Dapatkan Penawaran
Alloy | ASTM | Characteristics |
---|---|---|
A992 / A572-50 |
Construction of bridges and large-scale infrastructure projects. Framework support for commercial and industrial buildings. Support beams in parking garages and multi-story structures. |
CHEMICAL COMPOSITION
- The chemical composition of this category consists of approximately 0.23% Carbon (C), Manganese (Mn) ranging from 0.5% to 1.6%, 0.4% Silicon (Si), 0.15% Vanadium (V), 0.05% Cobalt (Co), 0.035% Phosphorus (P), and 0.045% Sulfur (S).
MECHANICAL INFORMATION
- The material characterized by its chemical composition, including elements such as Carbon (C) at 0.23%, Manganese (Mn) ranging from 0.5% to 1.6%, Silicon (Si) at 0.4%, Vanadium (V) at 0.15%, Cobalt (Co) at 0.05%, Phosphorus (P) at 0.035%, and Sulfur (S) at 0.045%, possesses particular mechanical properties. These include an ultimate tensile strength of 65,000 psi (448 MPa) and a yield tensile strength of 50,000 psi (345 MPa), with a Brinell hardness of 143. Available in a variety of sizes, the range includes section dimensions from 3" x 5.7# to 10" x 35#, with varying depths, widths, thicknesses, lengths, and respective weights. These specifications offer versatility for different applications, proving the material's adaptability to specific project requirements. Please reach out to the Customer Service Department for detailed material test reports and further inquiries.
AVAILABLE SIZES
- Available sizes for this category include: 3" x 5.7# with a depth of 3", width of 2.33", thickness of .170", and lengths of 240.00" or 480.00" with a weight of 5.700 lbs/ft; 3" x 7.5# with a depth of 3", width of 2.509", thickness of .349", length of 240.00", and weight of 7.500 lbs/ft; 4" x 7.7# with a depth of 4", width of 2.663", thickness of .193", and lengths of 240.00" or 480.00" with a weight of 7.700 lbs/ft; 4" x 9.5# with a depth of 4", width of 2.8", thickness of .326", length of 240.00", and weight of 9.500 lbs/ft; 5" x 10# with a depth of 5", width of 3.004", thickness of .214", and lengths of 240.00" or 480.00" with a weight of 9.999 lbs/ft; 6" x 12.5# with a depth of 6", width of 3.332", thickness of .232", length of 240.00", and weight of 12.500 lbs/ft; 6" x 17.25# with a depth of 6", width of 3.565", thickness of .465", and lengths of 240.00" or 480.00" with a weight of 17.250 lbs/ft; 8" x 18.4# with a depth of 8", width of 4.001", thickness of .271", length of 240.00", and weight of 18.399 lbs/ft; 8" x 23# with a depth of 8", width of 4.171", thickness of .441", length of 240.00", and weight of 23.000 lbs/ft; 10" x 25.4# with a depth of 10", width of 4.661", thickness of .311", length of 240.00", and weight of 25.400 lbs/ft; and 10" x 35# with a depth of 10", width of 10", thickness of .491", length of 240.00", and weight of 35.000 lbs/ft.