Dapatkan Penawaran
Alloy | ASTM | Characteristics |
---|---|---|
A366/1008 | ASTM A1008 |
Automotive body panels and structural components. Appliance housing and internal mechanical parts. Construction materials, including roofing and wall cladding. |
CHEMICAL COMPOSITION
- The chemical composition of this material primarily consists of 99.31 - 99.7% Fe, 0.3 - 0.5% Mn, with a maximum of 0.05% S and a maximum of 0.4% P.
MECHANICAL INFORMATION
- The mechanical properties of the material include a density of 0.284 lb/in³ (7.87 g/cc), an ultimate tensile strength ranging from 49,900 psi (303 - 358 MPa), and a yield tensile strength between 26,100 to 34,800 psi (108 - 240 MPa). The material is produced through a cold roll method. The sizes available range from 24 gauge to 11 gauge, with dimensions including a thickness that varies, a standard width of 48.00 inches or 60.00 inches, a length of 96.00 inches or 120.00 inches, and weights ranging from 0.999 lbs/ft to 5.000 lbs/ft, depending on the gauge.
AVAILABLE SIZES
- Available sizes include various gauges and dimensions. For 24ga, available sizes are 48.00" in width by 120.00" and 96.00" in length, both with a weight of 0.999 lbs/ft. In 22ga, the choices are 48.00" by 120.00" and 96.00", each weighing 1.250 lbs/ft. The 20ga options expand to 48.00" and 60.00" widths by 120.00" and 96.00" lengths, with a consistent weight of 1.500 lbs/ft. For 18ga, the sizes are 48.00" by 120.00" and 96.00", each with a weight of 2.000 lbs/ft. Moving to 16ga, available dimensions are 48.00" and 60.00" widths by 120.00" and 96.00" lengths, all weighing 2.500 lbs/ft. The 14ga options include 48.00" and 60.00" widths by 120.00" and 96.00" lengths, with each piece weighing 3.125 lbs/ft. For 12ga, size is available at 48.00" by 120.00" and 96.00", weighing 4.375 lbs/ft. Lastly, for 11ga, the dimensions are 48.00" by 120.00" and 96.00", and each weighs 5.000 lbs/ft.