Dapatkan Penawaran
Alloy | ASTM | Characteristics |
---|---|---|
A36 | ASTM A36 |
Structural support in construction and building frameworks. Manufacturing of machinery and industrial equipment. Creation of transportation infrastructure such as bridges and overpasses. |
CHEMICAL COMPOSITION
- The chemical composition of this category includes 0.26% Carbon (C), 0.2% Copper (Cu), approximately 99% Iron (Fe), 0.75% Manganese (Mn), with a maximum of 0.04% Phosphorus (P) and a maximum of 0.05% Sulfur (S).
MECHANICAL INFORMATION
- The material possesses a chemical composition of 0.26% Carbon, 0.2% Copper, 99% Iron, and 0.75% Manganese, with maximum allowable limits of 0.04% Phosphorus and 0.05% Sulfur. Its mechanical properties feature a density of 0.282 lb/in³ (7.8 g/cc), an ultimate tensile strength of 58,000 psi (400 MPa), a yield tensile strength of 47,700 psi (315 MPa), a shear strength of 43,500 psi (300 MPa), and a hardness of 140 Brinell. The material has a melting point range of 2,590 - 2,670°F (1,420 - 1,460°C) and is produced via a hot-rolled method. The dimensions available vary extensively, including sizes such as 3" x 7.1# and 18" x 45.8#, each with specific depth, width, thickness, length, and weight specifications. Please note that these chemical compositions and mechanical properties are general approximations, and our Customer Service Department can provide detailed material test reports upon request.
AVAILABLE SIZES
- The available sizes for this product category include the following dimensions with their respective depths, widths, thicknesses, lengths, and weights in pounds per foot: 3" x 7.1# with a depth of 3", width of 1.938", thickness of 0.312", length of 240.00", and weight of 7.100 lbs/ft; 4" x 13.8# with a depth of 4", width of 2.5", thickness of 0.5", length of 240.00", and weight of 13.800 lbs/ft; 6" x 12# with a depth of 6", width of 2.497", thickness of 0.31", length of 240.00", and weight of 12.000 lbs/ft; 6" x 15.3# with a depth of 6", width of 3.5", thickness of 0.34", length of 240.00", and weight of 15.300 lbs/ft; 6" x 16.3# with a depth of 6", width of 3", thickness of 0.375", length of 240.00", and weight of 16.300 lbs/ft; 6" x 18# with a depth of 6", width of 3.5", thickness of 0.379", length of 240.00", and weight of 18.000 lbs/ft; 8" x 8.5# with a depth of 8", width of 1.874", thickness of 0.179", length of 240.00", and weight of 8.500 lbs/ft; 8" x 18.7# with a depth of 8", width of 2.978", thickness of 0.353", length of 240.00", and weight of 18.700 lbs/ft; 8" x 20# with a depth of 8", width of 3.025", thickness of 0.4", length of 240.00", and weight of 20.000 lbs/ft; 8" x 22.8# with a depth of 8", width of 3.502", thickness of 0.427", length of 240.00", and weight of 22.800 lbs/ft; 10" x 8.4# with a depth of 10", width of 1.5", thickness of 0.17", length of 240.00", and weight of 8.400 lbs/ft; 10" x 22# with a depth of 10", width of 3.315", thickness of 0.29", length of 240.00", and weight of 21.999 lbs/ft; 12" x 10.6# with a depth of 12", width of 1.5", thickness of 0.19", length of 240.00", and weight of 10.599 lbs/ft; 18" x 42.7# with a depth of 18", width of 3.95", thickness of 0.45", length of 240.00", and weight of 42.700 lbs/ft; and 18" x 45.8# with a depth of 18", width of 4", thickness of 0.5", length of 240.00", and weight of 45.800 lbs/ft.