Metallurgical Characteristics
JIS SUS316L is an austenitic stainless steel with a face-centered cubic crystal structure. The low carbon content (≤ 0.030%) minimizes carbide precipitation, enhancing corrosion resistance and weldability. Molybdenum addition significantly improves resistance to pitting and crevice corrosion in chloride environments.
Manufacturing Process
MetalZenith employs electric arc furnace melting followed by AOD refining to achieve precise chemical composition. The steel undergoes solution annealing at 1050-1100°C followed by rapid cooling to maintain austenitic structure and prevent sensitization. Cold working and hot working processes are carefully controlled to achieve desired mechanical properties.
Heat Treatment
Solution annealing is performed at 1050-1100°C for 2-10 minutes per mm thickness, followed by rapid cooling in water or air. This treatment dissolves carbides and achieves optimal corrosion resistance. Stress relief annealing at 850-950°C may be applied for dimensional stability without compromising corrosion resistance.
Quality Standards & Testing
All products comply with JIS G4303 standards and undergo comprehensive testing including chemical analysis by optical emission spectroscopy, mechanical testing per JIS Z2241, ultrasonic testing for internal soundness, and intergranular corrosion testing per ASTM A262. MetalZenith provides complete material traceability and certified test reports with every shipment.
🧪 Chemical Composition
Element | Composition (%) |
---|---|
Carbon (C) | ≤ 0.030 |
Silicon (Si) | ≤ 1.00 |
Manganese (Mn) | ≤ 2.00 |
Phosphorus (P) | ≤ 0.045 |
Sulfur (S) | ≤ 0.030 |
Chromium (Cr) | 16.00 - 18.00 |
Nickel (Ni) | 10.00 - 14.00 |
Molybdenum (Mo) | 2.00 - 3.00 |
Nitrogen (N) | ≤ 0.10 |
Iron (Fe) | Balance |
⚙️ Mechanical Properties
Property | Value |
---|---|
Tensile Strength | ≥ 520 MPa |
Yield Strength (0.2% Offset) | ≥ 205 MPa |
Elongation (50mm gauge) | ≥ 40% |
Hardness (HRB) | ≤ 95 |
Hardness (HV) | 200 - 250 |
Impact Energy (Charpy V-notch, 20°C) | ≥ 120 J |
Young's Modulus | 200 GPa |
Fatigue Limit (107 cycles) | 240 MPa |
Poisson's Ratio | 0.30 |
🔬 Physical Properties
Property | Value |
---|---|
Density (20°C) | 8.00 g/cm³ |
Melting Point | 1400 - 1450°C |
Thermal Conductivity (20°C) | 16.3 W/m·K |
Thermal Expansion Coefficient (20-100°C) | 16.0×10-6/K |
Specific Heat Capacity (20°C) | 500 J/kg·K |
Electrical Resistivity (20°C) | 0.74 µΩ·m |
Magnetic Permeability | 1.02 (Non-magnetic) |
Thermal Diffusivity (20°C) | 4.1×10-6 m²/s |
📏 Product Specifications
Specification | Available Options |
---|---|
Product Forms | Round bars, square bars, flat bars, sheets, plates, tubes, pipes, coils |
Round Bar Diameter | 6mm - 300mm |
Sheet Thickness | 0.3mm - 6.0mm |
Plate Thickness | 6mm - 100mm |
Tube Outer Diameter | 6mm - 219mm |
Standards Compliance | JIS G4303, ASTM A240, ASTM A276, EN 10088-2 |
Surface Finish | Hot rolled, cold rolled, 2B, BA, No.4, hairline, mirror |
Dimensional Tolerance | ±0.1mm to ±0.5mm (depending on product form) |
Length Options | Standard lengths: 3m, 6m, 12m; Custom lengths available |
Let Us Create Success for Your Project
Professional Team, Premium Products, Complete Service - Your Project Success is Our Mission
Our Advantages in Processing JIS SUS316L

Advanced AOD Refining Technology
MetalZenith employs cutting-edge Argon Oxygen Decarburization (AOD) technology combined with vacuum degassing to achieve ultra-low carbon content (≤ 0.030%) and precise alloy composition control, ensuring superior corrosion resistance and weldability in every batch of JIS SUS316L.
Comprehensive Quality Control System
Our integrated quality management system features real-time chemical analysis using optical emission spectroscopy, automated mechanical testing, and advanced non-destructive testing methods. Every product undergoes rigorous inspection with full material traceability and certified test reports meeting JIS G4303 standards.


Flexible Customization & Global Supply
MetalZenith offers extensive customization capabilities including specialized heat treatments, precision machining, and custom dimensions. Our global distribution network ensures reliable delivery worldwide, supported by technical engineering services and application-specific material solutions.
YOUR TRUSTED STEEL
MANUFACTURING PARTNER
Quick Inquiry
Industries We Serve
Professional steel solutions across major industries
Qualifications & Certifications