ASTM A786 |
Industrial flooring in factories and warehouses. Stair treads and walkways in commercial buildings. Vehicular and pedestrian ramps for added traction. |
CHEMICAL COMPOSITION
- The chemical composition of this category consists of carbon (C) ranging from 0.1% to 0.3%, manganese (Mn) ranging from 0.3% to 0.7%, phosphorus (P) at 0.05%, and sulfur (S) at 0.05%.
MECHANICAL INFORMATION
- The material features a chemical composition of 0.1-0.3% Carbon, 0.3-0.7% Manganese, and 0.05% each for Phosphorus and Sulfur. It exhibits an ultimate tensile strength of 60,000 psi (414 MPa) and a yield tensile strength of 33,000 psi (207 MPa). These mechanical values are approximations, and for precise data, material test reports can be requested from our Customer Service Department. This material is available in various sizes and weights, including thickness options like 14 gauge to 1/2 inch, with corresponding widths from 48.00 inches to 60.00 inches, and lengths up to 144.00 inches, featuring weights ranging from 3.750 lbs/ft to 21.470 lbs/ft. For detailed sizing and weight specifications, please contact us.
AVAILABLE SIZES
- The available sizes for this category are as follows: for a thickness of 14 gauge, the available options are 48.00" width with lengths of either 120.00" or 96.00", both weighing 3.750 lbs/ft. For a thickness of 12 gauge, sizes are available in 48.00" width with lengths of either 120.00" or 96.00", with a weight of 5.250 lbs/ft. The 1/8" thickness comes in widths of 48.00" and 60.00", with lengths of 120.00", 144.00", and 96.00", all weighing 6.160 lbs/ft. For the 3/16" thickness, widths are available in 48.00" and 60.00" with lengths of either 120.00" or 96.00", weighing 8.711 lbs/ft. The 1/4" thickness offers widths of 48.00" and 60.00" with lengths of 120.00" and 96.00", weighing 11.259 lbs/ft. For the 3/8" thickness, options include 48.00" and 60.00" widths with lengths of 120.00" and 96.00", weighing 16.370 lbs/ft. Finally, for a 1/2" thickness, the available dimensions are 48.00" and 60.00" widths with lengths of 120.00" and 96.00", each weighing 21.470 lbs/ft.