Dapatkan Penawaran
Alloy | ASTM | Characteristics |
---|---|---|
1055 | ASTM 1055 |
General-purpose hand tools for cutting tasks in construction and metalworking. Precision cutting tools for manufacturing and industrial applications. Gardening tools for trimming and shaping plants and shrubs. |
CHEMICAL COMPOSITION
- The chemical composition of the material consists of Carbon (C) in the range of 0.50 to 0.60%, Manganese (Mn) within 0.60 to 0.90%, Phosphorus (P) with a maximum of 0.04%, and Sulfur (S) with a maximum of 0.05%.
MECHANICAL INFORMATION
- The mechanical properties of this material include a density of 0.284 lb/in3 (7.87 g/cc), an ultimate tensile strength of 94,300 psi (650 MPa), and a yield tensile strength of 51,500 psi (355 MPa). The Brinell hardness is measured at 192. This information, alongside the chemical composition of 0.50-0.60% Carbon, 0.60-0.90% Manganese, and a maximum of 0.04% Phosphorus and 0.05% Sulfur, provides a general understanding of the material's capabilities. Available sizes for this material vary in dimensions and include 3/8"x3" with a weight of 3.330 lbs/ft, 1/2"x3", 1/2"x4", 1/2"x6", 5/8"x6", 3/4"x4", 3/4"x6", 3/4"x8", and 1"x8", with corresponding lengths and weights as specified. For precise material test reports and further details, please contact our Customer Service Department.
AVAILABLE SIZES
- The available sizes for this category are 3/8"x3" with a length of 246.00" and weight of 3.330 lbs/ft, 1/2"x3" with a length of 246.00" and weight of 4.400 lbs/ft, 1/2"x4" with a length of 294.00" and weight of 6.040 lbs/ft, 1/2"x6" with a length of 294.00" and weight of 9.450 lbs/ft, 5/8"x6" with a length of 294.00" and weight of 11.360 lbs/ft, 3/4"x4" with a length of 294.00" and weight of 8.480 lbs/ft, 3/4"x6" with a length of 294.00" and weight of 13.600 lbs/ft, 3/4"x8" with a length of 294.00" and weight of 18.410 lbs/ft, and 1"x8" with a length of 294.00" and weight of 25.170 lbs/ft.