Alloy | ASTM | Characteristics |
---|---|---|
A36 | ASTM A36 |
Construction and Structural Framework Industrial Equipment Manufacturing Infrastructure and Transportation Projects |
CHEMICAL COMPOSITION
- The chemical composition of the material primarily consists of the following elements: Carbon at 0.26%, Copper at 0.2%, Iron at 99%, Manganese at 0.75%, with Phosphorus having a maximum of 0.04% and Sulfur having a maximum of 0.05%.
MECHANICAL INFORMATION
- The material features a carbon content of 0.26%, copper at 0.2%, and a predominant presence of iron at 99%, along with manganese at 0.75%, with phosphorus and sulfur each capped at 0.04% and 0.05% respectively. It exhibits a density of 0.282 lb/in³ or 7.8 g/cc. The ultimate tensile strength reaches 58,000 psi (400 MPa), while its yield tensile strength is 47,700 psi (315 MPa), and its shear strength measures 43,500 psi (300 MPa). The melting point ranges from 2,590 to 2,670°F (1,420 to 1,460°C). A Brinell Hardness of 140 and a production method of hot rolling characterize this material. The available sizes vary in thickness and weight, with lengths consistently at 240 inches, demonstrating a wide range of applications.
AVAILABLE SIZES
- The available sizes for this category include a variety of dimensions with specific thicknesses and lengths, all measured in inches. The sizes offered are 1" x 5/8" x 1/8" with a thickness of 1/8", resulting in a weight of 0.639 lbs/ft over a length of 240.00"; 2" x 1-1/4" x 3/16" with a thickness of 3/16" and a weight of 1.959 lbs/ft over 240.00"; 2" x 1-1/2" pieces are available in thicknesses of 1/8" (1.440 lbs/ft), 3/16" (2.120 lbs/ft), and 1/4" (2.769 lbs/ft), all with 240.00" lengths. For 2-1/2" x 1-1/2" sections, the 3/16" thickness weighs 2.439 lbs/ft and the 1/4" thickness weighs 3.189 lbs/ft, with each spanning 240.00". The 2-1/2" x 2" pieces can be acquired in 3/16" (2.750 lbs/ft), 1/4" (3.620 lbs/ft), and 3/8" (5.300 lbs/ft) thicknesses, all extending to 240.00". The 3" x 2" dimensions feature diverse thicknesses, including 3/16" with a weight of 3.070 lbs/ft, 1/4" at 4.100 lbs/ft, 5/16" at 5.000 lbs/ft, 3/8" at 5.900 lbs/ft, and 1/2" at 7.700 lbs/ft, each maintaining the 240.00" length. Additional options are the 3" x 2-1/2" x 1/4" section with a weight of 4.500 lbs/ft, and 3" x 2-1/2" x 3/8" at 6.600 lbs/ft, both 240.00" long. The 3-1/2" x 2-1/2" sizes come in thicknesses ranging from 1/4" (4.899 lbs/ft), 5/16" (6.100 lbs/ft), and 3/8" (7.200 lbs/ft), likewise having a standard length of 240.00".