DP 780

DP 780

Advanced Dual Phase Steel DP 780

DP 780 is a high-strength dual phase steel featuring an innovative microstructure combining ferrite and martensite phases, delivering exceptional strength-to-weight ratio and superior formability. This advanced high-strength steel (AHSS) represents the cutting edge of automotive steel technology, offering tensile strengths of 780 MPa while maintaining excellent ductility for complex forming operations.

MetalZenith's Manufacturing Excellence

MetalZenith leverages state-of-the-art continuous annealing technology and precise thermal processing to achieve the optimal dual phase microstructure in DP 780. Our advanced intercritical annealing process ensures consistent mechanical properties and superior surface quality. With ISO/TS 16949 certification and comprehensive in-house testing capabilities, we guarantee material performance that exceeds automotive industry standards.

Key Applications & Advantages

  • Automotive structural components including B-pillars, door frames, and reinforcement parts
  • Crash-resistant safety components requiring high energy absorption
  • Weight reduction applications in transportation industry
  • Complex formed parts requiring excellent stretch-flangeability

Quality Assurance & Global Supply

MetalZenith's comprehensive quality management system includes real-time process monitoring, advanced metallurgical testing, and full traceability. Our global distribution network ensures reliable supply of DP 780 in various forms including cold-rolled sheets, hot-dip galvanized, and electrogalvanized coatings, with technical support available worldwide.

詳細を表示する

20 Years Experience | 1000+ Brand Partners | Full Customization

We have 20 years of industry experience, have partnered with over 1,000 brands, and support any customization needs.

Technical Specifications

Product Overview

Metallurgical Structure & Processing

DP 780 features a carefully engineered dual phase microstructure consisting of approximately 70-80% ferrite matrix with 20-30% martensite islands. This unique microstructure is achieved through MetalZenith's advanced intercritical annealing process, where the steel is heated to 750-820°C in the two-phase (ferrite + austenite) region, followed by controlled cooling to transform austenite to martensite while retaining the soft ferrite phase.

Manufacturing Process Excellence

MetalZenith employs state-of-the-art continuous annealing technology with precise atmosphere control (N2-H2 mixture) to prevent oxidation and ensure optimal surface quality. The thermal cycle includes rapid heating at 10-15°C/s, precise temperature control within ±5°C during soaking, and controlled cooling rates of 20-50°C/s to achieve the desired martensite fraction. Post-annealing skin-pass rolling (0.5-1.5% reduction) provides excellent surface finish and shape control.

Quality Standards & Testing

All DP 780 production follows ISO/TS 16949 automotive quality management standards with comprehensive testing protocols. Mechanical properties are verified through tensile testing per ASTM E8, hole expansion testing per ISO 16630, and bend testing per VDA 238-100. Microstructural analysis using optical microscopy and EBSD confirms proper phase distribution and grain size. Surface quality inspection includes visual examination, roughness measurement, and coating weight verification for galvanized products.

Application Engineering Support

MetalZenith provides comprehensive technical support including forming simulation using AutoForm and LS-DYNA software, springback prediction, and tooling design recommendations. Our application engineers work closely with customers to optimize part design, forming parameters, and welding procedures. Specialized testing services include formability assessment, crash simulation, and fatigue analysis to ensure optimal performance in automotive applications.

🧪 Chemical Composition

ElementComposition (%)
Carbon (C)0.05 - 0.12
Manganese (Mn)1.20 - 2.50
Silicon (Si)0.10 - 0.80
Phosphorus (P)≤ 0.025
Sulfur (S)≤ 0.015
Chromium (Cr)0.10 - 0.50
Molybdenum (Mo)0.05 - 0.25
Aluminum (Al)0.015 - 0.070
Niobium (Nb)0.015 - 0.060
Titanium (Ti)0.010 - 0.050
Vanadium (V)0.01 - 0.10
Boron (B)0.0005 - 0.0050

⚙️ Mechanical Properties

PropertyValue
Tensile Strength (Rm)780 - 950 MPa
Yield Strength (Rp0.2)420 - 580 MPa
Elongation (A80)≥ 12%
Total Elongation (A50)≥ 14%
Uniform Elongation≥ 7%
Hardness (HV10)240 - 300
Young's Modulus210 GPa
Poisson's Ratio0.30
Hole Expansion Ratio≥ 30%
Bending Angle (90°)1.0t - 2.0t
Fatigue Limit (107 cycles)280 - 350 MPa
Impact Energy (Charpy V, 20°C)≥ 80 J

🔬 Physical Properties

PropertyValue
Density7.85 g/cm³
Melting Point1510°C
Thermal Conductivity (20°C)50 W/m·K
Thermal Expansion Coefficient (20-100°C)12×10-6/K
Specific Heat Capacity460 J/kg·K
Electrical Resistivity (20°C)0.18 µΩ·m
Magnetic PermeabilityFerromagnetic
Curie Temperature770°C
Thermal Diffusivity (20°C)13.8 mm²/s
Emissivity (oxidized surface)0.85

📏 Product Specifications

SpecificationDetails
Available FormsCold-rolled sheet, Hot-dip galvanized, Electrogalvanized, Galvannealed
Thickness Range0.6 - 3.0 mm
Width Range600 - 2100 mm
Coil Weight5 - 35 tons
StandardsEN 10338, ASTM A1088, JIS G3135, VDA 239-100
Surface FinishBright annealed, Matte finish, Skin-passed
Thickness Tolerance± 0.02 - 0.05 mm
Width Tolerance+0/-3 mm
Flatness≤ 10 I-units
Edge ConditionMill edge, Trimmed edge
Coating Weight (galvanized)60 - 275 g/m²
Surface QualityAutomotive grade A, B surface

Let Us Create Success for Your Project

Professional Team, Premium Products, Complete Service - Your Project Success is Our Mission

Our Advantages in Processing DP 780

Manufacturing Advantage 1

Advanced Dual Phase Microstructure Control

MetalZenith's proprietary intercritical annealing technology precisely controls the ferrite-martensite microstructure, achieving optimal balance of strength and formability. Our continuous annealing lines feature advanced atmosphere control and rapid cooling systems for consistent dual phase formation.

Comprehensive Automotive Quality Systems

ISO/TS 16949 certified production with real-time process monitoring, advanced metallurgical testing including EBSD analysis, and full statistical process control. Every coil undergoes mechanical testing, surface inspection, and dimensional verification to automotive industry standards.

Manufacturing Advantage 2
Manufacturing Advantage 3

Global Supply Chain & Technical Support

Worldwide distribution network with local technical support teams providing forming simulation, tooling recommendations, and application engineering. Flexible production capabilities for custom chemistries, surface treatments, and delivery schedules to meet specific automotive program requirements.

YOUR TRUSTED STEEL

MANUFACTURING PARTNER

20
Years Experience
Leading Steel Manufacturing & Distribution
1000+
Brand Partners
Trusted by Global Industry Leaders
Full
Customization
Tailored Solutions for Every Project
50M+
Tons Delivered
High-Quality Steel Products Worldwide
95%
Client Retention
Long-term Partnership Success
ISO 9001
Certified Quality
International Standards Compliance
20
Years Experience
Leading Steel Manufacturing & Distribution
1000+
Brand Partners
Trusted by Global Industry Leaders
Full
Customization
Tailored Solutions for Every Project
50M+
Tons Delivered
High-Quality Steel Products Worldwide
95%
Client Retention
Long-term Partnership Success
ISO 9001
Certified Quality
International Standards Compliance
GET IN TOUCH

Quick Inquiry

Industries We Serve

Professional steel solutions across major industries

Construction

High-rise Buildings • Infrastructure • Commercial Real Estate

Oil & Gas

Pipeline Systems • Storage Equipment • Refinery Facilities

Manufacturing

Precision Machinery • Industrial Equipment • Automation Systems

Automotive

Body Structure • Chassis Components • Engine Parts

Shipbuilding

Hull Structure • Marine Engineering • Port Equipment

Energy & Power

Power Generation • Transmission Towers • Renewable Energy

Aerospace

Aircraft Materials • Precision Components • Special Alloys

Railway

Track Systems • Vehicle Manufacturing • Infrastructure

Qualifications & Certifications

Client logo
Client logo
Client logo
Client logo
Client logo