Dapatkan Penawaran
Alloy | ASTM | Characteristics |
---|---|---|
360 | ASTM B16 |
Used in the manufacturing of gears and locks due to its excellent machinability and strength. Utilized in decorative and architectural applications for its aesthetic appeal and corrosion resistance. Commonly employed in the production of marine hardware and fittings because of its durability and resistance to seawater. |
CHEMICAL COMPOSITION
- The chemical composition of this material consists of Copper (Cu) at 61.5%, Lead (Pb) at 3.00%, and Zinc (Zn) at 35.5%.
MECHANICAL INFORMATION
- The material with a chemical composition of 61.5% Cu, 3.00% Pb, and 35.5% Zn exhibits several mechanical properties. It has a density of 0.307 lb/in³ (8.50 g/cc) and a melting point range of 1,630 - 1,650°F (855 - 900°C). The ultimate tensile strength ranges from 49,000 to 68,000 psi (338 - 469 MPa), while the yield tensile strength varies between 18,000 to 45,000 psi (124 - 310 MPa). The shear strength is between 30,500 to 45,000 psi (210 - 310 MPa). It has a Rockwell hardness of B78 in the temper designation H02. The available sizes include diameters from 1/4" to 1-1/4", each with a length of 144.00" and varying weights ranging from 0.199 lbs/ft to 4.985 lbs/ft. The stated chemical compositions and mechanical properties are approximations, so for precise data, material test reports should be requested from the Customer Service Department.
AVAILABLE SIZES
- The available sizes for this category are as follows: 1/4 inch in diameter with a length of 144.00 inches and a weight of 0.199 lbs/ft, 5/16 inch in diameter with a length of 144.00 inches and a weight of 0.312 lbs/ft, 3/8 inch in diameter with a length of 144.00 inches and a weight of 0.449 lbs/ft, 7/16 inch in diameter with a length of 144.00 inches and a weight of 0.611 lbs/ft, 1/2 inch in diameter with a length of 144.00 inches and a weight of 0.798 lbs/ft, 5/8 inch in diameter with a length of 144.00 inches and a weight of 1.246 lbs/ft, 1 inch in diameter with a length of 144.00 inches and a weight of 3.190 lbs/ft, and 1-1/4 inch in diameter with a length of 144.00 inches and a weight of 4.985 lbs/ft.