Dapatkan Penawaran
Alloy | ASTM | Characteristics |
---|---|---|
110 | ASTM B152 |
Electrical conductivity applications Architectural and design elements Heat exchangers and cooling systems |
CHEMICAL COMPOSITION
- The chemical composition of this product consists of Copper (Cu) at 99.9% and Oxygen (O) at 0.04%.
MECHANICAL INFORMATION
- The mechanical information for this category includes a density of 0.323 lb/in3 or 8.94 g/cc, an ultimate tensile strength of 46,400 psi or 320 MPa, and a yield tensile strength of 40,600 psi or 280 MPa. The melting point ranges from 1,950 to 1,980°F or 1,070 to 1,080°C. The material is available in tempers H00 and H02. Please note that the provided mechanical properties are general approximations, and it is recommended to contact our Customer Service Department for detailed material test reports. Available sizes include thicknesses of 1/4" and 3/8" with corresponding widths of 36.00" and lengths of 96.00", weighing 11.591 lbs/ft and 17.390 lbs/ft respectively.
AVAILABLE SIZES
- The available sizes for this category include a thickness of 1/4 inch with a width of 36 inches and a length of 96 inches, weighing 11.591 lbs/ft, and a thickness of 3/8 inch with a width of 36 inches and a length of 96 inches, weighing 17.390 lbs/ft.