Dapatkan Penawaran
Alloy | ASTM | Characteristics |
---|---|---|
360 | ASTM B16 |
Manufacturing precise mechanical components such as gears and pinions. Producing decorative architectural elements and fixtures. Fabricating electrical connectors and terminals due to excellent conductivity. |
CHEMICAL COMPOSITION
- The chemical composition of this category includes Copper (Cu) at 61.5%, Lead (Pb) at 3.00%, and Zinc (Zn) at 35.5%.
MECHANICAL INFORMATION
- The material, composed of 61.5% Copper (Cu), 3.00% Lead (Pb), and 35.5% Zinc (Zn), exhibits a density of 0.307 lb/in³ (8.50 g/cm³). It has an ultimate tensile strength ranging from 49,000 to 68,000 psi (338 to 469 MPa) and a yield tensile strength between 18,000 and 45,000 psi (124 to 310 MPa). The shear strength varies from 30,500 to 45,000 psi (210 to 310 MPa) with a melting point between 1,630 and 1,650°F (855 to 900°C). The material is available in temper H02 and has a Rockwell hardness of B78. For detailed material test reports, please contact our Customer Service Department.
AVAILABLE SIZES
- The available sizes for this category include diameters ranging from 1/8" to 3", each with a consistent length of 144.00 inches. The weights per foot vary accordingly, starting from 0.045 lbs/ft for the 1/8" size, increasing incrementally through 0.102 lbs/ft for 3/16", 0.181 lbs/ft for 1/4", 0.283 lbs/ft for 5/16", 0.407 lbs/ft for 3/8", 0.554 lbs/ft for 7/16", 0.723 lbs/ft for 1/2", 0.915 lbs/ft for 9/16", 1.130 lbs/ft for 5/8", 1.628 lbs/ft for 3/4", 2.215 lbs/ft for 7/8", 2.893 lbs/ft for 1", 3.662 lbs/ft for 1-1/8", 4.521 lbs/ft for 1-1/4", 5.470 lbs/ft for 1-3/8", 6.510 lbs/ft for 1-1/2", 7.640 lbs/ft for 1-5/8", 8.861 lbs/ft for 1-3/4", 11.570 lbs/ft for 2", 14.650 lbs/ft for 2-1/4", 18.080 lbs/ft for 2-1/2", 21.880 lbs/ft for 2-3/4", and reaching up to 26.040 lbs/ft for the largest size of 3".