Dapatkan Penawaran
Alloy | ASTM | Characteristics |
---|---|---|
304 | ASTM A240 |
Architectural applications and interior design elements such as wall panels or decorative features. Fabrication of kitchen equipment and appliances due to its corrosion resistance and aesthetic appeal. Use in marine environments for boat trim and other equipment needing resistance to saltwater corrosion. |
CHEMICAL COMPOSITION
- The chemical composition of this category includes a maximum of 0.08% Carbon (C), Iron (Fe) ranging from 66.34% to 74%, a maximum of 2% Manganese (Mn), Nickel (Ni) between 8% and 10.5%, a maximum of 0.045% Phosphorus (P), a maximum of 0.03% Sulfur (S), a maximum of 1% Silicon (Si), and 20% Chromium (Cr).
MECHANICAL INFORMATION
- The mechanical information for this material indicates it has a density of 0.289 lb/in³ (8.0 g/cc) with an ultimate tensile strength of 73,200 psi (310 MPa) and a yield tensile strength of 31,200 psi (276 MPa). The melting point ranges between 2,550°F to 2,651°F (1,400°C to 1,455°C). The material is in an annealed temper state, with a Rockwell hardness of B70 and a Brinell hardness of 123. These properties reflect general approximations, and material test reports can be provided upon request from the Customer Service Department. Available sizes include 22ga to 16ga with a uniform width of 48.00 inches and length of 120.00 inches, with weights ranging from 1.260 lbs/ft to 2.520 lbs/ft.
AVAILABLE SIZES
- The available sizes for this category include the following gauges with corresponding dimensions and weights: 22 gauge with a thickness of 22ga, a width of 48.00 inches, a length of 120.00 inches, and a weight of 1.260 lbs per foot; 20 gauge with a thickness of 20ga, a width of 48.00 inches, a length of 120.00 inches, and a weight of 1.512 lbs per foot; 18 gauge with a thickness of 18ga, a width of 48.00 inches, a length of 120.00 inches, and a weight of 2.016 lbs per foot; and 16 gauge with a thickness of 16ga, a width of 48.00 inches, a length of 120.00 inches, and a weight of 2.520 lbs per foot.