St 60 Steel is a German structural steel grade classified as a low-carbon mild steel. It is primarily composed of iron (Fe) with a carbon content typically ranging from 0.06% to 0.12%. This low carbon content contributes to its excellent weldability and formability, making it suitable for various structural applications. The primary alloying elements in St 60 include manganese (Mn), which enhances hardenability and strength, and silicon (Si), which improves deoxidation during steelmaking.
Comprehensive Overview
St 60 steel is known for its good mechanical properties, including moderate tensile strength and ductility. It is often used in construction and engineering applications where high strength is not the primary requirement but where good weldability and formability are essential. The steel's yield strength typically ranges from 235 to 360 MPa, with elongation values around 20% to 25%, indicating its ability to deform without breaking.
Advantages:
- Weldability: St 60 can be easily welded using various methods, making it ideal for construction and fabrication.
- Formability: Its low carbon content allows for excellent formability, enabling complex shapes to be manufactured.
- Cost-Effectiveness: Generally, low-carbon steels like St 60 are more affordable compared to higher alloyed steels.
Limitations:
- Lower Strength: Compared to higher carbon or alloy steels, St 60 has lower tensile and yield strength, which may limit its use in high-stress applications.
- Corrosion Resistance: It may require protective coatings in corrosive environments, as it does not possess inherent corrosion resistance.
Historically, St 60 has been widely used in Europe, particularly in Germany, for structural applications such as beams, columns, and frames in buildings and bridges. Its commonality in the market is attributed to its balance of properties and cost, making it a go-to choice for many engineers and fabricators.
Alternative Names, Standards, and Equivalents
Standard Organization | Designation/Grade | Country/Region of Origin | Notes/Remarks |
---|---|---|---|
DIN | St 60 | Germany | Closest equivalent to S235JR |
EN | S235JR | Europe | Minor compositional differences |
ASTM | A36 | USA | Similar mechanical properties but different chemical composition |
JIS | SS400 | Japan | Comparable strength but lower ductility |
ISO | 10025 S235 | International | General structural steel grade |
The table above highlights several standards and equivalent grades to St 60. While these grades may be similar in mechanical properties, subtle differences in chemical composition can affect performance in specific applications. For instance, A36 steel has a higher carbon content, which may enhance strength but reduce weldability compared to St 60.
Key Properties
Chemical Composition
Element (Symbol and Name) | Percentage Range (%) |
---|---|
C (Carbon) | 0.06 - 0.12 |
Mn (Manganese) | 0.30 - 0.60 |
Si (Silicon) | 0.10 - 0.40 |
P (Phosphorus) | ≤ 0.045 |
S (Sulfur) | ≤ 0.045 |
Fe (Iron) | Balance |
The primary alloying elements in St 60 play crucial roles in determining its properties. Carbon, while present in low amounts, is essential for achieving the desired strength and hardness. Manganese enhances the steel's hardenability and toughness, while silicon aids in deoxidation during the steelmaking process, improving overall quality.
Mechanical Properties
Property | Condition/Temper | Typical Value/Range (Metric) | Typical Value/Range (Imperial) | Reference Standard for Test Method |
---|---|---|---|---|
Tensile Strength | Annealed | 235 - 360 MPa | 34 - 52 ksi | ASTM E8 |
Yield Strength (0.2% offset) | Annealed | ≥ 235 MPa | ≥ 34 ksi | ASTM E8 |
Elongation | Annealed | 20 - 25% | 20 - 25% | ASTM E8 |
Reduction of Area | Annealed | ≥ 50% | ≥ 50% | ASTM E8 |
Hardness (Brinell) | Annealed | 120 - 160 HB | 120 - 160 HB | ASTM E10 |
Impact Strength | Charpy V-notch, -20°C | ≥ 27 J | ≥ 20 ft-lbf | ASTM E23 |
The mechanical properties of St 60 make it suitable for various structural applications. Its moderate tensile and yield strengths allow it to withstand typical loads in construction, while its elongation and reduction of area indicate good ductility, essential for applications requiring deformation without fracture.
Physical Properties
Property | Condition/Temperature | Value (Metric) | Value (Imperial) |
---|---|---|---|
Density | Room Temperature | 7850 kg/m³ | 490 lb/ft³ |
Melting Point | - | 1425 - 1540 °C | 2600 - 2800 °F |
Thermal Conductivity | Room Temperature | 50 W/m·K | 34.5 BTU·in/h·ft²·°F |
Specific Heat Capacity | Room Temperature | 460 J/kg·K | 0.11 BTU/lb·°F |
Electrical Resistivity | Room Temperature | 0.0000017 Ω·m | 0.0000017 Ω·ft |
The density of St 60 indicates that it is a relatively heavy material, which is typical for structural steels. Its melting point suggests good thermal stability, while thermal conductivity and specific heat capacity values are important for applications involving heat transfer.
Corrosion Resistance
Corrosive Agent | Concentration (%) | Temperature (°C) | Resistance Rating | Notes |
---|---|---|---|---|
Atmospheric | Varies | Ambient | Fair | Susceptible to rust |
Chlorides | Varies | Ambient | Poor | Risk of pitting corrosion |
Acids | Varies | Ambient | Poor | Not recommended |
Alkaline | Varies | Ambient | Fair | Moderate resistance |
St 60 exhibits moderate corrosion resistance in various environments. It is susceptible to rusting in atmospheric conditions, particularly in the presence of moisture. Chlorides pose a significant risk, leading to pitting corrosion, while exposure to acids should be avoided entirely. Compared to stainless steels or higher alloyed grades, St 60 requires protective coatings or treatments in corrosive environments.
When compared to grades like S235JR or A36, St 60's corrosion resistance is generally lower, necessitating additional protective measures in applications exposed to harsh conditions.
Heat Resistance
Property/Limit | Temperature (°C) | Temperature (°F) | Remarks |
---|---|---|---|
Max Continuous Service Temp | 400 °C | 752 °F | Suitable for structural use |
Max Intermittent Service Temp | 500 °C | 932 °F | Short-term exposure only |
Scaling Temperature | 600 °C | 1112 °F | Risk of oxidation beyond this temp |
Creep Strength considerations | 300 °C | 572 °F | Begins to degrade at this temp |
St 60 maintains its mechanical properties up to moderate temperatures, making it suitable for structural applications where heat exposure is limited. However, at temperatures exceeding 400 °C, the risk of oxidation and loss of strength increases, necessitating careful consideration in design.
Fabrication Properties
Weldability
Welding Process | Recommended Filler Metal (AWS Classification) | Typical Shielding Gas/Flux | Notes |
---|---|---|---|
MIG | ER70S-6 | Argon + CO2 | Good for thin sections |
TIG | ER70S-2 | Argon | Clean welds, low distortion |
SMAW | E7018 | None | Suitable for outdoor use |
St 60 is highly weldable, making it a preferred choice for structural applications. The recommended filler metals ensure compatibility and strength in weld joints. Preheating may be necessary for thicker sections to avoid cracking.
Machinability
Machining Parameter | St 60 | AISI 1212 | Notes/Tips |
---|---|---|---|
Relative Machinability Index | 70% | 100% | Good for general machining |
Typical Cutting Speed | 30 m/min | 45 m/min | Adjust based on tooling |
St 60 offers reasonable machinability, though it is not as easily machined as free-machining steels like AISI 1212. Proper tooling and cutting speeds can enhance performance during machining operations.
Formability
St 60 exhibits excellent formability due to its low carbon content. It can be cold-formed into various shapes, including bends and complex geometries. The steel's work hardening characteristics allow it to maintain strength while being deformed, making it suitable for applications requiring intricate designs.
Heat Treatment
Treatment Process | Temperature Range (°C/°F) | Typical Soaking Time | Cooling Method | Primary Purpose / Expected Result |
---|---|---|---|---|
Annealing | 600 - 700 °C / 1112 - 1292 °F | 1 - 2 hours | Air | Improve ductility and reduce hardness |
Normalizing | 850 - 900 °C / 1562 - 1652 °F | 1 - 2 hours | Air | Refine grain structure |
Quenching | 800 - 850 °C / 1472 - 1562 °F | 30 minutes | Water/Oil | Increase hardness |
Heat treatment processes such as annealing and normalizing can significantly alter the microstructure of St 60, enhancing its mechanical properties. Annealing improves ductility, while normalizing refines the grain structure, resulting in improved toughness.
Typical Applications and End Uses
Industry/Sector | Specific Application Example | Key Steel Properties Utilized in this Application | Reason for Selection (Brief) |
---|---|---|---|
Construction | Structural beams | Good weldability, moderate strength | Cost-effective and easy to fabricate |
Automotive | Chassis components | Ductility, formability | Lightweight and strong |
Machinery | Frames and supports | Strength, toughness | Reliable under load |
St 60 is commonly used in construction for structural beams and frames due to its excellent weldability and formability. In the automotive industry, it is utilized for chassis components where weight reduction and strength are critical. Its versatility makes it suitable for various machinery applications as well.
Other applications include:
- Bridges: Used in the construction of bridge components due to its structural integrity.
- Industrial Equipment: Employed in manufacturing equipment where moderate strength is required.
Important Considerations, Selection Criteria, and Further Insights
Feature/Property | St 60 | S235JR | A36 | Brief Pro/Con or Trade-off Note |
---|---|---|---|---|
Key Mechanical Property | Moderate Strength | Moderate Strength | Higher Strength | St 60 is more weldable |
Key Corrosion Aspect | Fair | Fair | Poor | All require protection in corrosive environments |
Weldability | Excellent | Excellent | Good | St 60 is easier to weld |
Machinability | Good | Fair | Excellent | A36 is easier to machine |
Formability | Excellent | Good | Fair | St 60 allows for complex shapes |
Approx. Relative Cost | Moderate | Moderate | Low | Cost-effective for structural use |
Typical Availability | Common | Common | Very Common | A36 is widely available |
When selecting St 60, considerations include its mechanical properties, weldability, and cost-effectiveness. While it may not offer the highest strength compared to alternatives like A36, its excellent formability and weldability make it a preferred choice for many structural applications. Additionally, its availability in the market ensures that it can be sourced easily for projects.