The 360 Brass Square Bar is known for its excellent machinability and corrosion resistance, making it a popular choice for applications requiring precise fabrication and reliable strength. This versatile material is often used in the manufacturing of fittings, valve stems, fasteners, and gears, offering a balance of workability and durability. With its distinctive golden color, it is also favored in decorative and architectural projects.

Vollständige Details anzeigen

Dapatkan Penawaran

Alloy ASTM Characteristics
360 ASTM B16

Manufacturing components for commercial fittings and valves.

Creating decorative items and architectural hardware.

Producing parts for marine and electrical applications.

CHEMICAL COMPOSITION

  • The chemical composition of this category includes 61.5% Copper (Cu), 3.00% Lead (Pb), and 35.5% Zinc (Zn).

MECHANICAL INFORMATION

  • This product consists primarily of Copper (Cu) at 61.5%, with additional components of Lead (Pb) at 3.00% and Zinc (Zn) at 35.5%. The material has a density of 0.307 lb/in³ (8.50 g/cc). It possesses an ultimate tensile strength ranging from 49,000 to 68,000 psi (338 to 469 MPa) and a yield tensile strength of 18,000 to 45,000 psi (124 to 310 MPa). The shear strength varies between 30,500 to 45,000 psi (210 to 310 MPa). The melting point of this alloy ranges from 1,630 to 1,650°F (855 to 900°C). It is tempered to H02 and features a Rockwell hardness of B78. Standard available sizes include diameters from 1/4" to 2" at a uniform length of 144" with corresponding weights from 0.230 to 14.740 lbs/ft. For detailed material test reports, please contact our Customer Service Department.

AVAILABLE SIZES

  • Available sizes for this category include components with a length of 144 inches and varying weights per foot: 0.230 lbs/ft for 1/4", 0.518 lbs/ft for 3/8", 0.921 lbs/ft for 1/2", 1.439 lbs/ft for 5/8", 2.072 lbs/ft for 3/4", 3.684 lbs/ft for 1", 5.756 lbs/ft for 1-1/4", 8.289 lbs/ft for 1-1/2", 11.280 lbs/ft for 1-3/4", and 14.740 lbs/ft for 2".