Dapatkan Penawaran
Alloy | ASTM | Characteristics |
---|---|---|
A1011 | ASTM A1011 |
Structural framework for buildings and bridges. Manufacturing of automotive components. Production of heavy machinery and equipment. |
CHEMICAL COMPOSITION
- The chemical composition of the material is comprised of a maximum of 0.15% Carbon (C), a maximum of 0.6% Manganese (Mn), a maximum of 0.03% Phosphorus (P), and a maximum of 0.035% Sulfur (S).
MECHANICAL INFORMATION
- The mechanical information for this material includes a density of 7.87 g/cc (0.284 lb/in³), an ultimate tensile strength of 400 MPa (58,000 psi), and a yield tensile strength of 250 MPa (36,300 psi). The Brinell hardness of the material is 75. The chemical composition features elements like Carbon (C) with a maximum of 0.15%, Manganese (Mn) up to 0.6%, Phosphorus (P) up to 0.03%, and Sulfur (S) up to 0.035%. These values are general approximations, and material test reports can be obtained from our Customer Service Department. This material is available in various sizes, with thickness options ranging from 10ga to 16ga, widths from 48.00" to 72.00", and lengths from 96.00" to 144.00". The weight per foot varies accordingly, from 2.500 lbs/ft for 16ga to 5.625 lbs/ft for 10ga.
AVAILABLE SIZES
- Available sizes for this category include the following: 16 gauge with dimensions of 48.00 inches in width and available lengths of 120.00 inches, 144.00 inches, and 96.00 inches carrying a weight of 2.500 lbs/ft; 14 gauge with a 48.00 inch width and available lengths of 120.00 inches, 144.00 inches, and 96.00 inches with a weight of 3.125 lbs/ft, as well as a 60.00 inch width and 120.00 inch length with the same weight per foot; 12 gauge with a 48.00 inch width in lengths of 120.00 inches, 144.00 inches, and 96.00 inches, or a 60.00 inch width with a length of 120.00 inches, all weighing 4.375 lbs/ft; 11 gauge in a 48.00 inch width and lengths of 120.00 inches, 144.00 inches, and 96.00 inches, or a 60.00 inch width available in lengths of 120.00 inches and 144.00 inches, plus a 72.00 inch width with a 120.00 inch length, each with a weight of 5.000 lbs/ft; and 10 gauge available in a 48.00 inch width with lengths of 120.00 inches and 96.00 inches, as well as a 60.00 inch width with a 120.00 inch length, all weighing 5.625 lbs/ft.