Zu Produktinformationen springen
1 von 1

Hot Rolled Steel Junior Beam

Hot Rolled Steel Junior Beam

Hot Rolled Steel Junior Beam is a type of structural steel beam that is manufactured through the hot rolling process, providing it with a robust and durable profile. Known for its high strength and load-bearing capacity, this beam is commonly used in construction and engineering projects, offering superior performance in supporting structures. Its versatility and resilience make it ideal for frameworks, bridges, platforms, and various architectural applications.

Vollständige Details anzeigen

Dapatkan Penawaran

Alloy ASTM Characteristics
A992 / A572-50

Construction of building frameworks and support structures.

Manufacturing of bridges and infrastructure projects.

Fabrication of industrial machinery and equipment.

CHEMICAL COMPOSITION

  • The chemical composition of this category is characterized by the following elements with their respective percentages: Carbon (C) at 0.23%, Manganese (Mn) ranging from 0.5% to 1.6%, Silicon (Si) at 0.4%, Vanadium (V) at 0.15%, Cobalt (Co) at 0.05%, Phosphorus (P) at 0.035%, and Sulfur (S) at 0.045%.

MECHANICAL INFORMATION

  • The mechanical properties of this material are characterized by an ultimate tensile strength of 65,000 psi (448 MPa) and a yield tensile strength of 50,000 psi (345 MPa), with a Brinell hardness of 143. This material's chemical composition includes a carbon content of 0.23%, manganese ranging from 0.5% to 1.6%, silicon at 0.4%, vanadium at 0.15%, cobalt at 0.05%, phosphorus at 0.035%, and sulfur at 0.045%. Available in various sizes, such as 3" x 2.9#, 4" x 3.2#, 6" x 4.4#, and 8" x 6.5#, each differing in dimensions and weight, these specifications are general approximations. For precise data, please contact our Customer Service Department for material test reports.

AVAILABLE SIZES

  • Available sizes for this category include 3" x 2.9# with a depth of 3", width of 2.25", thickness of 0.09", flange thickness of 0.13", length of 412.00", and weight of 2.900 lbs/ft; 4" x 3.2# with a depth of 4", width of 2.25", thickness of 0.092", flange thickness of 0.13", length of 412.00", and weight of 3.200 lbs/ft; 6" x 4.4# with a depth of 6", width of 1.844", thickness of 0.114", flange thickness of 0.171", length of 240.00", and weight of 4.400 lbs/ft; 8" x 6.5# with a depth of 8", width of 2.281", thickness of 0.135", flange thickness of 0.189", length of 240.00", and weight of 6.500 lbs/ft.