S355J2H steel is a structural hollow section grade that falls under the category of low-carbon steel, specifically designed for use in construction and engineering applications. It is part of the S355 family, which is known for its high strength and excellent weldability. The primary alloying elements in S355J2H include carbon (C), manganese (Mn), and silicon (Si), with the following general composition:

Element Percentage Range (%)
Carbon (C) 0.17 - 0.20
Manganese (Mn) 1.20 - 1.60
Silicon (Si) 0.10 - 0.40
Phosphorus (P) ≤ 0.035
Sulfur (S) ≤ 0.035

Key Characteristics and Properties

S355J2H is characterized by its high yield strength, which typically ranges from 355 MPa (51.5 ksi) to 470 MPa (68.2 ksi), making it suitable for load-bearing applications. Its toughness at low temperatures is another significant property, with a Charpy impact test value of at least 27 J at -20°C (-4°F). This steel grade is also known for its good ductility, allowing for deformation without fracture.

Advantages:
- High Strength: Provides excellent load-bearing capacity.
- Weldability: Suitable for various welding techniques, facilitating construction.
- Versatility: Can be used in a wide range of applications, from bridges to buildings.

Limitations:
- Corrosion Resistance: Moderate resistance, requiring protective coatings in aggressive environments.
- Not Suitable for High-Temperature Applications: Limited performance at elevated temperatures compared to alloy steels.

S355J2H holds a significant position in the market due to its balance of strength, weldability, and cost-effectiveness, making it a popular choice in structural applications.

Alternative Names, Standards, and Equivalents

Standard Organization Designation/Grade Country/Region of Origin Notes/Remarks
EN S355J2H Europe Commonly used in structural applications
ASTM A500 Grade B USA Similar mechanical properties but different chemical composition
DIN 17100 St 52-3 Germany Closest equivalent with minor differences
JIS G3106 SM490A Japan Comparable grade with different impact requirements
ISO 630 International General standard for structural steels

While S355J2H is often compared to other grades, subtle differences in chemical composition and mechanical properties can affect performance in specific applications. For instance, A500 Grade B has a lower manganese content, which may influence its toughness.

Key Properties

Chemical Composition

Element Percentage Range (%)
Carbon (C) 0.17 - 0.20
Manganese (Mn) 1.20 - 1.60
Silicon (Si) 0.10 - 0.40
Phosphorus (P) ≤ 0.035
Sulfur (S) ≤ 0.035

The primary alloying elements in S355J2H play crucial roles in its properties:
- Carbon (C): Enhances strength and hardness.
- Manganese (Mn): Improves hardenability and toughness.
- Silicon (Si): Contributes to deoxidation during steelmaking and enhances strength.

Mechanical Properties

Property Condition/Temper Typical Value/Range (Metric) Typical Value/Range (Imperial) Reference Standard for Test Method
Yield Strength (0.2% offset) Normalized 355 MPa 51.5 ksi EN 10002-1
Tensile Strength Normalized 470 - 630 MPa 68.2 - 91.5 ksi EN 10002-1
Elongation Normalized 20% 20% EN 10002-1
Impact Strength -20°C ≥ 27 J ≥ 20 ft-lbf EN 10045
Hardness (Brinell) - ≤ 200 HB ≤ 200 HB EN 10003

The combination of these mechanical properties makes S355J2H suitable for structural applications where high strength and toughness are required, such as in bridges and buildings.

Physical Properties

Property Condition/Temperature Value (Metric) Value (Imperial)
Density - 7850 kg/m³ 0.284 lb/in³
Melting Point - 1420 - 1540 °C 2590 - 2800 °F
Thermal Conductivity 20°C 50 W/m·K 29 BTU·in/(hr·ft²·°F)
Specific Heat Capacity 20°C 460 J/kg·K 0.11 BTU/lb·°F
Coefficient of Thermal Expansion 20-100°C 12 x 10⁻⁶ /K 6.67 x 10⁻⁶ /°F

The density of S355J2H is significant for weight calculations in structural applications, while its thermal conductivity and specific heat capacity are important for applications involving heat transfer.

Corrosion Resistance

Corrosive Agent Concentration (%) Temperature (°C/°F) Resistance Rating Notes
Atmospheric - Ambient Fair Requires protective coatings
Chlorides - Ambient Poor Susceptible to pitting corrosion
Acids - Ambient Poor Not recommended for acidic environments
Alkalis - Ambient Fair Moderate resistance

S355J2H exhibits moderate corrosion resistance, making it suitable for many environments but requiring protective measures in aggressive conditions. Compared to stainless steels, S355J2H is less resistant to pitting and stress corrosion cracking, particularly in chloride-rich environments.

Heat Resistance

Property/Limit Temperature (°C) Temperature (°F) Remarks
Max Continuous Service Temp 400 °C 752 °F Limited oxidation resistance
Max Intermittent Service Temp 500 °C 932 °F Risk of scaling
Creep Strength Considerations 300 °C 572 °F Begins to lose strength

At elevated temperatures, S355J2H can experience oxidation and scaling, which can affect its structural integrity. It is not recommended for applications requiring high-temperature performance.

Fabrication Properties

Weldability

Welding Process Recommended Filler Metal (AWS Classification) Typical Shielding Gas/Flux Notes
MIG ER70S-6 Argon/CO2 Good for thin sections
TIG ER70S-2 Argon Excellent for precision work
SMAW E7018 - Suitable for thicker sections

S355J2H is known for its excellent weldability, making it suitable for various welding processes. Pre-heating may be required for thicker sections to avoid cracking.

Machinability

Machining Parameter [S355J2H] [AISI 1212] Notes/Tips
Relative Machinability Index 60% 100% Moderate machinability
Typical Cutting Speed (Turning) 80 m/min 120 m/min Use sharp tools

S355J2H has moderate machinability, requiring appropriate tooling and cutting speeds to achieve optimal results.

Formability

S355J2H can be cold and hot formed, with good ductility allowing for bending and shaping. However, care must be taken to avoid work hardening, which can lead to cracking.

Heat Treatment

Treatment Process Temperature Range (°C/°F) Typical Soaking Time Cooling Method Primary Purpose / Expected Result
Normalizing 900-950 °C 1-2 hours Air Refine grain structure
Annealing 600-700 °C 1-2 hours Air Improve ductility
Quenching & Tempering 850-900 °C 1-2 hours Water/Oil Increase strength

Heat treatment processes such as normalizing and quenching can significantly alter the microstructure of S355J2H, enhancing its mechanical properties.

Typical Applications and End Uses

Industry/Sector Specific Application Example Key Steel Properties Utilized in this Application Reason for Selection (Brief)
Construction Structural beams High yield strength, weldability Essential for load-bearing structures
Automotive Chassis components Toughness, ductility Required for safety and performance
Oil & Gas Pipelines Corrosion resistance, strength Critical for durability in harsh environments

Other applications include:
- Bridges
- Industrial buildings
- Heavy machinery

S355J2H is often selected for its balance of strength and weldability, making it ideal for structural components in various industries.

Important Considerations, Selection Criteria, and Further Insights

Feature/Property [S355J2H] [Alternative Grade 1] [Alternative Grade 2] Brief Pro/Con or Trade-off Note
Yield Strength 355 MPa 350 MPa 360 MPa Comparable strength
Corrosion Aspect Fair Good Excellent Trade-off for cost
Weldability Excellent Good Fair Important for construction
Machinability Moderate High Low Affects manufacturing cost
Approx. Relative Cost Moderate High Low Cost-effective for structural use
Typical Availability High Moderate Low Readily available in the market

When selecting S355J2H, considerations include cost-effectiveness, availability, and specific application requirements. Its moderate corrosion resistance may necessitate protective coatings in certain environments, while its weldability makes it a preferred choice for structural applications.

In summary, S355J2H steel is a versatile and robust material that meets the demands of various engineering applications, providing a balance of strength, weldability, and cost-effectiveness.