14 Medium Moderate (10–18%) Good Very good Quarter hard; common for sheet applications
H22 Medium Moderate (10–18%) Good Very good Thermally stabilized after partial anneal
H24 Medium–High Lower (8–14%) Fair Good Strain-hardened and partially annealed
H32 High Low (6–12%) Limited Good Strain-hardened and stabilized; common structural temper
T temper (T5 / T6 / T651) N/A N/A N/A N/A 5251 is a non-heat-treatable alloy; T tempers are not applicable

Temper has a decisive effect on 5251’s mechanical envelope: O provides maximum ductility for forming while H-index tempers deliver progressively higher yield and tensile strengths at the expense of elongation. Weldability remains good across tempers because 5251 does not rely on age hardening, but heat-affected zones will locally soften strain-hardened conditions and can reduce local strength.

Chemical Composition

Element % Range Notes
Si ≤ 0.25 Impurity; low content to preserve corrosion resistance
Fe ≤ 0.40 Common impurity that can form intermetallics affecting ductility
Mn 0.20–0.80 Controls grain structure and recovery; reduces recrystallization
Mg 2.0–3.0 Primary strengthening element via solid solution; improves corrosion resistance
Cu ≤ 0.10–0.15 Kept low to avoid reduced corrosion resistance
Zn ≤ 0.20 Minor; small amounts tolerated without large property changes
Cr ≤ 0.25 May be present to control grain growth and improve recrystallization resistance
Ti ≤ 0.15 Grain refiner when intentionally added; usually residual
Others ≤ 0.05 each / ≤ 0.15 total Trace elements and residuals limited by standards

The composition of 5251 is engineered to exploit magnesium-driven solid-solution strengthening while minimizing elements that encourage intermetallic formation or localized corrosion. Mn and Cr act as microstructure stabilizers and help the alloy retain strength after warm working, while low Cu and controlled Fe and Si keep corrosion resistance high and maintain good ductility.

Mechanical Properties

5251 exhibits tensile behavior characteristic of the cold-worked 5xxx family: ductile and tough in the annealed condition with a pronounced increase in yield and tensile strength when strain-hardened. Yield strength increases significantly with H-tempers while tensile-to-yield ratios remain moderate, producing predictable plastic deformation characteristics useful for forming operations. Elongation drops as strength rises, so forming and final forming operations must be sequenced before or controlled during strain hardening.

Hardness correlates with temper; annealed alloys present low Brinell/Vickers hardness while H-tempers push hardness into ranges useful for structural applications. Fatigue performance is generally favorable for marine and atmospheric exposures thanks to a ductile fracture mode and resistance to localized corrosion; however fatigue limits fall as thickness increases and surface condition deteriorates. Thickness affects both yield and forming behavior: thinner gauges form more readily, whereas thicker sections retain more through-thickness strength and may be less susceptible to through-thickness cracking during bending.

Property O/Annealed Key Temper (H32) Notes
Tensile Strength 95–155 MPa 240–310 MPa Range depends on cold work and thickness; H32 provides typical structural strength
Yield Strength 30–80 MPa 170–220 MPa Substantial increase from O to H32 due to strain hardening
Elongation 18–30% 6–12% Elongation decreases as temper hardness increases
Hardness 20–45 HB 70–95 HB Brinell hardness approximations; varies with temper and processing

Physical Properties

Property Value Notes
Density 2.68 g/cm³ Typical for Al-Mg alloys; good strength-to-weight ratio
Melting Range ≈ 600–655 °C Solidus-to-liquidus range typical of wrought aluminum alloys
Thermal Conductivity ≈ 120–150 W/m·K Lower than pure Al but still high; useful for thermal management
Electrical Conductivity ≈ 28–38 % IACS Reduced from pure Al due to alloying; adequate for some conductive applications
Specific Heat ≈ 0.90 J/g·K (900 J/kg·K) Standard for aluminum alloys; useful for thermal mass calculations
Thermal Expansion ≈ 23–24 µm/m·K Comparable to other Al alloys; important in multi-material assemblies

5251 retains favorable thermal and electrical transport properties compared with many structural alloys, which makes it useful in applications where both formability and heat conduction are needed. The density and thermal expansion characteristics support lightweight, thermally-stable designs, but designers should account for modest reductions in conductivity relative to pure aluminum when precise thermal or electrical performance is required.

Product Forms

Form Typical Thickness/Size Strength Behavior Common Tempers Notes
Sheet 0.3–4.0 mm Consistent with temper; thin gauges easier to form O, H14, H24, H32 Most common form for automotive and architectural panels
Plate 4–25 mm Higher through-thickness strength; less formable H22, H24, H32 Used for structural components requiring stiffness
Extrusion Variable cross-sections Strength depends on post-extrusion cold work O, H14 Extruded profiles often further worked to increase strength
Tube 0.5–6.0 mm wall Strength and fatigue depend on work and wall thickness O, H14, H32 Used in lightweight structural systems and marine tubing
Bar/Rod 6–100 mm Bulk sections retain good machinability O, H12, H14 Used for machined components, fittings, and fasteners

Differences in product form control available tempers and final mechanical properties; thinner sheets are produced and processed for maximum formability whereas plate and thick extrusions are offers for load-bearing components. Processing routes such as cold rolling, annealing, and stabilization are used to tailor ductility or strength prior to fabrication and final finishing.

Equivalent Grades

Standard Grade Region Notes
AA 5251 USA Standard American Alloy designation for wrought 5251
EN AW 5251 Europe EN version aligns closely with AA composition and tempers
JIS A5251 (approx.) Japan Japanese standards reference comparable Al-Mg grades; check local spec
GB/T 5251 (approx.) China Chinese designation uses similar numbering; verify local tolerances

Equivalency tables are approximate because regional specifications can differ in allowable impurity limits, process qualifications, and temper definitions. When substituting alloys across standards, engineers should verify chemistry, mechanical properties, and certification requirements rather than rely solely on numeric correspondence.

Corrosion Resistance

5251 offers good atmospheric corrosion resistance typical of Al-Mg alloys; a natural aluminum oxide film combined with the presence of magnesium gives enhanced performance in outdoor and mildly aggressive environments. It performs well for general marine and coastal exposure scenarios, although localized pitting resistance depends on surface finish and Mg content compared to higher-Mg alloys.

Stress corrosion cracking susceptibility in 5251 is low relative to some higher-strength Al-Mg alloys; because it is not age-hardened, it avoids precipitate-assisted SCC mechanisms that plague certain heat-treatable alloys. Contact with more noble metals or cathodic materials can introduce galvanic couples; designers should avoid direct coupling with stainless steels or copper without insulating barriers when continuous wetting is expected.

Compared with 6xxx series alloys, 5251 provides improved general corrosion resistance but lower maximum strength. Versus 3xxx and 1xxx alloys, 5251 trades slightly reduced formability and electrical conductivity for higher structural capability and better corrosion behavior in chloride environments.

Fabrication Properties

Weldability

5251 welds readily with MIG (GMAW) and TIG (GTAW) processes using aluminum filler wires in the 4xxx and 5xxx series alloys. Recommended fillers include ER4043 (silicon) for reduced cracking risk and ER5356 or ER5183 (Al-Mg fillers) when matching strength and corrosion resistance is important; minimize porosity through good joint fit-up and cleaning. Hot-cracking risk is low compared with heat-treatable alloys, but the HAZ in strain-hardened tempers will soften and reduce local strength.

Machinability

Machinability of 5251 is fair to moderate and generally better than higher-strength 5xxx alloys due to its balance of ductility and strength; it is not a free-machining aluminum. Carbide tooling with positive rake and high-feed, lower-speed strategies yield the best surface finishes and tool life. Chip control is typically achievable with sharp tools and proper coolant; avoid excessive work hardening of the immediate cut zone.

Formability

Formability in the O temper is excellent for deep drawing, bending and complex stamping operations, with relatively low springback compared with stronger alloy tempers. Recommended bend radii depend on thickness and temper but generally follow common aluminum rules of thumb (e.g., internal radius ≥ 1–2× thickness for H-tempers and ≥ 0.5–1× thickness for O temper). Cold working is the primary strengthening pathway, so sequential forming and controlled recovery anneals are normal practice to reach complex geometries without cracking.

Heat Treatment Behavior

5251 is classified as a non-heat-treatable alloy; it cannot achieve significant precipitation hardening through solution and aging treatments. Attempts to apply T-type heat treatment will not produce the strength gains seen in 6xxx and 7xxx alloys and can lead to undesirable microstructural effects.

Work hardening through cold deformation is the principal mechanism to raise yield and tensile strengths. Standard annealing (e.g., full anneal to O) will restore ductility by recovery and recrystallization, and stabilization treatments (designated H3x/H4x) are used to minimize subsequent changes in mechanical properties during fabrication or service.

High-Temperature Performance

Elevated temperatures reduce the strength of 5251 progressively, with appreciable softening often occurring above 100–150 °C depending on temper and stress level. Continuous exposure to temperatures approaching the alloy melting range is not appropriate; for intermittent elevated-temperature use, designers must allow for reduced load-carrying capacity and accelerated creep mechanisms.

Oxidation at service temperatures is limited to the formation of a stable aluminum oxide film which is protective; there is no significant scale or embrittlement as seen in some steels. The thermal stability of cold-worked tempers is moderate, so prolonged exposure to moderately elevated temperatures can relax residual stresses and lower yield strength in H-tempers, particularly near welds and high-strain regions.

Applications

Industry Example Component Why 5251 Is Used
Automotive Interior and exterior body panels Good formability and moderate strength; corrosion resistance
Marine Structural panels and non-critical fittings Saltwater resistance and good fatigue performance
Aerospace Secondary fittings and fairings Favorable strength-to-weight and corrosion resistance for non-critical parts
Electronics Chassis and heat spreaders Thermal conductivity and corrosion stability
Architecture Curtain wall panels and cladding Formability for complex shapes and long-term outdoor durability

5251 occupies a practical niche where formability, corrosion resistance, and reasonable structural strength are required simultaneously and where heat treatment would add cost or complexity. It is widely used in sheet and extruded forms that undergo significant forming operations before final deployment.

Selection Insights

5251 is a logical choice when an engineer needs more strength than commercially pure aluminum (e.g., 1100) but still requires good formability and corrosion resistance. Compared with 1100, 5251 trades higher strength and slightly reduced electrical/thermal conductivity for structural capacity and better corrosion performance in chlorinated environments.

Compared with other work-hardened alloys such as 3003 and 5052, 5251 generally sits closer to 5052 in strength and corrosion resistance, offering comparable marine performance but often better formability than highly strain-hardened variants. When designers need stronger, heat-treatable alloys like 6061, 5251 is selected if corrosion resistance, weldability, or formability in the O temper is prioritized over maximum achievable strength.

Choose 5251 when fabrication sequences involve significant cold forming or welding and when long-term atmospheric or marine exposure is anticipated; balance cost and availability against slightly lower peak strengths than heat-treatable alternatives.

Closing Summary

5251 remains a relevant and practical Al-Mg alloy for modern engineering because it combines formability, weldability, and corrosion resistance with a workable strength range obtained through cold work. Its predictable behavior across tempers, wide product form availability, and service-proven performance in automotive, marine, and architectural applications make it a dependable choice where a durable, formable aluminum is required.