Alloy | ASTM | Characteristics |
---|---|---|
360 | ASTM B16 |
Used in the production of marine hardware due to its corrosion resistance and strength. Commonly used for manufacturing industrial machinery parts requiring excellent machinability. Utilized in the creation of decorative architectural components for its aesthetic appeal and workability. |
CHEMICAL COMPOSITION
- The chemical composition consists of copper (Cu) at 61.5%, lead (Pb) at 3.00%, and zinc (Zn) at 35.5%.
MECHANICAL INFORMATION
- The material with Cu 61.5%, Pb 3.00%, and Zn 35.5% composition has a density of 0.307 lb/in³ (8.50 g/cc) and exhibits an ultimate tensile strength ranging from 49,000 to 68,000 psi (338 to 469 MPa), a yield tensile strength from 18,000 to 45,000 psi (124 to 310 MPa), and a shear strength between 30,500 and 45,000 psi (210 to 310 MPa). It has a melting point of 1,630 to 1,650°F (855 to 900°C) and is provided in H02 temper with a Rockwell hardness of B78. Various sizes are available, with lengths of 144 inches and weights ranging from 0.230 to 7.368 lbs/ft, across different width and thickness combinations such as 1/8" x 1/2", 1/4" x 1", and others as specified. For precise material test reports, it is advised to contact the Customer Service Department.
AVAILABLE SIZES
- The available sizes for this category include a range of options with specific dimensions and weights suitable for various applications. The sizes are as follows: 1/8" x 1/2" with a length of 144 inches and a weight of 0.230 lbs/ft, 1/8" x 3/4" also at 144 inches and weighing the same at 0.230 lbs/ft, escalating to 1/8" x 1" with a weight of 0.461 lbs/ft. Further available sizes include 1/8" x 1-1/2" weighing 0.691 lbs/ft; 3/16" x 3/4" at 0.518 lbs/ft; and progressing in size and weight up to 1" x 2" which measures 7.368 lbs/ft. Notably, increments in thickness and width offer various configurations like 1/4" x 4" weighing 3.684 lbs/ft, and 3/8" x 3" at 4.145 lbs/ft, providing versatility and adaptability for diverse industrial needs. Each option maintains a consistent standard length of 144 inches, ensuring uniformity across different sizes.