Alloy | ASTM | Characteristics |
---|---|---|
A615 | ASTM A615 |
Reinforcing concrete in construction projects such as foundations, beams, and columns. Providing tensile strength to infrastructure developments like bridges and highways. Used in the construction of high-rise buildings for improved structural stability. |
CHEMICAL COMPOSITION
- The chemical composition of this category includes phosphorus with a maximum percentage of 0.06%, while the percentages of carbon, silicon, manganese, and sulfur are not specified. The material offers mechanical information for two standards, A615 SCH40 and A615 SCH60. The A615 SCH40 standard exhibits an ultimate tensile strength of 60,000 psi (414 MPa) and a yield tensile strength of 40,000 psi (276 MPa). In contrast, the A615 SCH60 standard demonstrates a higher ultimate tensile strength of 90,000 psi (620 MPa) and a yield tensile strength of 60,000 psi (414 MPa). The available sizes range from 3/8"-Grade40 to 1"-Grade60, with varying weights from 0.375 lbs/ft to 2.670 lbs/ft, all at a standard length of 240.00 inches.
MECHANICAL INFORMATION
- The A615 SCH40 and SCH60 products boast robust mechanical properties, with the SCH40 variant offering an ultimate tensile strength of 60,000 psi (414 MPa) and a yield tensile strength of 40,000 psi (276 MPa), while the SCH60 variant provides a higher ultimate tensile strength of 90,000 psi (620 MPa) and yield tensile strength of 60,000 psi (414 MPa). The chemical composition indicates a maximum of 0.06% phosphorus, with other elements not specified. For specific material test reports, please contact our Customer Service Department. These products are available in various sizes, including 3/8" to 1" in 240" lengths, with corresponding weights ranging from 0.375 lbs/ft to 2.670 lbs/ft.
AVAILABLE SIZES
- The available sizes for this category include 3/8"-Grade40 with a length of 240.00" and a weight of 0.375 lbs/ft, 1/2"-Grade40 with a length of 240.00" and a weight of 0.667 lbs/ft, 5/8"-Grade40 with a length of 240.00" and a weight of 1.043 lbs/ft, 5/8"-Grade60 with the same length and weight as 5/8"-Grade40 at 240.00" and 1.043 lbs/ft, 3/4"-Grade60 with a length of 240.00" and a weight of 1.502 lbs/ft, 7/8"-Grade60 with a length of 240.00" and a weight of 2.043 lbs/ft, and 1"-Grade60 with a length of 240.00" and a weight of 2.670 lbs/ft.