Alloy | ASTM | Characteristics |
---|---|---|
110 | ASTM B187 |
Electrical conductors and busbars in power systems Heat exchangers and cooling components Plumbing fixtures and water supply systems |
CHEMICAL COMPOSITION
- 110 copper round bar consists of 99.9% copper with minimal oxygen content (0.04%), making it an exceptionally pure copper product. This high purity contributes to its outstanding electrical and thermal conductivity properties.
MECHANICAL INFORMATION
- With impressive mechanical characteristics including a density of 8.94 g/cc, ultimate tensile strength of 320 MPa, and yield strength of 280 MPa, this H04 temper material offers excellent performance in demanding applications. Its melting point ranges from 1,070 to 1,080°C, and it features a Rockwell hardness of B45.
AVAILABLE SIZES
- The product is available in various diameters ranging from 1/8" to 2", all in standard 144" lengths. Weight per foot varies significantly based on diameter, from just 0.048 lbs/ft for 1/8" bar to 12.180 lbs/ft for 2" bar, providing options for diverse industrial applications.