EN 13CrMo4-5 is a high-performance chrome-molybdenum alloy steel specifically designed for pressure vessel applications operating at elevated temperatures. This low-alloy steel combines excellent creep resistance, superior weldability, and outstanding mechanical properties, making it the preferred choice for critical industrial applications requiring reliable performance under extreme conditions.

MetalZenith's Advanced Manufacturing Excellence

As a leading steel manufacturer, MetalZenith employs state-of-the-art electric arc furnace technology and advanced secondary refining processes to produce EN 13CrMo4-5 with exceptional chemical homogeneity and mechanical consistency. Our controlled atmosphere heat treatment facilities ensure optimal microstructure development, while our comprehensive quality management system guarantees compliance with international standards including EN 10028-2, ASTM A387, and PED 2014/68/EU.

Key Applications & Industries

  • Pressure vessels and boilers operating up to 530°C
  • Petrochemical processing equipment and reactors
  • Power generation components and steam systems
  • Oil and gas refinery equipment
  • Chemical processing vessels and heat exchangers

Quality Assurance & Certification

MetalZenith's EN 13CrMo4-5 undergoes rigorous testing including chemical analysis, mechanical property verification, non-destructive testing, and microstructural examination. Our ISO 9001:2015 certified facilities ensure consistent quality, while our technical support team provides comprehensive engineering assistance for optimal material selection and application-specific customization.

Vollständige Details anzeigen

20 Years Experience | 1000+ Brand Partners | Full Customization

We have 20 years of industry experience, have partnered with over 1,000 brands, and support any customization needs.

Technical Specifications

Product Overview

Metallurgical Characteristics

EN 13CrMo4-5 is a low-alloy chrome-molybdenum steel with a ferritic-pearlitic microstructure optimized for high-temperature pressure vessel applications. The chromium content provides oxidation resistance and hardenability, while molybdenum enhances creep strength and thermal stability. The controlled carbon content ensures excellent weldability without preheating requirements for most applications.

Heat Treatment Process

MetalZenith's EN 13CrMo4-5 undergoes precision heat treatment consisting of normalizing at 920-960°C followed by tempering at 680-720°C. This thermal processing develops optimal mechanical properties and stress relief while maintaining fine grain structure. Our computer-controlled furnaces ensure uniform heating and cooling rates, resulting in consistent microstructure and mechanical properties throughout the material cross-section.

Manufacturing Excellence

Our advanced steelmaking process begins with electric arc furnace melting using premium raw materials, followed by ladle refining and vacuum degassing to achieve ultra-low inclusion content. Continuous casting and controlled rolling ensure excellent surface quality and dimensional accuracy. Post-rolling heat treatment in protective atmosphere furnaces prevents decarburization and surface oxidation.

Quality Standards & Compliance

All EN 13CrMo4-5 products manufactured by MetalZenith comply with international standards including EN 10028-2, ASTM A387 Grade 11, and PED 2014/68/EU requirements. Our quality management system encompasses complete chemical analysis, mechanical property testing, ultrasonic inspection, and microstructural examination. Full traceability documentation and material certificates are provided with every shipment, ensuring compliance with pressure equipment regulations and customer specifications.

🧪 Chemical Composition

ElementComposition (%)
Carbon (C)0.08 - 0.18
Silicon (Si)0.15 - 0.50
Manganese (Mn)0.40 - 0.80
Phosphorus (P)≤ 0.025
Sulfur (S)≤ 0.015
Chromium (Cr)0.70 - 1.15
Molybdenum (Mo)0.45 - 0.65
Nickel (Ni)≤ 0.30
Aluminum (Al)≥ 0.020
Copper (Cu)≤ 0.30
Vanadium (V)≤ 0.02
Niobium (Nb)≤ 0.02

⚙️ Mechanical Properties

PropertyValue
Tensile Strength (Rm)440 - 590 MPa
Yield Strength (Rp0.2)≥ 275 MPa
Elongation (A5)≥ 22%
Reduction of Area (Z)≥ 50%
Brinell Hardness (HB)130 - 180 HB
Impact Energy (KV) at 20°C≥ 40 J
Impact Energy (KV) at 0°C≥ 27 J
Young's Modulus (E)210 GPa
Poisson's Ratio (ν)0.30
Fatigue Limit (107 cycles)200 MPa
Creep Rupture Strength (100,000h at 500°C)120 MPa
Creep Rupture Strength (100,000h at 530°C)90 MPa

🔬 Physical Properties

PropertyValue
Density7.85 g/cm³
Melting Point1480 - 1520°C
Thermal Conductivity (20°C)42 W/m·K
Thermal Conductivity (500°C)35 W/m·K
Thermal Expansion Coefficient (20-100°C)11.5×10-6/K
Thermal Expansion Coefficient (20-500°C)12.8×10-6/K
Specific Heat Capacity (20°C)460 J/kg·K
Specific Heat Capacity (500°C)580 J/kg·K
Electrical Resistivity (20°C)0.25 µΩ·m
Magnetic PermeabilityFerromagnetic
Curie Temperature770°C
Thermal Diffusivity (20°C)11.6×10-6 m²/s

📏 Product Specifications

SpecificationAvailable Options
Product FormsPlates, Sheets, Bars, Forgings, Tubes, Pipes
Plate Thickness6 - 250 mm
Sheet Thickness0.5 - 6 mm
Bar Diameter10 - 500 mm
Tube Outer Diameter10 - 610 mm
Maximum Dimensions3000 × 12000 mm (plates)
Standards ComplianceEN 10028-2, ASTM A387 Gr.11, JIS G3118, GB 713
Heat Treatment ConditionNormalized and Tempered (+NT)
Surface FinishHot Rolled, Pickled, Shot Blasted, Machined
Dimensional Tolerance±0.5mm (thickness), ±5mm (width/length)
Edge ConditionMill Edge, Sheared, Flame Cut, Machined
Testing RequirementsEN 10204 3.1/3.2, NACE MR0175, PED 2014/68/EU

Let Us Create Success for Your Project

Professional Team, Premium Products, Complete Service - Your Project Success is Our Mission

Our Advantages in Processing EN 13CrMo4-5

Manufacturing Advantage 1

Advanced Metallurgical Processing

MetalZenith utilizes cutting-edge electric arc furnace technology combined with ladle refining and vacuum degassing to achieve superior chemical homogeneity and reduced inclusion content in EN 13CrMo4-5, ensuring exceptional mechanical properties and enhanced service life in high-temperature applications.

Comprehensive Quality Control System

Our state-of-the-art testing laboratory performs complete chemical analysis, mechanical property testing, ultrasonic inspection, and microstructural examination on every heat of EN 13CrMo4-5, guaranteeing compliance with international standards and providing full traceability documentation for critical applications.

Manufacturing Advantage 2
Manufacturing Advantage 3

Custom Solutions & Global Supply

MetalZenith offers extensive customization capabilities including precision cutting, heat treatment optimization, and surface finishing for EN 13CrMo4-5, supported by our global logistics network ensuring timely delivery and technical support worldwide for pressure vessel manufacturers and engineering contractors.

YOUR TRUSTED STEEL

MANUFACTURING PARTNER

20
Years Experience
Leading Steel Manufacturing & Distribution
1000+
Brand Partners
Trusted by Global Industry Leaders
Full
Customization
Tailored Solutions for Every Project
50M+
Tons Delivered
High-Quality Steel Products Worldwide
95%
Client Retention
Long-term Partnership Success
ISO 9001
Certified Quality
International Standards Compliance
20
Years Experience
Leading Steel Manufacturing & Distribution
1000+
Brand Partners
Trusted by Global Industry Leaders
Full
Customization
Tailored Solutions for Every Project
50M+
Tons Delivered
High-Quality Steel Products Worldwide
95%
Client Retention
Long-term Partnership Success
ISO 9001
Certified Quality
International Standards Compliance
GET IN TOUCH

Quick Inquiry

Industries We Serve

Professional steel solutions across major industries

Construction

High-rise Buildings • Infrastructure • Commercial Real Estate

Oil & Gas

Pipeline Systems • Storage Equipment • Refinery Facilities

Manufacturing

Precision Machinery • Industrial Equipment • Automation Systems

Automotive

Body Structure • Chassis Components • Engine Parts

Shipbuilding

Hull Structure • Marine Engineering • Port Equipment

Energy & Power

Power Generation • Transmission Towers • Renewable Energy

Aerospace

Aircraft Materials • Precision Components • Special Alloys

Railway

Track Systems • Vehicle Manufacturing • Infrastructure

Qualifications & Certifications

Client logo
Client logo
Client logo
Client logo
Client logo