Alloy | ASTM | Characteristics |
---|---|---|
AR200 | ASTM A514 |
Heavy machinery and equipment manufacturing Mining and construction industries Transportation and material handling systems |
CHEMICAL COMPOSITION
- The chemical composition for this category may typically include Carbon (C) at 0.12-0.20%, Manganese (Mn) at 0.60-1.65%, Phosphorus (P) at a maximum of 0.04%, Sulfur (S) at a maximum of 0.05%, and Silicon (Si) at 0.15-0.30%.
MECHANICAL INFORMATION
- Ultimate tensile strength is 90,000 psi (621 MPa), and yield tensile strength is 70,000 psi (483 MPa). The Brinell hardness range is 180 to 235. Note that this material is not intended for structural use. The chemical compositions and mechanical properties provided are general approximations. For detailed material test reports, please contact our Customer Service Department. Available sizes include a thickness of 3/16" with dimensions of 60.00" x 120.00" and a weight of 7.659 lbs/ft, and a thickness of 3/8" with dimensions of both 48.00" x 120.00" and 60.00" x 120.00", each with a weight of 15.320 lbs/ft.
AVAILABLE SIZES
- The available sizes for this category are as follows: a thickness of 3/16 inch with a width of 60 inches and a length of 120 inches, weighing 7.659 pounds per foot; a thickness of 3/8 inch with a width of 48 inches and a length of 120 inches, weighing 15.320 pounds per foot; and a thickness of 3/8 inch with a width of 60 inches and a length of 120 inches, also weighing 15.320 pounds per foot.