Mold steel is a specialized category of steel primarily used in the manufacturing of molds for various applications, including plastic injection molding, die casting, and stamping. This steel grade is typically classified as medium-carbon alloy steel, with a composition that includes significant amounts of chromium, nickel, and molybdenum, which enhance its hardness, toughness, and wear resistance.

Comprehensive Overview

Mold steel is engineered to withstand the rigorous demands of high-volume production environments. Its primary alloying elements—chromium (Cr), nickel (Ni), and molybdenum (Mo)—contribute to its exceptional hardness and toughness, making it suitable for applications where high wear resistance is essential. The presence of chromium enhances corrosion resistance, while nickel improves toughness at low temperatures. Molybdenum increases hardenability and strength at elevated temperatures.

Key Characteristics:
- High Hardness: Essential for maintaining shape and precision in molds.
- Excellent Wear Resistance: Reduces the frequency of mold replacement.
- Good Toughness: Prevents cracking under stress during operation.

Advantages:
- Durability: Mold steel can endure high-stress conditions, leading to longer service life.
- Versatility: Suitable for various molding processes, including plastics and metals.
- Cost-Effectiveness: Reduces downtime and maintenance costs due to its longevity.

Limitations:
- Brittleness: Can be prone to cracking if not properly heat-treated.
- Machinability: More challenging to machine compared to lower carbon steels.
- Cost: Generally more expensive than standard mild steels.

Historically, mold steels have played a crucial role in the advancement of manufacturing technologies, enabling the mass production of complex shapes and components.

Alternative Names, Standards, and Equivalents

Standard Organization Designation/Grade Country/Region of Origin Notes/Remarks
UNS A2 (D2) USA Closest equivalent with similar properties.
AISI/SAE AISI D2 USA High carbon content; excellent wear resistance.
ASTM ASTM A681 USA Specification for tool steels.
EN 1.2379 Europe Equivalent to AISI D2; minor compositional differences.
DIN X153CrMoV12 Germany Similar properties; often used in Europe.
JIS SKD11 Japan Comparable to AISI D2; used in similar applications.
GB 9CrSi China Closest equivalent; variations in toughness.
ISO ISO 4957 International Standard for tool steels.

The differences between these grades can affect performance in specific applications. For instance, while AISI D2 and EN 1.2379 are often considered equivalent, the heat treatment processes may yield different hardness levels, impacting wear resistance.

Key Properties

Chemical Composition

Element (Symbol and Name) Percentage Range (%)
C (Carbon) 1.40 - 1.60
Cr (Chromium) 11.00 - 13.00
Mo (Molybdenum) 0.70 - 1.20
Ni (Nickel) 0.80 - 1.50
Si (Silicon) 0.20 - 0.60
Mn (Manganese) 0.60 - 1.00
P (Phosphorus) ≤ 0.030
S (Sulfur) ≤ 0.030

The primary role of key alloying elements in mold steel includes:
- Carbon (C): Increases hardness and strength through heat treatment.
- Chromium (Cr): Enhances wear resistance and corrosion resistance.
- Molybdenum (Mo): Improves hardenability and strength at high temperatures.

Mechanical Properties

Property Condition/Temper Test Temperature Typical Value/Range (Metric) Typical Value/Range (Imperial) Reference Standard for Test Method
Tensile Strength Quenched & Tempered Room Temp 800 - 1200 MPa 1160 - 1740 ksi ASTM E8
Yield Strength (0.2% offset) Quenched & Tempered Room Temp 600 - 900 MPa 87 - 130 ksi ASTM E8
Elongation Quenched & Tempered Room Temp 10 - 15% 10 - 15% ASTM E8
Hardness (HRC) Quenched & Tempered Room Temp 58 - 62 HRC 58 - 62 HRC ASTM E18
Impact Strength Quenched & Tempered -20°C (-4°F) 20 - 30 J 15 - 22 ft-lbf ASTM E23

The combination of these mechanical properties makes mold steel particularly suitable for applications requiring high strength and wear resistance, such as in the production of molds for plastic injection and die casting. Its high tensile strength and hardness allow it to maintain dimensional stability under high pressure and temperature conditions.

Physical Properties

Property Condition/Temperature Value (Metric) Value (Imperial)
Density Room Temp 7.85 g/cm³ 0.284 lb/in³
Melting Point/Range - 1425 - 1540 °C 2600 - 2800 °F
Thermal Conductivity Room Temp 25 W/m·K 14.5 BTU·in/h·ft²·°F
Specific Heat Capacity Room Temp 0.46 kJ/kg·K 0.11 BTU/lb·°F
Electrical Resistivity Room Temp 0.000001 Ω·m 0.000001 Ω·in

Key physical properties such as density and thermal conductivity are significant for mold steel applications. The high density contributes to the material's durability, while the thermal conductivity is crucial for efficient heat dissipation during the molding process, preventing overheating and ensuring consistent mold temperatures.

Corrosion Resistance

Corrosive Agent Concentration (%) Temperature (°C/°F) Resistance Rating Notes
Chlorides 3-5% 20-60°C (68-140°F) Fair Risk of pitting corrosion.
Acids 10-20% 20-40°C (68-104°F) Poor Not recommended for strong acids.
Alkaline Solutions 5-10% 20-60°C (68-140°F) Fair Susceptible to stress corrosion cracking.
Atmospheric - - Good Performs well in mild environments.

Mold steel exhibits varying degrees of corrosion resistance depending on the environment. It performs well in atmospheric conditions but is susceptible to pitting in chloride-rich environments and stress corrosion cracking in alkaline solutions. Compared to stainless steels, mold steel generally has lower corrosion resistance, making it less suitable for applications in highly corrosive environments.

Heat Resistance

Property/Limit Temperature (°C) Temperature (°F) Remarks
Max Continuous Service Temp 200 392 Suitable for prolonged exposure.
Max Intermittent Service Temp 300 572 Short-term exposure only.
Scaling Temperature 600 1112 Risk of oxidation above this temp.
Creep Strength Considerations 400 752 Begins to degrade at this temp.

At elevated temperatures, mold steel maintains its structural integrity up to a certain limit. However, beyond the maximum continuous service temperature, the risk of oxidation and loss of mechanical properties increases. Proper heat treatment can enhance its performance in high-temperature applications.

Fabrication Properties

Weldability

Welding Process Recommended Filler Metal (AWS Classification) Typical Shielding Gas/Flux Notes
MIG ER70S-6 Argon + CO2 mix Preheat recommended.
TIG ER80S-Ni Argon Requires post-weld heat treatment.
Stick E7018 - Suitable for thicker sections.

Mold steel can be welded, but care must be taken to avoid cracking. Preheating before welding and post-weld heat treatment are essential to relieve stresses and ensure the integrity of the weld. The choice of filler metal is crucial for maintaining the desired properties.

Machinability

Machining Parameter Mold Steel (A2) AISI 1212 Notes/Tips
Relative Machinability Index 60 100 More difficult to machine.
Typical Cutting Speed 30 m/min 50 m/min Use carbide tools for best results.

Mold steel presents challenges in machining due to its hardness. Utilizing appropriate cutting tools and speeds is critical to achieving desired tolerances and surface finishes.

Formability

Mold steel is generally not as formable as lower carbon steels due to its higher hardness. Cold forming is limited, while hot forming is more feasible but requires careful temperature control to avoid cracking. Work hardening can occur, necessitating attention to bend radii and forming techniques.

Heat Treatment

Treatment Process Temperature Range (°C/°F) Typical Soaking Time Cooling Method Primary Purpose / Expected Result
Annealing 600 - 700 / 1112 - 1292 1-2 hours Air Reduce hardness, improve machinability.
Quenching 1000 - 1100 / 1832 - 2012 30 minutes Oil/Water Increase hardness and strength.
Tempering 150 - 200 / 302 - 392 1 hour Air Reduce brittleness, enhance toughness.

Heat treatment significantly affects the microstructure and properties of mold steel. Quenching increases hardness, while tempering helps to relieve internal stresses and improve toughness, making it suitable for demanding applications.

Typical Applications and End Uses

Industry/Sector Specific Application Example Key Steel Properties Utilized in this Application Reason for Selection (Brief)
Automotive Injection molds for bumpers High hardness, wear resistance Durability under high volume production.
Consumer Goods Molds for plastic containers Toughness, dimensional stability Precision and longevity in use.
Aerospace Die casting molds High strength, thermal stability Performance under extreme conditions.

Other applications include:
- Electronics: Molds for housings and components.
- Medical Devices: Precision molds for surgical instruments.
- Industrial Equipment: Molds for machine parts.

Mold steel is chosen for these applications due to its ability to maintain dimensional accuracy and withstand the rigors of production processes.

Important Considerations, Selection Criteria, and Further Insights

Feature/Property Mold Steel (A2) AISI D2 AISI P20 Brief Pro/Con or Trade-off Note
Key Mechanical Property High hardness Similar Lower hardness A2 offers better wear resistance.
Key Corrosion Aspect Fair Poor Good P20 is better for corrosion resistance.
Weldability Moderate Poor Good P20 is easier to weld.
Machinability Challenging Moderate Good P20 is more machinable.
Formability Limited Limited Good P20 offers better formability.
Approx. Relative Cost Moderate High Moderate Cost varies with market demand.
Typical Availability Common Common Common All grades are widely available.

When selecting mold steel, considerations include mechanical properties, corrosion resistance, and machinability. Mold steel is often favored for its superior hardness and wear resistance, while alternatives like P20 may be chosen for applications requiring better corrosion resistance and machinability. Cost-effectiveness and availability also play significant roles in material selection.

In conclusion, mold steel is a critical material in modern manufacturing, offering a unique combination of properties that make it suitable for high-performance applications. Understanding its characteristics, advantages, and limitations is essential for engineers and designers in selecting the right material for their specific needs.