Dapatkan Penawaran
Alloy | ASTM | Characteristics |
---|---|---|
A1011 | ASTM A1011 |
Construction industry for building structural components. Manufacturing sector for producing machinery and equipment. Automotive industry for forming vehicle parts and panels. |
CHEMICAL COMPOSITION
- The chemical composition of the material is as follows: Carbon (C) content is a maximum of 0.15%, Manganese (Mn) content is a maximum of 0.6%, Phosphorus (P) content is a maximum of 0.03%, and Sulfur (S) content is a maximum of 0.035%.
MECHANICAL INFORMATION
- The material features a maximum carbon content of 0.15%, manganese at 0.6% max, phosphorus at 0.03% max, and sulfur at 0.035% max. It has a density of 0.284 lb/in³ or 7.87 g/cc. The ultimate tensile strength is measured at 58,000 psi (400 MPa) and the yield tensile strength is 36,300 psi (250 MPa). This material displays a Brinell hardness of 75. The available sizes for this material include thicknesses of 1/4", 5/16", 3/8", and 1/2" with corresponding widths and lengths ranging from 48.00" to 60.00" and 96.00" to 120.00", respectively. Weight per foot varies with thickness, with values such as 10.210 lbs/ft for 1/4" thickness and 20.421 lbs/ft for 1/2" thickness. These mechanical properties are general approximations; for precise material test reports, please contact our Customer Service Department.
AVAILABLE SIZES
- Available sizes for this category include a variety of thicknesses, widths, and lengths, each with specific weights per foot. The thickness options are 1/4", 5/16", 3/8", and 1/2". For a thickness of 1/4", the available sizes are 48.00" x 120.00" and 48.00" x 96.00", both weighing 10.210 lbs/ft, and also 60.00" x 120.00" with the same weight. For a thickness of 5/16", the size available is 60.00" x 120.00", weighing 12.760 lbs/ft. For 3/8" thick sheets, the available dimensions are 48.00" x 120.00", 48.00" x 96.00", and 60.00" x 120.00", each weighing 15.320 lbs/ft. Lastly, at 1/2" thickness, the available sizes are 48.00" x 120.00", 48.00" x 96.00", and 60.00" x 120.00", all with a weight of 20.421 lbs/ft.